# US 2008/0290064 A1 · Method for forming sapphire micro-lens in led process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0290064 A1
- Document ID: US20080290064A1
- Status: Published application
- Kind: A1
- Application number: 12/125,952
- Filed: 2008-05-23
- Published: 2008-11-27
- Earliest claimed: 2007-05-25
- Inventors: Ki-Jun Yun
- Web page: https://patentgrep.com/patent/US20080290064A1

## CPC

- B29D 11/00365: {Production of microlenses (lenticular sheets B29D11/00278)}
- G02B 3/0006: {Arrays (G02B3/02, G02B5/188 take precedence)}
- H10H 20/819: characterised by their shape, e.g. curved or truncated substrates
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

A method for forming a micro-lens on a sapphire substrate in an LED process. In the method for forming the micro-lens on the sapphire substrate in the LED process, the ratio of source power and bias power used to generate plasma into a chamber is set to the optimum ratio of 3:1 in order to minimize the burning phenomenon of a photoresist mask caused by plasma having strong potential when a conventional micro-lens is formed. In essence, plasma having low potential energy can be realized in RIE etch used to form the micro-lens on the sapphire substrate, thereby minimizing the burning phenomenon of the photoresist mask. A yield rate can be improved in the LED process.

## Claims

### Claim 1

A method for forming a sapphire micro-lens for an LED, the method comprising:
providing a sapphire substrate on a support; and then
coating a photoresist layer on a sapphire substrate in order to form an LED; and then
forming a mask pattern on the sapphire substrate; and then
forming a plurality of micro-lenses on the sapphire substrate by performing reaction ion etching with respect to the sapphire substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein during forming the plurality of microlenses, the reaction ion etching is performed using a plasma source in a state in which a ratio between a source power and a bias power is set to a ratio of 2.5:1 to 3.5:1.

### Claim 3 (depends on 2)

The method of claim 2, wherein during forming the plurality of micro-lenses, the substrate support is maintained at a temperature in range of −15° C. to −25° C.

### Claim 4 (depends on 2)

The method of claim 2, wherein during forming the plurality of micro-lenses, the source power is set in a range of 300 W to 1800 W.

### Claim 5 (depends on 2)

The method of claim 2, wherein during forming the plurality of micro-lenses, the bias power is set in a range of 100 W to 600 W.

### Claim 6 (depends on 1)

The method of claim 1, wherein forming the mask pattern comprises performing a photolithography process with respect to the photoresist layer.

### Claim 7

A reaction ion etching apparatus comprising:
a chamber for receiving a substrate;
an antenna provided over an upper portion of the chamber;
an electrode provided in a lower portion of the chamber;
a source power unit for supplying a first power to the antenna; and
a bias power unit for supplying a second power to the electrode.

### Claim 8 (depends on 7)

The reaction ion etching apparatus of claim 7, wherein the antenna comprises at least one conductive pipe.

### Claim 9 (depends on 7)

The reaction ion etching apparatus of claim 7, wherein the antenna comprises at a plurality of conductive pipes connected to each other in parallel.

### Claim 10 (depends on 8)

The reaction ion etching apparatus of claim 8, further comprising a ceramic window provided in a surface wall of the chamber, wherein the antenna is provided over the ceramic window.

### Claim 11 (depends on 7)

The reaction ion etching apparatus of claim 7, wherein the first power and the second power have a ratio of 2.5:1 to 3.5:1.

### Claim 12 (depends on 7)

The reaction ion etching apparatus of claim 7, wherein the first power is in a range of about 300 W to about 1800 W band the second power is in a range of about 100 W to about 600 W.

### Claim 13 (depends on 7)

The reaction ion etching apparatus of claim 7, further comprising a gas supply unit for supplying a gas for generating plasma in the chamber.

### Claim 14 (depends on 13)

The reaction ion etching apparatus of claim 13, wherein the gas supply unit supplies Ar in a range of 300 sccm to 500 sccm, BCl3 in a range of 40 sccm to 70 sccm, and Cl2 in a range of 20 sccm to 35 sccm.

### Claim 15 (depends on 7)

The reaction ion etching apparatus of claim 7, wherein the chamber has an internal pressure in a range of 1 mtorr to 3 mtorr.

### Claim 16

A method for forming a micro-lens comprising:
providing a sapphire substrate on a support in a chamber; and then
coating a photoresist layer on a sapphire substrate; and then
forming a mask pattern on the sapphire substrate; and then
performing a reaction ion etching process on the sapphire substrate while maintaining the support at a temperature in range of −15° C. to −25° C. to form a micro-lens composed of sapphire.

### Claim 17 (depends on 16)

The method of claim 16, wherein performing the reaction ion etching process comprises supplying a source power to the chamber and a bias power to the support at a ratio of 2.5:1 to 3.5:1.

### Claim 18 (depends on 16)

The method of claim 16, wherein performing the reaction ion etching process comprises supplying a source power to the chamber in a range of about 300 W to about 1800 W and a bias power to the support in a range of about 100 W to about 600 W.

### Claim 19 (depends on 16)

The method of claim 16, wherein performing the reaction ion etching process comprises supplying Ar in a range of 300 sccm to 500 sccm, BCl3 in a range of 40 sccm to 70 sccm, and Cl2 in a range of 20 sccm to 35 sccm.

### Claim 20 (depends on 19)

The method of claim 19, wherein the supply ratio of BCl3 and Cl2 is 1.75:1 to 2.25:1.