# US 2008/0290552 A1 · Microporous polyolefin film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0290552 A1
- Document ID: US20080290552A1
- Status: Published application
- Kind: A1
- Application number: 12/111,121
- Filed: 2008-04-28
- Published: 2008-11-27
- Earliest claimed: 2003-10-27
- Assignees: Asahi Kasei Chemicals Corporation
- Inventors: Daisuke INAGAKI; Takahiko KONDO
- Web page: https://patentgrep.com/patent/US20080290552A1

## CPC

- C08L 23/04: Homopolymers or copolymers of ethene
- C08J 5/18: Manufacture of films or sheets
- C08L 23/06: Polyethylene
- H01M 50/417: Polyolefins
- H01M 50/489: Separators, membranes, diaphragms or spacing elements inside the cells, characterised by their physical properties, e.g. swelling degree, hydrophilicity or shut down properties
- H01M 50/491: Porosity
- C08J 2205/05: Open cells, i.e. more than 50% of the pores are open
- C08J 2323/04: Homopolymers or copolymers of ethene
- C08J 2323/06: Polyethene
- C08L 2205/02: containing two or more polymers of the same C08L -group
- Y02E 60/10: Energy storage using batteries
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A microporous polyolefin film which comprises 5 to 95 wt. % polyethylene (A) having a viscosity-average molecular weight (Mv) of 2,000,000 or higher, a first-melting-peak signal height as determined by DSC (differential scanning calorimetry) of 3.0 mW/mg or higher, a specific surface area of 0.7 m2/g or larger, and an average particle diameter of 1 to 150 μm and 95 to 5 wt. % polyethylene (B) having an Mw of 10,000 to 200,000, excluding 10,000 and 200,000, wherein the ratio of the Mv of the compound (A) to that of the compound (B), (A)/(B), is 10 or higher, the film as a whole has a molecular weight of 300,000 to 1,500,000, and the film has a fuse temperature of 120 to 140° C., a breaking temperature of 150° C. or higher, and a ratio of the piercing strength at 25° C. to the piercing strength at 140° C. of from 0.01 to 0.25.

## Claims

### Claim at position 1

1-10. (canceled)

### Claim 11

A process for producing a microporous polyolefin film which has a molecular weight of 300,000 to 1,500,000 as a whole of the film, a fuse temperature of 120 to 140° C., a film breakage temperature of 150° C. or more, and a ratio of the piercing strength at 140° C. to the piercing strength at 25° C. of 0.01 to 0.25, the process comprising kneading a mixture comprising a polyolefin composition comprising 5 to 95 wt % of polyethylene (A) having a viscosity average molecular weight (Mv) of 2,000,000 or more, a first melting-peak signal height as determined by DSC (differential scanning calorimetry) of 3.0 mW/mg or more, a specific surface area of 0.7 m2/g or more and an average particle size of 1 to 150 μm and 95 to 5 wt % of polyethylene (B) having an Mw of more than 10,000 and less than 200,000, wherein the Mv ratio of the component (A) to the component (B), (A)/(B), is 10 or more, with a plasticizer; extruding the kneaded product and then molding the product into a gel-like sheet to cool and solidify the sheet; drawing the resulting gel-like sheet; extracting the plasticizer to dry the sheet; and thermally fixing the film, wherein the thermal fixation step comprises a step of drawing the film in a TD direction after extracting the plasticizer and a subsequent step of thermally shrinking the film in the TD direction with reference to film width after the drawing step.

### Claim 12 (depends on 11)

The process according to claim 11, wherein the drawing step is a step of drawing the film after extracting the plasticizer by at least 20% in the TD direction and the thermal shrinkage step is a step of thermally shrinking the film after extracting the plasticizer by at least 10% in the TD direction with reference to the film width after the drawing step.