# US 2008/0289726 A1 · Cold rolled, dual phase, steel sheet and method of manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0289726 A1
- Document ID: US20080289726A1
- Status: Published application
- Kind: A1
- Application number: 12/180,861
- Filed: 2008-07-28
- Published: 2008-11-27
- Earliest claimed: 2004-11-24
- Assignees: Nucor Corporation
- Inventors: Weiping Sun
- Web page: https://patentgrep.com/patent/US20080289726A1

## CPC

- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/06: containing aluminium
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A steel sheet having (a) a dual phase microstructure with a martensite phase and a ferrite phase and (b) a composition containing by percent weight: 0.01% to 0.2% C; 0.3% to 3% Mn; 0.05% to 2% Si; 0.1% to 2% Cr; 0.01% to 0.10% Al; and 0.0005% to 0.01% Ca, with the balance of the composition being iron and incidental ingredients. Also, the steel sheet is made by a batch annealing method, and has a tensile strength of at least approximately 400 MPa and an n-value of at least approximately 0.175.

## Claims

### Claim 1

A steel sheet comprising:
(a) a dual phase microstructure comprising a martensite phase up to about 35% by volume embedded in a ferrite matrix phase before cold rolling and batch annealing;
(b) a composition comprising:
carbon in a range from about 0.01% by weight to about 0.2% by weight,
manganese in a range from about 0.3% by weight to about 3% by weight,
silicon in a range from about 0.05% by weight to about 2% by weight,
chromium in a range from about 0.1% by weight to about 2% by weight,
aluminum in a range from about 0.01% by weight to about 0.10% by weight, and
calcium in a range from about 0.0005% by weight to about 0.01% by weight,
with the balance of the composition comprising iron and incidental ingredients;
and
(c) properties comprising a tensile strength of at least about 400 MPa and an n-value of at least about 0.175 after cold rolling and batch annealing lower than about the Ac1 temperature.

### Claim 2 (depends on 1)

The steel sheet of claim 1, wherein the properties comprise a tensile strength of about least about 450 MPa, and an n-value of at least about 0.18.

### Claim 3 (depends on 1)

The steel sheet of claim 1, wherein the martensite phase comprises from about 3% by volume to about 30% by volume of the microstructure.

### Claim 4 (depends on 1)

The steel sheet of claim 1, wherein the composition further comprises one or more of titanium in an amount up to about 0.2% by weight; vanadium in an amount up to about 0.2% by weight; niobium in an amount up to about 0.2% by weight; boron in an amount up to about 0.008% by weight; molybdenum in an amount up to about 0.8% by weight; copper in an amount up to about 0.8% by weight; nickel in an amount up to about 0.8% by weight; phosphorous in an amount up to about 0.1% by weight; sulfur in an amount up to about 0.03% by weight; and nitrogen in an amount up to about 0.02% by weight.

### Claim 5 (depends on 1)

The steel sheet of claim 1, wherein the steel sheet further comprises one or both of a zinc coating or a zinc alloy coating.

### Claim 6 (depends on 1)

The steel sheet of claim 1, wherein the carbon ranges from about 0.02% to about 0.12% by weight, the manganese ranges from about 0.5% to about 2.5% by weight, the silicon ranges from about 0.08% to about 1.5% by weight, the chromium ranges from about 0.2% to about 1.5% by weight, the aluminum ranges from about 0.015% to about 0.09% by weight, the calcium ranges from about 0.0008% to about 0.009% by weight, or a combination thereof.

### Claim 7 (depends on 6)

The steel sheet of claim 6, wherein the carbon ranges from about 0.03% to about 0.1% by weight, the manganese ranges from about 0.5% to about 2% by weight, the silicon ranges from about 0.1% to about 1.2% by weight, the chromium ranges from about 0.3% to about 1.2% by weight, the aluminum ranges from about 0.02% to about 0.08% by weight, the calcium ranges from about 0.001% to about 0.008% by weight, or a combination thereof.

### Claim 8

A steel sheet comprising:
(a) a dual phase microstructure comprising a martensite phase and a ferrite phase;
(b) a composition comprising:
carbon in a range from about 0.01% by weight to about 0.2% by weight,
manganese in a range from about 0.3% by weight to about 3% by weight,
silicon in a range from about 0.05% by weight to about 2% by weight,
chromium in a range from about 0.1% by weight to about 2% by weight,
aluminum in a range from about 0.01% by weight to about 0.10% by weight, and
calcium in a range from about 0.0005% by weight to about 0.01% by weight,
with the balance of said composition comprising iron and incidental ingredients;
and
(c) properties comprising a tensile strength of at least about 400 MPa and an n-value of at least about 0.175;
and
wherein the steel sheet is made by a batch annealing method comprising:
(I) hot rolling a steel slab having said composition into a hot band and complete the hot rolling process at a temperature in a range between about (Ar3-60)° C. and about 980° C. (about 1796° F.);
(II) cooling the hot band at a mean rate of at least about 5° C./s (about 9° F./s) to a temperature not higher than about 750° C. (about 1382° F.) obtaining a steel sheet comprising a dual phase microstructure comprising a martensite phase up to about 35% by volume and a ferrite phase at least 65% by volume;
(III) coiling the cooled band to form a coil;
(IV) cold rolling the coil to a desired steel sheet thickness, with a total reduction of at least about 35%;
(V) annealing the cold rolled steel sheet in a batch furnace at a temperature higher than about 500° C. (about 932° F.) but lower than about the Ac1 temperature for longer than about 60 minutes; and
(VI) cooling the annealed steel sheet to a temperature lower than about 400° C. (about 752° F.).

### Claim 9 (depends on 8)

The steel sheet of claim 8, wherein the properties comprise a tensile strength of about least about 450 MPa, and an n-value of at least about 0.18.

