# US 2008/0292800 A1 · Hydrophilic member and process for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0292800 A1
- Document ID: US20080292800A1
- Status: Published application
- Kind: A1
- Application number: 12/031,304
- Filed: 2008-02-14
- Published: 2008-11-27
- Earliest claimed: 2007-02-16
- Assignees: FUJIFILM Corporation
- Inventors: Yuichiro MURAYAMA; Sumiaki Yamasaki; Kazushi Furukawa
- Web page: https://patentgrep.com/patent/US20080292800A1

## CPC

- C09D 5/1668: {Vinyl-type polymers}
- B05D 5/04: to obtain a surface receptive to ink or other liquid (B05D5/02, {B41M5/52} take precedence)
- C03C 17/28: with organic material (C03C17/34, C03C17/44 take precedence)
- C09D 7/63: organic
- C09D 133/26: Homopolymers or copolymers of acrylamide or methacrylamide
- C09D 143/04: Homopolymers or copolymers of monomers containing silicon
- C23C 18/122: {Inorganic polymers, e.g. silanes, polysilazanes, polysiloxanes}
- C23C 18/1254: {Sol or sol-gel processing}
- C03C 2217/75: Hydrophilic and oleophilic coatings
- C03C 2218/116: by spin-coating, centrifugation
- C08K 5/057: Metal alcoholates {(metal enolates C08K5/0091)}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A process for producing a hydrophilic member, includes: coating a surface of a base material with a hydrophilic composition containing at least (a) a catalyst, (b) a hydrophilic polymer and (c) a metal alkoxide; and drying the composition, wherein a temperature for the drying is from 10° C. to 60° C.

## Claims

### Claim 1

A process for producing a hydrophilic member, comprising: coating a surface of a base material with a hydrophilic composition containing at least (a) a catalyst, (b) a hydrophilic polymer and (c) a metal alkoxide; and drying the composition, wherein a temperature for the drying is from 10° C. to 60° C.

### Claim 2 (depends on 1)

The process for producing a hydrophilic member according to claim 1, wherein the metal alkoxide is an alkoxide of an element selected among Si, Ti, Zr and Al.

### Claim 3 (depends on 1)

The process for producing a hydrophilic member according to claim 1, wherein a weight ratio of the catalyst to the metal alkoxide contained in the hydrophilic composition is from 50/50 to 20/80.

### Claim 4 (depends on 2)

The process for producing a hydrophilic member according to claim 2, wherein a weight ratio of the catalyst to the metal alkoxide contained in the hydrophilic composition is from 50/50 to 20/80.

### Claim 5 (depends on 1)

The process for producing a hydrophilic member according to claim 1, wherein the base material comprises glass, a plastic, a metal or a tile.

### Claim 6 (depends on 2)

The process for producing a hydrophilic member according to claim 2, wherein the base material comprises glass, a plastic, a metal or a tile.

### Claim 7 (depends on 3)

The process for producing a hydrophilic member according to claim 3, wherein the base material comprises glass, a plastic, a metal or a tile.

### Claim 8 (depends on 4)

The process for producing a hydrophilic member according to claim 4, wherein the base material comprises glass, a plastic, a metal or a tile.

### Claim 9 (depends on 1)

The process for producing a hydrophilic member according to claim 1, wherein a weight ratio of the catalyst to the metal alkoxide contained in the hydrophilic composition is from 45/55 to 30/70.

### Claim 10 (depends on 1)

The process for producing a hydrophilic member according to claim 1, wherein a temperature for the drying is from 25° C. to 50° C.

### Claim 11 (depends on 1)

The process for producing a hydrophilic member according to claim 1, wherein a time for the drying is from 5 minutes to one hour.

### Claim 12 (depends on 1)

The process for producing a hydrophilic member according to claim 1, wherein a time for the drying is from 10 minutes to 30 minutes.

### Claim 13 (depends on 1)

The process for producing a hydrophilic member according to claim 1, wherein the metal alkoxide is represented by the following formula (IV-1) or (IV-2):
(R8)m-Z-(OR9)4-m (IV-1)
Al—(OR9)3 (IV-2)
wherein R8 represents a hydrogen atom, an alkyl group which may have a substituent or an aryl group which may have a substituent; R9 represents an alkyl group which may have a substituent or an aryl group which may have a substituent; Z represents Si, Ti or Zr; and m represents an integer of from 0 to 2.

### Claim 14 (depends on 3)

The process for producing a hydrophilic member according to claim 3, wherein the metal alkoxide is represented by the following formula (IV-1) or (IV-2):
(R8)m-Z-(OR9)4−m (IV-1)
Al—(OR9)3 (IV-2)
wherein R8 represents a hydrogen atom, an alkyl group which may have a substituent or an aryl group which may have a substituent; R9 represents an alkyl group which may have a substituent or an aryl group which may have a substituent; Z represents Si, Ti or Zr; and m represents an integer of from 0 to 2.

### Claim 15 (depends on 1)

A hydrophilic member obtained by the process according to any one of claim 1.