# US 2008/0291257 A1 · Ink jet recording material and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0291257 A1
- Document ID: US20080291257A1
- Status: Published application
- Kind: A1
- Application number: 12/024,615
- Filed: 2008-02-01
- Published: 2008-11-27
- Earliest claimed: 2007-03-14
- Assignees: FUJIFILM Corporation
- Inventors: Yasuhiro OGATA
- Web page: https://patentgrep.com/patent/US20080291257A1

## CPC

- B41M 5/504: {Backcoats}
- B41M: PRINTING, DUPLICATING, MARKING, OR COPYING PROCESSES; COLOUR PRINTING, (correction of typographical errors B41J; processes for applying transfer pictures or the like B44C1/16; fluid media for correction of typographical errors by coating C09D10/00; printing textiles D06P)

## Abstract

The present invention provides an ink jet recording material and a method for manufacturing the same, wherein the ink jet recording material comprises: a support having a base paper and polyolefin resin layers covering the both sides of the base paper; an ink receiving layer formed on one side of the support; and a back layer containing a polyurethane resin formed on the other side of the support opposite to the side having the ink receiving layer, wherein the back layer is formed within three hours after the polyolefin resin layer is formed on the other side of the base paper.

## Claims

### Claim 1

An ink jet recording material, comprising:
a support having a base paper and polyolefin resin layers covering the both sides of the base paper;
an ink receiving layer formed on one side of the support; and
a back layer containing a polyurethane resin formed on the other side of the support opposite to the side having the ink receiving layer,
wherein the back layer is formed within three hours after the polyolefin resin layer is formed on the other side of the base paper.

### Claim 2

A method for manufacturing an ink jet recording material, comprising:
forming a support having a base paper and polyolefin resin layers covering the both sides of the base paper;
forming an ink receiving layer on one side of the support; and
forming a back layer containing a polyurethane resin on the other side of the support opposite to the side having the ink receiving layer,
wherein the back layer is formed within three hours after the polyolefin resin layer is formed on the other side of the base paper.

### Claim 3 (depends on 2)

The method of claim 2 for manufacturing an ink jet recording material, wherein the polyolefin resin layer and the back layer on the other side of the support are formed in succession.

### Claim 4 (depends on 1)

The ink jet recording material of claim 1, wherein the ink receiving layer includes, from the support side, an ink absorption layer containing inorganic fine particles, polyvinyl alcohol, and a thioether-based compound, and a layer containing colloidal silica.

### Claim 5 (depends on 2)

The method of claim 2 for manufacturing an ink jet recording material, wherein the ink receiving layer includes, from the support side, an ink absorption layer containing inorganic fine particles, polyvinyl alcohol, and a thioether-based compound, and a layer containing colloidal silica.

### Claim 6 (depends on 3)