# US 2008/0292706 A1 · Hydrogel composition and methods for making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0292706 A1
- Document ID: US20080292706A1
- Status: Published application
- Kind: A1
- Application number: 12/180,262
- Filed: 2008-07-25
- Published: 2008-11-27
- Earliest claimed: 2004-09-30
- Assignees: DePuy Products, Inc.
- Inventors: Richard S. King; George Lawrence Grobe, III
- Web page: https://patentgrep.com/patent/US20080292706A1

## CPC

- A61L 31/145: {Hydrogels or hydrocolloids}
- A61L 15/60: Liquid-swellable gel-forming materials, e.g. super-absorbents
- A61L 26/008: {Hydrogels or hydrocolloids}
- A61L 27/52: Hydrogels or hydrocolloids
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)

## Abstract

The invention provides a hydrogel composition comprising water and a hydrophilic polymer, wherein the hydrogel composition has (a) an ultimate tensile strength of about 10 kPa or more, (b) a compressive strength of about 70 kPa or more, or (c) an ultimate tensile strength of about 10 kPa or more and a compressive strength of about 70 kPa or more. The invention further provides methods for producing a hydrogel composition.

## Claims

### Claim at position 1

1-30. (canceled)

### Claim 31

A method for producing a hydrogel composition water and a crosslinked hydrophilic polymer, wherein the hydrogel composition has (a) an ultimate tensile strength of about 10 kPa or more, (b) a compressive strength of about 70 kPa or more, or (c) an ultimate tensile strength of about 10 kPa or more and a compressive strength of about 70 kPa or more, the method comprising the steps of:
(a) providing a compression mold having an internal volume,
(b) providing a hydrogel precursor comprising a melt-processable, radiation crosslinkable, hydrophilic polymer,
(c) filling at least a portion of the internal volume of the compression mold with the precursor,
(d) compressing the precursor contained within the compression mold to form a molded body therefrom,
(e) irradiating at least a portion of the molded body to crosslink at least a portion of the hydrophilic polymer contained within the molded body, and
(f) hydrating the irradiated molded body to form a hydrogel therefrom.

### Claim 32 (depends on 31)

The method of claim 31, wherein the melt-processable, radiation crosslinkable, hydrophilic polymer has an average molecular weight of about 1,000,000 atomic mass units or more.

### Claim 33 (depends on 32)

The method of claim 32, wherein the melt-processable, radiation crosslinkable, hydrophilic polymer is poly(ethylene oxide).

### Claim 34 (depends on 31)

The method of claim 31, wherein the precursor is compressed at a pressure of about 3,800 kPa to about 14,000 kPa during step (d).

### Claim 35 (depends on 31)

The method of claim 31, wherein the precursor is heated to a temperature of about 120° C. to about 140° C. during step (d).

### Claim 36 (depends on 31)

The method of claim 31, wherein the precursor is compressed for about 5 to about 10 minutes during step (d).

### Claim 37 (depends on 31)

The method of claim 31, wherein the molded body is irradiated in step (e) by exposing the molded body to about 1.5 to about 6 Mrad of gamma radiation.

### Claim 38 (depends on 31)

The method of claim 31, wherein the molded body is hydrated by submerging at least a portion of the molded body in an aqueous solution having a temperature of about 50° C. to about 90° C. for about 120 hours to about 220 hours.

### Claim 39 (depends on 38)

The method of claim 38, wherein the aqueous solution further comprises an active ingredient selected from the group consisting of a drug, a therapeutic agent, a humectant, and mixtures thereof.

### Claim 40 (depends on 31)

The method of claim 31, wherein the hydrogel precursor further comprises an active ingredient selected from the group consisting of a drug, a therapeutic agent, a humectant, and mixtures thereof.

### Claim 41

A method for producing a hydrogel composition water and a crosslinked hydrophilic polymer, wherein the hydrogel composition has (a) an ultimate tensile strength of about 10 kPa or more, (b) a compressive strength of about 70 kPa or more, or (c) an ultimate tensile strength of about 10 kPa or more and a compressive strength of about 70 kPa or more, the method comprising the steps of:
(a) providing a dispersion comprising a crosslinking agent,
(b) providing a hydrogel precursor comprising a melt-processable, hydrophilic polymer,
(c) coating at least a portion of the hydrogel precursor with the dispersion,
(d) providing a compression mold having an internal volume,
(e) filling at least a portion of the internal volume of the compression mold with the coated precursor produced in step (c),
(f) compressing the precursor contained within the compression mold to form a molded body therefrom and crosslink at least a portion of the hydrophilic polymer contained within the molded body, and
(g) hydrating the molded body to form a hydrogel therefrom.

### Claim 42 (depends on 41)

The method of claim 41, wherein the crosslinking agent is a peroxide.

### Claim 43 (depends on 42)

The method of claim 42, wherein the crosslinking agent is benzoyl peroxide.

### Claim 44 (depends on 41)

The method of claim 41, wherein the melt-processable, hydrophilic polymer has an average molecular weight of about 1,000,000 atomic mass units or more.

### Claim 45 (depends on 44)

The method of claim 44, wherein the melt-processable, hydrophilic polymer is poly(ethylene oxide).

### Claim 46 (depends on 41)

The method of claim 41, wherein the precursor is compressed at a pressure of about 3,800 kPa to about 14,000 kPa during step (f).

### Claim 47 (depends on 41)

The method of claim 41, wherein the precursor is heated to a temperature of about 120° C. to about 140° C. during step (f).

### Claim 48 (depends on 41)

The method of claim 41, wherein the precursor is compressed for about 5 to about 10 minutes during step (f).

### Claim 49 (depends on 41)

The method of claim 41, wherein the molded body is hydrated by submerging at least a portion of the molded body in an aqueous solution having a temperature of about 50° C. to about 90° C. for about 120 hours to about 220 hours.

### Claim 50 (depends on 49)

The method of claim 49, wherein the aqueous solution further comprises an active ingredient selected from the group consisting of a drug, a therapeutic agent, a humectant, and mixtures thereof.

### Claim 51 (depends on 41)

The method of claim 41, wherein the hydrogel precursor further comprises an active ingredient selected from the group consisting of a drug, a therapeutic agent, a humectant, and mixtures thereof.

### Claim 52 (depends on 31)

The method of claim 31, wherein the hydrogel precursor further comprises a second polymer.

### Claim 53 (depends on 31)

The method of claim 31, which further includes incorporating a second polymer into the hydrogel.

### Claim 54 (depends on 41)

The method of claim 41, wherein the hydrogel precursor further comprises a second polymer.

### Claim 55 (depends on 41)

The method of claim 41, which further includes incorporating a second polymer into the hydrogel.

### Claim 56

A drug delivery device comprising a hydrogel composition comprising water, a crosslinked hydrophilic polymer, and a drug, wherein the hydrogel composition has (a) an ultimate tensile strength of about 10 kPa or more, (b) a compressive strength of about 70 kPa or more, or (c) an ultimate tensile strength of about 10 kPa or more and a compressive strength of about 70 kPa or more, and an active ingredient dispersed or dissolved in the hydrogel composition.

### Claim 57

A wound dressing comprising a hydrogel composition comprising comprising water and a crosslinked hydrophilic polymer, wherein the hydrogel composition has (a) an ultimate tensile strength of about 10 kPa or more, (b) a compressive strength of about 70 kPa or more, or (c) an ultimate tensile strength of about 10 kPa or more and a compressive strength of about 70 kPa or more.