# US 2008/0292797 A1 · Agent and method for flame-retardant processing of polyester-based fiber products

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0292797 A1
- Document ID: US20080292797A1
- Status: Published application
- Kind: A1
- Application number: 12/219,591
- Filed: 2008-07-24
- Published: 2008-11-27
- Earliest claimed: 2001-10-19
- Assignees: Daikyo Chemical Co., Ltd.
- Inventors: Terufumi Iwaki; Katsuo Sasa; Takeshi Masuda
- Web page: https://patentgrep.com/patent/US20080292797A1

## CPC

- D06M 13/453: Phosphates or phosphites containing nitrogen atoms
- D06M 2101/32: Polyesters
- D06M 2200/30: Flame or heat resistance, fire retardancy properties
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS

## Abstract

The invention provides a flame-retardant processing agent capable of imparting durable flame retardance to polyester-based fiber products without using halogen-based flame retardant. The flame-retardant processing agent is obtained by dispersing at least one phosphoric acid amide selected from the group consisting of 1,4-piperazinediyl bis(diarylphosphate), diaryl aminophosphate and aryl diaminophosphate as a flame retardant in a solvent in the presence of a nonionic surfactant or an anionic surfactant.

## Claims

### Claim at position 1

1-6. (canceled)

### Claim 7

A method for flame-retardant treatment of a polyester-based fiber product, comprising applying the polyester-based fiber product with a flame-retardant treating agent obtained by mixing a phosphoric acid amide represented by formula (I):
wherein Ar1, Ar2, Ar3 and Ar4 independently denote an aryl group, with water together with at least one surfactant selected from the group consisting of nonionic surfactants and anionic surfactants, and then milling the phosphoric acid amide into fine particles having a particle diameter in the range of 0.3 to 3 μm, so that the polyester-based fiber product has the phosphoric acid amide attached thereto in an amount of 0.5 to 20% by weight based on the polyester-based fiber product.

### Claim 8

A method for flame-retardant treatment of a polyester-based fiber product, comprising applying a flame-retardant treating agent obtained by mixing a phosphoric acid amide represented by formula (I):
wherein Ar1, Ar2, Ar3 and Ar4 independently denote an aryl group, with water together with at least one surfactant selected from the group consisting of nonionic surfactants and anionic surfactants, and then milling the phosphoric acid amide into fine particles having a particle diameter in the range of 0.3 to 3 μm, to the polyester-based fiber product, drying the resultant, and heat-treating the resultant at a temperature from 170 to 220° C., so that the polyester-based fiber product has the phosphoric acid amide attached thereto in an amount of 0.5 to 20% by weight based on the polyester-based fiber.

### Claim 9

A method for flame-retardant treatment of a polyester-based fiber product, comprising treating the polyester-based fiber product by an exhaustion method in which the polyester-based fiber product is immersed in a bath containing a flame-retardant treating agent therein and is heated at a temperature from 110 to 140° C. so that the polyester-based fiber product takes up the flame-retardant treating agent therein, the flame-retardant treating agent being obtained by mixing a phosphoric acid amide represented by formula (I):
wherein Ar1, Ar2, Ar3 and Ar4 independently denote an aryl group, with water together with at least one surfactant selected from the group consisting of nonionic surfactants and anionic surfactants, and then milling the phosphoric acid amide into fine particles having a particle diameter in the range of 0.3 to 3 μm, so that the polyester-based fiber product has the phosphoric acid amide attached thereto in an amount of 0.5 to 20% by weight based on the polyester-based fiber.

### Claim 10 (depends on 7)

The method according to claim 7 wherein the polyester-based fiber product has the phosphoric acid amide attached thereto in an amount of 0.5 to 2.8% by weight based on the polyester-based fiber product.

### Claim 11 (depends on 8)

The method according to claim 8 wherein the polyester-based fiber product has the phosphoric acid amide attached thereto in an amount of 0.5 to 2.8% by weight based on the polyester-based fiber product.

### Claim 12 (depends on 9)

The method according to claim 9 wherein the polyester-based fiber product has the phosphoric acid amide attached thereto in an amount of 0.5 to 2.8% by weight based on the polyester-based fiber product.

### Claim 13 (depends on 9)

The method according to claim 9 wherein the bath further contains a dispersion dye thereby the polyester-based fiber product is dyed and provided with the phosphoric acid amide.

### Claim 14 (depends on 7)

The method according to claim 7 wherein the aryl group is a phenyl group.

### Claim 15 (depends on 8)

The method according to claim 8 wherein the aryl group is a phenyl group.

### Claim 16 (depends on 9)

The method according to claim 9 wherein the aryl group is a phenyl group.