# US 2008/0290393 A1 · Nonvolatile semiconductor memory device and manufacturing method thereof, semiconductor device and manufacturing method thereof, and manufacturing method of insulating film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0290393 A1
- Document ID: US20080290393A1
- Status: Published application
- Kind: A1
- Application number: 11/802,093
- Filed: 2007-05-18
- Published: 2008-11-27
- Earliest claimed: 2006-05-26
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Tetsuya Kakehata; Tetsuhiro Tanaka; Yoshinobu Asami
- Web page: https://patentgrep.com/patent/US20080290393A1

## CPC

- H10P 14/6532: {by exposure to a plasma}
- H10B 41/30: characterised by the memory core region
- H10B 69/00: Erasable-and-programmable ROM [EPROM] devices not provided for in groups H10B41/00 - H10B63/00, e.g. ultraviolet erasable-and-programmable ROM [UVEPROM] devices
- H10D 30/0411: {of FETs having floating gates}
- H10D 30/6739: {Conductor-insulator-semiconductor electrodes}
- H10D 30/6758: {characterised by the insulating substrates}
- H10D 30/681: {having only two programming levels (Floating gate IGFETs programmable by two single electrons H10D30/688)}
- H10D 86/40: characterised by multiple TFTs
- H10D 86/60: wherein the TFTs are in active matrices
- H10P 14/6304: {Formation by oxidation, e.g. oxidation of the substrate}
- H10P 14/6322: {Formation by thermal treatments (formation by plasma treatment H10P14/6319)}
- H10P 14/6329: {using physical ablation of a target, e.g. physical vapour deposition or pulsed laser deposition}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6927: {the material being a silicon oxynitride, e.g. SiON or SiON:H}
- H10P 14/69391: {the material containing aluminium, e.g. Al2O3}
- H10P 14/69392: {the material containing hafnium, e.g. HfO2}
- H10P 14/69393: {the material containing tantalum, e.g. Ta2O5}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

An object is to provide a technique to manufacture an insulating film having excellent film characteristics. In particular, an object is to provide a technique to manufacture a dense insulating film with a high withstand voltage. Moreover, an object is to provide a technique to manufacture an insulating film with few electron traps. An insulating film including oxygen is subjected to plasma treatment using a high frequency under the conditions where the electron density is 1×1011 cm−3 or more and the electron temperature is 1.5 eV or less in an atmosphere including oxygen.

## Claims

### Claim 1

A method for manufacturing a nonvolatile semiconductor memory device comprising:
forming a semiconductor region;
forming a first insulating film including hydrogen over the semiconductor region;
reducing a hydrogen content of the first insulating film by performing plasma treatment on the first insulating film in an atmosphere including oxygen;
forming a floating gate electrode over the first insulating film;
forming a second insulating film over the floating gate electrode;
forming a control gate electrode over the second insulating film; and
adding an impurity element to the semiconductor region.

### Claim 2 (depends on 1)

The method for manufacturing the nonvolatile semiconductor memory device according to claim 1, further comprising:
performing plasma treatment on the second insulating film in an atmosphere including oxygen.

### Claim 3 (depends on 1)

The method for manufacturing the nonvolatile semiconductor memory device according to claim 1, wherein the plasma is excited by microwave.

### Claim 4 (depends on 1)

The method for manufacturing the nonvolatile semiconductor memory device according to claim 1, wherein each of the first insulating film and the second insulating film has a hydrogen concentration of 5×1019 atoms/cm3 or less by a secondary ion mass spectrometry.

### Claim 5 (depends on 1)

The method for manufacturing the nonvolatile semiconductor memory device according to claim 1, wherein each of the first insulating film and the second insulating film is formed by a method selected from the group consisting of a CVD method, a sputtering method, and a thermal oxidation method.

### Claim 6 (depends on 1)

The method for manufacturing the nonvolatile semiconductor memory device according to claim 1, wherein each of the first insulating film and the second insulating film comprises a material selected from the group consisting of a silicon oxide, silicon oxynitride, silicon nitride oxide, aluminum oxide, tantalum oxide, and hafnium oxide.

### Claim 7 (depends on 1)

The method for manufacturing the nonvolatile semiconductor memory device according to claim 1, wherein the atmosphere including oxygen further includes a noble gas.

### Claim 8

A method for manufacturing a semiconductor device comprising:
forming a semiconductor region;
forming a gate insulating film including hydrogen over the semiconductor region;
reducing a hydrogen content of the gate insulating film by performing plasma treatment on the gate insulating film in an atmosphere including oxygen;
forming a gate electrode over the gate insulating film; and
adding an impurity element to the semiconductor region.

### Claim 9 (depends on 8)

The method for manufacturing the semiconductor device according to claim 8, wherein the plasma is excited by microwave.

### Claim 10 (depends on 8)

The method for manufacturing the semiconductor device according to claim 8, wherein the gate insulating film has a hydrogen concentration of 5×1019 atoms/cm3 or less by a secondary ion mass spectrometry.

### Claim 11 (depends on 8)

The method for manufacturing the semiconductor device according to claim 8, wherein the gate insulating film is formed by a method selected from the group consisting of a CVD method, a sputtering method, and a thermal oxidation method.

### Claim 12 (depends on 8)

The method for manufacturing the semiconductor device according to claim 8, wherein the gate insulating film comprises a material selected from the group consisting of a silicon oxide, silicon oxynitride, silicon nitride oxide, aluminum oxide, tantalum oxide, and hafnium oxide.

### Claim 13 (depends on 8)

The method for manufacturing the semiconductor device according to claim 8, wherein the atmosphere including oxygen further includes a noble gas.

### Claim 14

A nonvolatile semiconductor memory device comprising:
a semiconductor region having a channel formation region between a pair of impurity regions;
a floating gate electrode provided over the semiconductor region with a first insulating film interposed therebetween; and
a control gate electrode provided over the floating gate electrode with a second insulating film interposed therebetween,
wherein each of the first insulating film and the second insulating film has a hydrogen concentration of 5×1019 atoms/cm3 or less by a secondary ion mass spectrometry.

### Claim 15 (depends on 14)

The nonvolatile semiconductor memory device according to claim 14, wherein each of the first insulating film and the second insulating film has an etching rate of 8 nm/min or less with respect to 0.5 wt % hydrofluoric acid.

### Claim 16

A semiconductor device comprising:
a semiconductor region having a channel formation region between a pair of impurity regions; and
a gate electrode provided over the semiconductor region with a gate insulating film interposed therebetween,
wherein the gate insulating film has a hydrogen concentration of 5×1019 atoms/cm3 or less by a secondary ion mass spectrometry.

### Claim 17 (depends on 16)

The semiconductor device according to claim 16, wherein the gate insulating film has an etching rate of 8 nm/min or less with respect to 0.5 wt % hydrofluoric acid.