# US 2008/0290569 A1 · Crucibles for melting titanium alloys

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0290569 A1
- Document ID: US20080290569A1
- Status: Published application
- Kind: A1
- Application number: 11/863,492
- Filed: 2007-09-28
- Published: 2008-11-27
- Earliest claimed: 2007-04-30
- Assignees: General Electric Company
- Inventors: BERNARD PATRICK BEWLAY; Brian Michael Ellis; Michael Francis Xavier Gigliotti; Thomas Jospeh Kelly; Mohamed Rahmane; Stephen Francis Rutkowski; Michael James Weimer; Joseph Carl Wukusick
- Web page: https://patentgrep.com/patent/US20080290569A1

## CPC

- F27B 14/10: Crucibles
- C22B 9/003: {by induction}
- C22B 34/1295: {Refining, melting, remelting, working up of titanium}
- F27B 2014/104: {Crucible linings}
- Y02P 10/25: Process efficiency
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Crucibles for melting titanium alloys having a facecoat including at least one facecoat layer containing an oxide selected from scandium oxide, yttrium oxide, hafnium oxide, a lanthanide series oxide, and combinations thereof, and a backing including at least one backing layer where the crucible has a backing to facecoat thickness ratio of from about 6.5:1 to about 20:1.

## Claims

### Claim 1

A crucible for melting titanium alloys comprising:
a facecoat including at least one facecoat layer comprising an oxide selected from the group consisting of scandium oxide, yttrium oxide, hafnium oxide, a lanthanide series oxide, and combinations thereof; and
a backing including at least one backing layer
wherein the crucible has a backing to facecoat thickness ratio of from about 6.5:1 to about 20:1.

### Claim 2 (depends on 1)

The crucible of claim 1 wherein the lanthanide series oxide comprises an oxide selected from the group consisting of lanthanum oxide, cerium oxide, prasiodymium oxide, neodymium oxide, promethium oxide, samarium oxide, europium oxide, gadolinium oxide, terbium oxide, dysprosium oxide, holmium oxide, erbium oxide, ytterbium oxide, lutetium oxide, and combinations thereof.

### Claim 3 (depends on 1)

The crucible of claim 1 wherein the at least one facecoat layer comprises from about 40% to about 100% of the oxide by weight.

### Claim 4 (depends on 1)

The crucible of claim 1 wherein the at least one facecoat layer is made from a facecoat slurry comprising an oxide powder in a colloidal suspension wherein the colloidal suspension comprises a colloid selected from the group consisting of colloidal silica, colloidal yttria, colloidal alumina, colloidal calcium oxide, colloidal magnesium oxide, colloidal zirconium oxide, colloidal lanthanide series oxide, and mixtures thereof.

### Claim 5 (depends on 1)

The crucible of claim 1 wherein the at least one backing layer is made from a backing slurry comprising a refractory material selected from the group consisting of aluminum oxide, zirconium silicate, silicon dioxide, and combinations thereof, in a colloidal silica suspension.

### Claim 6 (depends on 1)

The crucible of claim 1 wherein the facecoat comprises at least two facecoat layers.

### Claim 7 (depends on 6)

The crucible of claim 6 wherein each facecoat layer comprises the same oxide.

### Claim 8 (depends on 1)

The crucible of claim 1 wherein the at least one facecoat layer has a thickness of from about 50 microns to about 500 microns.

### Claim 9 (depends on 1)

The crucible of claim 1 comprising from 2 to 40 backing layers.

### Claim 10 (depends on 4)

The crucible of claim 4 wherein the facecoat slurry comprises a yttrium oxide powder in a colloidal suspension wherein the colloidal suspension comprises a colloid selected from the group consisting of colloidal silica, colloidal yttria, colloidal alumina, colloidal calcium oxide, colloidal magnesium oxide, colloidal zirconium oxide, colloidal lanthanide series oxide, and mixtures thereof.

### Claim 11 (depends on 1)

The crucible of claim 1 further comprising a stucco layer applied to each facecoat layer wherein the stucco layer comprises an oxide combined with a refractory material.

### Claim 12 (depends on 5)

The crucible of claim 5 further comprising a stucco layer applied to each backing layer wherein the stucco layer comprises an oxide combined with a refractory material.

### Claim 13 (depends on 1)

The crucible of claim 1 further comprising a topcoat including a yttrium oxide powder in a colloidal suspension wherein the colloidal suspension comprises a colloid selected from the group consisting of colloidal silica, colloidal yttria, colloidal alumina, colloidal calcium oxide, colloidal magnesium oxide, colloidal zirconium oxide, colloidal lanthanide series oxide, and mixtures thereof.

### Claim 14

A crucible for melting titanium alloys comprising:
a facecoat including at least one facecoat layer comprising an oxide selected from the group consisting of scandium oxide, yttrium oxide, hafnium oxide, a lanthanide series oxide, and combinations thereof; and
a backing including at least one backing layer
wherein the crucible has an overall wall thickness of from about 6.5 mm to about 40 mm.

### Claim 15 (depends on 14)

The crucible of claim 14 comprising a stucco layer applied to each facecoat layer and each backing layer.

### Claim 16 (depends on 15)

The crucible of claim 15 wherein the stucco layers are graded to account for differences in thermal expansion between each facecoat layer and each backing layer.

### Claim 17 (depends on 14)

The crucible of claim 14 further comprising a topcoat made from a yttrium oxide powder in a colloidal suspension wherein the colloidal suspension comprises a colloid selected from the group consisting of colloidal silica, colloidal yttria, colloidal alumina, colloidal calcium oxide, colloidal magnesium oxide, colloidal zirconium oxide, colloidal lanthanide series oxide, and mixtures thereof.

### Claim 18

A crucible for melting titanium alloys comprising:
a facecoat including at least one facecoat layer comprising an oxide selected from the group consisting of scandium oxide, yttrium oxide, hafnium oxide, a lanthanide series oxide, and combinations thereof;
a backing including at least one backing layer made from a backing slurry comprising a refractory material selected from the group consisting of aluminum oxide, zirconium silicate, silicon dioxide, and combinations thereof, in a colloidal silica suspension; and
a stucco layer applied to each facecoat layer and each backing layer wherein each facecoat layer has a thickness of from about 50 microns to about 500 microns and wherein the crucible has a backing to facecoat thickness ratio of from about 6.5:1 to about 20:1.

### Claim 19 (depends on 18)

The crucible of claim 18 wherein the stucco layers are graded to account for differences in thermal expansion between each facecoat layer and each backing layer.

### Claim 20 (depends on 18)

The crucible of claim 18 further comprising a topcoat made from a yttrium oxide powder in a colloidal suspension wherein the colloidal suspension comprises a colloid selected from the group consisting of colloidal silica, colloidal yttria, colloidal alumina, colloidal calcium oxide, colloidal magnesium oxide, colloidal zirconium oxide, colloidal lanthanide series oxide, and mixtures thereof.