# US 2008/0291583 A1 · Thin film magnetic head comprising metal layer and method of producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0291583 A1
- Document ID: US20080291583A1
- Status: Published application
- Kind: A1
- Application number: 11/802,220
- Filed: 2007-05-21
- Published: 2008-11-27
- Earliest claimed: 2007-05-21
- Assignees: TDK Corporation
- Inventors: Kosuke Tanaka; Kazuki Sato; Eiji Komura
- Web page: https://patentgrep.com/patent/US20080291583A1

## CPC

- G11B 5/3967: {Composite structural arrangements of transducers, e.g. inductive write and magnetoresistive read (G11B5/3906 takes precedence)}
- B82Y 25/00: Nanomagnetism, e.g. magnetoimpedance, anisotropic magnetoresistance, giant magnetoresistance or tunneling magnetoresistance
- G01R 33/093: {using multilayer structures, e.g. giant magnetoresistance sensors (thin magnetic films H01F10/00)}
- G11B 5/3912: {Arrangements in which the active read-out elements are transducing in association with active magnetic shields, e.g. magnetically coupled shields (G11B5/3916 takes precedence)}
- G11B 5/3932: {Magnetic biasing films}
- H10N 50/01: Manufacture or treatment
- H10N 50/10: Magnetoresistive devices
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- G01R: MEASURING ELECTRIC VARIABLES; MEASURING MAGNETIC VARIABLES (indicating correct tuning of resonant circuits H03J3/12)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

A method of producing a thin film magnetic head includes the steps of: forming a pair of openings in a predetermined region of a TMR layer formed on a lower magnetic shield layer; forming a pair of bias-applying layers in the pair of Openings so that an upper surface thereof may be located above an upper surface of the TMR layer; laminating a metal layer that covers the upper surface of a portion located between the pair of bias-applying layers in the TMR layer and the upper surface of the pair of bias-applying layers; forming a resist layer across the upper surface of a portion located above the pair of bias-applying layers in the metal layer and the upper surface of a portion located above the TMR layer in the metal layer; and etching a part of the TMR layer and a part of the pair of bias-applying layers with the resist layer being as a mask. Here, the reflectivity R for the incident light having a wavelength of 248 nm at an interface between the metal layer and the resist layer is set so as to satisfy the condition represented by the following formula (1), and also the magnitude D of a step is set so as to satisfy the condition represented by the following formula (2). R≧0.2 (1) D≧210 exp(−7.6R) [nm] (2)

## Claims

### Claim 1

A method of producing a thin film magnetic head, comprising the steps of:
forming a lower magnetic shield layer on a base;
forming a magneto-resistance effect layer on the lower magnetic shield layer;
forming a pair of openings in a predetermined region of the magneto-resistance effect layer;
forming a pair of bias-applying layers in the pair of openings so that an upper surface thereof may be located above an upper surface of the magneto-resistance effect layer;
forming a metal layer group by laminating at least one metal layer, which covers an upper surface of a portion located between the pair of bias-applying layers in the magneto-resistance effect layer and an upper surface of the pair of bias-applying layers;
forming a resist layer across the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and the upper surface of a portion located above the magneto-resistance effect layer of the metal layer group;
etching a part of the magneto-resistance effect layer and a part of the pair of bias-applying layers with the resist layer being as a mask;
forming an insulating layer in a state where the resist layer remains; and
forming an upper magnetic shield layer after removing the resist layer: wherein
reflectivity R1 for an incident light having a wavelength of 248 nm, the reflectivity being obtained by dividing a total value of a reflected light flux from each metal layer constituting the metal layer group at an interface between the metal layer group and the resist layer by a value of an incident light flux at the interface between the metal layer group and the resist layer, is set so as to satisfy a condition represented by the following formula (1); and wherein a magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect layer of the metal layer group, is set so as to satisfy the condition represented by the following formula (2).
R1≧0.2 (1)
D≧210 exp(−7.6R1) [nm] (2)

### Claim 2 (depends on 1)

The method of producing a thin film magnetic head according to claim 1, wherein the magnitude D of the step is set so as to further satisfy the condition that the magnitude D is not more than ½ of the direct distance between the upper magnetic shield layer and the lower magnetic shield layer.