### Claim 10 (depends on 8)

The steel sheet of claim 8, wherein the martensite phase comprises from about 3% by volume to about 30% by volume of the microstructure.

### Claim 11 (depends on 8)

The steel sheet of claim 8, wherein the composition further comprises one or more of titanium in an amount up to about 0.2% by weight; vanadium in an amount up to about 0.2% by weight; niobium in an amount up to about 0.2% by weight; boron in an amount up to about 0.008% by weight; molybdenum in an amount up to about 0.8% by weight; copper in an amount up to about 0.8% by weight; nickel in an amount up to about 0.8% by weight; phosphorous in an amount up to about 0.1% by weight; sulfur in an amount up to about 0.03% by weight; or nitrogen in an amount up to about 0.02% by weight.

### Claim 12 (depends on 8)

The steel sheet of claim 8, wherein the steel sheet further comprises one or both of a zinc coating or a zinc alloy coating.

### Claim 13 (depends on 8)

The steel sheet of claim 8, wherein the carbon ranges from about 0.02% to about 0.12% by weight, the manganese ranges from about 0.5% to about 2.5% by weight, the silicon ranges from about 0.08% to about 1.5% by weight, the chromium ranges from about 0.2% to about 1.5% by weight, the aluminum ranges from about 0.015% to about 0.09% by weight, the calcium ranges from about 0.0008% to about 0.009% by weight, or a combination thereof.

### Claim 14 (depends on 13)

The steel sheet of claim 13, wherein the carbon ranges from about 0.03% to about 0.1% by weight, the manganese ranges from about 0.5% to about 2% by weight, the silicon ranges from about 0.1% to about 1.2% by weight, the chromium ranges from about 0.3% to about 1.2% by weight, the aluminum ranges from about 0.02% to about 0.08% by weight, the calcium ranges from about 0.001% to about 0.008% by weight, or a combination thereof.

### Claim 15 (depends on 8)

The steel sheet of claim 8, wherein complete the hot rolling process at a temperature in a range between about (Ar3-30)° C. and about 950° C. (about 1742° F.).

### Claim 16 (depends on 8)

The steel sheet of claim 8, wherein cooling the hot band is at a mean rate of at least about 10° C./s (about 18° F./s) to a temperature not higher than about 650° C. (about 1202° F.).

### Claim 17 (depends on 8)

The steel sheet of claim 8, wherein the coil is pickled.

### Claim 18 (depends on 8)

The steel sheet of claim 8, wherein the total reduction ranges from about 45% to about 85%.

### Claim 19 (depends on 8)

The steel sheet of claim 8, wherein the annealing is a temperature higher than about 500° C. (about 932° F.) and lower than about the Ac1 temperature in the subcritical temperature region for a time from about 180 minutes to about 7 days.

### Claim 20 (depends on 8)

The steel sheet of claim 8, wherein cooling the annealed sheet is to a temperature from about 300° C. (about 572° F.) to about ambient temperature.

### Claim 21

A steel sheet comprising:
(a) a dual phase microstructure comprising a martensite phase embedded in a ferrite matrix phase, wherein the martensite phase comprises from about 3% by volume to about 35% by volume of the microstructure and the ferrite phase comprises at least 65% by volume before cold rolling and batch annealing;
(b) a composition comprising:
carbon in a range from about 0.01% by weight to about 0.2% by weight,
manganese in a range from about 0.3% by weight to about 3% by weight,
silicon in a range from about 0.05% by weight to about 2% by weight,
chromium in a range from about 0.1% by weight to about 2% by weight,
aluminum in a range from about 0.01% by weight to about 0.10% by weight, and
calcium in a range from about 0.0005% by weight to about 0.01% by weight,
with the balance of the composition comprising iron and incidental ingredients;
and
(c) properties comprising a tensile strength of at least about 400 MPa, and an n-value of at least about 0.175 after cold rolling and batch annealing lower than about the Ac1 temperature.

### Claim 22

A steel sheet comprising:
(a) a dual phase microstructure comprising a martensite phase embedded in a ferrite matrix phase, wherein the martensite phase comprises from about 3% by volume to about 35% by volume and the ferrite phase comprises at least 65% by volume of the microstructure before cold rolling and batch annealing;
(b) a composition comprising:
carbon in a range from about 0.01% by weight to about 0.2% by weight,
manganese in a range from about 0.3% by weight to about 3% by weight,
silicon in a range from about 0.05% by weight to about 2% by weight,
chromium in a range from about 0.1% by weight to about 2% by weight,
aluminum in a range from about 0.01% by weight to about 0.10% by weight, and
calcium in a range from about 0.0005% by weight to about 0.01% by weight,
with the balance of said composition comprising iron and incidental ingredients;
and
(c) properties comprising a tensile strength of at least about 400 MPa, and an n-value of at least about 0.175 after cold rolling and batch annealing lower than about the Ac1 temperature;
and
wherein the steel sheet is made by a batch annealing method comprising:
(I) hot rolling a steel slab having said composition into a hot band and complete the hot rolling process at a temperature in a range between about (Ar3-30)° C. and about 950° C. (about 1742° F.);
(II) cooling the hot band at a mean rate of at least about 10° C./s (about 18° F./s) to a temperature not higher than about 650° C. (about 1202° F.);
(III) coiling the cooled band to form a coil;
(IV) cold rolling the coil at about ambient temperature to a desired steel sheet thickness, with a total reduction ranging from about 45% to about 85%;
(V) annealing the cold rolled steel sheet in a batch furnace to a temperature higher than about 650° C. (about 1202° F.) but lower than about the Ac1 temperature for longer than about 60 minutes; and
(VI) cooling the annealed steel sheet to a temperature lower than about 300 ° C. (about 572° F.).