# US 2008/0290035 A1 · Method and Sorbant for Removing Contaminates From Water

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0290035 A1
- Document ID: US20080290035A1
- Status: Published application
- Kind: A1
- Application number: 12/097,281
- Filed: 2006-02-02
- Published: 2008-11-27
- Earliest claimed: 2006-02-02
- Inventors: Frederick W. Vance; Robert E. Reim
- Web page: https://patentgrep.com/patent/US20080290035A1

## CPC

- B01J 20/06: comprising oxides or hydroxides of metals not provided for in group B01J20/04
- B01J 20/045: {containing sulfur, e.g. sulfates, thiosulfates, gypsum}
- B01J 20/28004: {Sorbent size or size distribution, e.g. particle size}
- B01J 20/28016: {Particle form}
- B01J 20/2803: {Sorbents comprising a binder, e.g. for forming aggregated, agglomerated or granulated products}
- B01J 20/3021: {Milling, crushing or grinding}
- B01J 20/3042: {Use of binding agents; addition of materials ameliorating the mechanical properties of the produced sorbent}
- C02F 1/281: {using inorganic sorbents}
- B01J 2220/42: Materials comprising a mixture of inorganic materials (materials coated or impregnated on a carrier B01J20/32)
- C02F 2101/103: {Arsenic compounds}
- C02F 2101/20: Heavy metals or heavy metal compounds
- C02F 2101/22: Chromium or chromium compounds, e.g. chromates
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)

## Abstract

A method for removing dissolved contaminants, such as arsenate, from water by the step of contacting a sorbant with the water, the sorbant comprising more than ten weight percent of an oxide of titanium and more than one tenth weight percent of a sulfate salt, such as calcium sulfate, having a solubility in water at room temperature of less than 0.5 grams per liter of water, wherein the oxide of titanium is primarily titanium dioxide.

## Claims

### Claim 1

A method for removing dissolved contaminants from water, comprising the step of contacting a sorbant with the water, the sorbant comprising more than twenty weight percent titanium on an elemental analysis basis and more than 2 weight percent of a sulfate salt having a solubility in water at room temperature of less than 0.5 grams per liter of water, wherein the oxide of titanium is primarily titanium dioxide.

### Claim at position 2

2-3. (canceled)

### Claim 4 (depends on 1)

The method of claim 1, wherein the sorbant comprises more than 5 percent by weight of the sulfate salt.

### Claim 5 (depends on 1)

The method of claim 1, wherein the sorbant comprises more than 10 percent by weight of the sulfate salt.

### Claim 6 (depends on 2)

The method of claim 2, wherein the sulfate salt is a calcium sulfate salt.

### Claim 7 (depends on 6)

The method of claim 6, wherein the sorbant comprises less than 5% calcium on an elemental analysis basis by weight.

### Claim at position 7

8-18. (canceled)

### Claim 19 (depends on 1)

The method of claim 1, wherein the sorbant comprises more than forty weight percent titanium on an elemental analysis basis, more than one weight percent sulfur on an elemental analysis basis, and less than five weight percent calcium on an elemental analysis basis.

### Claim 20 (depends on 19)

The method of claim 19, wherein the sorbant comprises more than two weight percent sulfur on an elemental analysis basis.

### Claim at position 10

21-23. (canceled)

### Claim 24

A sorbant comprising more than twenty weight percent titanium on an elemental analysis basis, and more than 2 weight percent of a sulfate salt having a solubility in water at room temperature of less than 0.5 grams per liter of water, wherein the oxide of titanium is primarily titanium dioxide.

### Claim at position 12

25-29. (canceled)

### Claim 30 (depends on 1)

The method of claim 1 wherein the sorbant is formed by adding lime and water to uncalcined titanium dioxide.

### Claim 31 (depends on 1)

The method of claim 1 where the step of contacting the sorbant with water comprises flowing water through a bed of the sorbant.

### Claim 32 (depends on 24)

The sorbant of claim 24 comprising more than 5 weight percent of the sulfate salt.

### Claim 33 (depends on 24)

The sorbant of claim 24 comprising more than 10 weight percent of the sulfate salt.

### Claim 34 (depends on 24)

The sorbant of claim 24 wherein the sulfate salt comprises calcium sulfate.

### Claim 35 (depends on 24)

The sorbant of claim 24 comprising less than five weight percent calcium on an elemental analysis basis.

### Claim 36 (depends on 24)

The sorbant of claim 24 comprising more than forty weight percent titanium on an elemental analysis basis, more than one weight percent sulfur on an elemental analysis basis, and less than five weight percent calcium on an elemental analysis basis.

### Claim 37 (depends on 36)

The sorbant of claim 36 comprising more than two weight percent sulfur on an elemental analysis basis.