### Claim 3 (depends on 1)

The method of producing a thin film magnetic head according to claim 1, wherein the magnitude D of the step is set so as to further satisfy the condition represented by the following formula (3).
D≦45 [nm] (3)

### Claim 4 (depends on 3)

The method of producing a thin film magnetic head according to claim 3, wherein the magnitude D of the step is set so as to further satisfy the condition represented by the following formula (4).
D≦20 [nm] (4)

### Claim 5 (depends on 1)

The method of producing a thin film magnetic head according to claim 1, wherein the reflectivity R1 is set so as to further satisfy the condition represented by the following formula (5).
R1≧0.3 (5)

### Claim 6 (depends on 1)

The method of producing a thin film magnetic head according to claim 1: wherein reflectivity R2 for the incident light having a wavelength of 248 nm at an interface between a metal layer located on The uppermost part of the metal layer group and the resist layer is set so as to satisfy the condition represented by the following formula (6); and wherein the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect element of the metal layer group, is set so as to satisfy the condition represented by the following formula (7).
R2≧0.2 (6)
D≧210 exp(−7.6R2) [nm] (7)

### Claim 7 (depends on 1)

The method of producing a thin film magnetic head according to claim 1, wherein the resist layer has the refractive index of 1.6 to 1.8 for the incident light with a wavelength of 248 nm and the absorption coefficient of 0 to 0.001.

### Claim 8

A method of producing a thin film magnetic head, comprising the steps of:
forming a lower magnetic shield layer on a base;
forming a magneto-resistance effect layer on the lower magnetic shield layer;
forming a pair of openings in a predetermined region of the magneto-resistance effect layer;
forming a pair of bias-applying layers in the pair of openings so that an upper surface thereof may be located above an upper surface of the magneto-resistance effect layer;
forming a metal layer group by laminating at least one metal layer, which covers an upper surface of a portion located between the pair of bias-applying layers in the magneto-resistance effect layer and an upper surface of the pair of bias-applying layers;
forming a resist layer across the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and the upper surface of a portion located above the magneto-resistance effect layer of the metal layer group;
etching a part of the magneto-resistance effect layer and a part of the pair of bias-applying layers with the resist layer being as a mask;
forming an insulating layer in a state where the resist layer remains; and
forming an upper magnetic shield layer after removing the resist layer: wherein
a metal layer located on the uppermost part of the metal layer group is comprised of Ti and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect layer of the metal layer group, is set to not less than 36.0 nm; or wherein
a metal layer located on the uppermost part of the metal layer group is comprised of Ta and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect layer of the metal layer group, is set to not less than 31.2 nm; or wherein
a metal layer located on the uppermost part of the metal layer group is comprised of W and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect layer of the metal layer group, is set to not less than 18.0 nm; or wherein
a metal layer located on the uppermost part of the metal layer group is comprised of NiCr and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect layer of the metal layer group, is set to not less than 16.7 nm; or wherein
a metal layer located on the uppermost part of the metal layer group is comprised of Mo and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect layer of the metal layer group, is set to not less than 8.1 nm; or wherein
a metal layer located on the uppermost part of the metal layer group is comprised of Ru and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect layer of the metal layer group, is set to not less than 2.3 nm; or wherein
a metal layer located on the uppermost part of the metal layer group is comprised of Al and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect layer of the metal layer group, is set to not less than 0.2 nm.

### Claim 9

A thin film magnetic head having a medium facing surface, comprising:
an upper magnetic shield layer and a lower magnetic shield layer opposed to each other;
a magneto-resistance effect element located between the upper magnetic shield layer and the lower magnetic shield layer;
a pair of bias-applying layers which is located between the upper magnetic shield layer and the lower magnetic shield layer and applies a bias magnetic field to the magneto-resistance effect element; and
a metal layer group which is located in a region corresponding to the magneto-resistance effect element and the pair of bias-applying layers as seen from a laminating direction, and is formed by laminating at least one metal layer above the magneto-resistance effect element and the pair of bias-applying layers; wherein
an upper surface of the pair of bias-applying layers is located closer to the upper magnetic shield layer side than an upper surface of the magneto-resistance effect element; wherein
the width of the pair of bias-applying layers in the depth direction relative to the medium facing surface is larger than that of the magneto-resistance effect element in the depth direction relative to the medium facing surface; and wherein
the metal layer group is set such that reflectivity R3 for an incident light having a wavelength of 248 nm, the reflectivity being obtained by dividing a total value of a reflected light flux from each metal layer constituting the metal layer group at an interface between the metal layer group and a resist layer, assuming that the resist layer is adjacent onto the metal layer group, by a value of an incident light flux at the interface between the metal layer group and the assumed resist layer, satisfies the condition represented by the following formula (8), and also the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect element of the metal layer group, is set so as to satisfy the condition represented by the following formula (9).
R3≧0.2 (8)
D≧210 exp(−7.6R3) [nm] (9)

### Claim 10 (depends on 9)

The thin film magnetic head according to claim 9, wherein the magnitude D of the step is set so as to further satisfy the condition that the magnitude D is not more than ½ of a direct distance between the upper magnetic shield layer and the lower magnetic shield layer.

### Claim 11 (depends on 9)

The thin film magnetic head according to claim 9, wherein the magnitude D of the step is set so as to further satisfy the condition represented by the following formula (10).
D≦45 [nm] (10)

### Claim 12 (depends on 11)

The thin film magnetic head according to claim 11, wherein the magnitude D of the step is set so as to further satisfy the condition represented by the following formula (11).
D≦20 [nm] (11)

### Claim 13 (depends on 9)

The thin film magnetic head according to claim 9, wherein the reflectivity R3 is set so as to further satisfy the condition represented by the following formula (12).
R3≧0.3 (12)

### Claim 14 (depends on 9)

The thin film magnetic head according to claim 9: wherein the metal layer group is set such that reflectivity R4 for an incident light having a wavelength of 248 nm at an interface between a metal layer located on the uppermost part of the metal layer group and the assumed resist layer satisfies the condition represented by the following formula (13); and wherein the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect element of the metal layer group, is set so as to satisfy the condition represented by the following formula (14).
R4≧0.2 (13)
D≧210 exp(−7.6R4) [nm] (14)

### Claim 15 (depends on 9)

A thin film magnetic head according to claim 9, wherein the assumed resist layer has the refractive index of 1.6 to 1.8 for the incident light with a wavelength of 248 nm and the absorption coefficient of 0 to 0.001.

### Claim 16

A thin film magnetic head having a medium facing surface, comprising:
an upper magnetic shield layer and a lower magnetic shield layer opposed to each other;
a magneto-resistance effect element located between the upper magnetic shield layer and the lower magnetic shield layer;
a pair of bias-applying layers; which is located between the upper magnetic shield layer and the lower magnetic shield layer and applies a bias magnetic field to the magneto-resistance effect element; and
a metal layer group which is located in a region corresponding to the magneto-resistance effect element and the pair of bias-applying layers as seen from a laminating direction, and is formed by laminating at least one metal layer above the magneto-resistance effect element and the pair of bias-applying layers; wherein
an upper surface of the pair of bias-applying layers is located closer to the upper magnetic shield layer side than an upper surface of the magneto-resistance effect element; wherein
a width of the pair of bias-applying layers in the depth direction relative to the medium facing surface is larger than that of the magneto-resistance effect element in the depth direction relative to the medium facing surface; wherein
a metal layer located on the uppermost part of the metal layer group is comprised of Ti and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect element of the metal layer group, is set to not less than 36.0 nm; or wherein
a metal layer located on the uppermost part of the metal layer group is comprised of Ta and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect element of the metal layer group, is set to not less than 31.2 nm; or wherein
a metal layer located on the uppermost part of the metal layer group is comprised of W and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect element of the metal layer group, is set to not less than 18.0 nm; or wherein
a metal layer located on the uppermost part of the metal layer group is comprised of NiCr and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect element of the metal layer group, is set to not less than 16.7 nm; or wherein
a metal layer located on the uppermost part of the metal layer group is comprised of Mo and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect element of the metal layer group, is set to not less than 8.1 nm; or wherein
a metal layer located on the uppermost part of the metal layer group is comprised of Ru and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect element of the metal layer group, is set to not less than 2.3 nm; or wherein
a metal layer located on the uppermost part of the metal layer group is comprised of Al and the magnitude D of a step, which is a direct distance between a virtual plane including the upper surface of a portion located above the pair of bias-applying layers of the metal layer group and a virtual plane including the upper surface of a portion located above the magneto-resistance effect element of the metal layer group, is set to not less than 0.2 nm.