# US 2008/0287699 A1 · Process for Hydrosilylation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0287699 A1
- Document ID: US20080287699A1
- Status: Published application
- Kind: A1
- Application number: 12/091,780
- Filed: 2006-10-13
- Published: 2008-11-20
- Earliest claimed: 2005-10-27
- Assignees: Wacker Chemie AG
- Inventors: Gilbert Geisberger; Frank Baumann
- Web page: https://patentgrep.com/patent/US20080287699A1

## CPC

- C08K 9/06: with silicon-containing compounds
- C08K 5/34: Heterocyclic compounds having nitrogen in the ring
- C08K 5/5415: containing at least one Si—O bond
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

Compounds containing unsaturated carbon-carbon bonds are hydrosilylated with H-silanes or H-siloxanes in the presence of a noble metal catalyst, wherein the water content of the reaction mixture is less than 500 ppm and the noble metal catalyst is supplied as a liquid, and is present in an amount of not more than 50 ppm.

## Claims

### Claim at position 1

-12. (canceled)

### Claim 13

A process for hydrosilylating compounds (A) containing carbon-carbon double bonds or carbon-carbon triple bonds with organosilicon compounds (B) having silicon-bonded hydrogen by catalysis with a compound or complex of a noble metal of transition group VIII as a catalyst (C), comprising desiccating starting materials with a desiccant selected from the group consisting of calcium chloride, magnesium sulfate, sodium sulfate, metals, molecular sieves or H-free chlorosilanes, such that the water content of the reaction mixture is not more than 500 ppm and the catalyst is added in liquid form to the reaction mixture, with the proviso that the noble metal concentration is not more than 50 ppm based on the entire reaction composition.

### Claim 14 (depends on 13)

The process of claim 13, wherein the noble metal catalyst concentration is from 5 to 25 ppm based on the entire reaction composition.

### Claim 15 (depends on 13)

The process of claim 13, wherein the water content of the reaction mixture is not more than 100 ppm.

### Claim 16 (depends on 14)

The process of claim 14, wherein the water content of the reaction mixture is not more than 100 ppm.

### Claim 17 (depends on 13)

The process of claim 13, wherein the catalyst (C) comprises one or more compounds or complexes of a noble metal selected from the group consisting of platinum, ruthenium, iridium, rhodium and palladium.

### Claim 18 (depends on 13)

The process of claim 13, wherein the catalyst (C) used comprises at least one platinum-olefin complex or platinum-divinyltetramethyldisiloxane complex.

### Claim 19 (depends on 13)

The process of claim 13, wherein the process is carried out at a temperature of from 60 to 140° C.

### Claim 20 (depends on 13)

The process of claim 13, wherein the process is carried out at a pressure of from 1 to 20 bar.

### Claim 21 (depends on 13)

The process of claim 13, wherein organosilicon compounds with silicon-bonded hydrogen (B) comprise compounds containing units of the formula (II)
R2cHdSiO(4-c-d)/2 (II)
where
R2 are identical or different monovalent radicals selected from the group consisting of —F, —Cl, —Br, —CN, —SCN, —NCO, alkoxy radicals, and SiC-bonded, substituted or unsubstituted hydrocarbon radicals optionally interrupted by oxygen atoms or a —C(O)— group,
c is 0, 1, 2 or 3 and d is 0, 1 or 2,
with the proviso that the sum of c+d is ≦ and at least one Si-bonded hydrogen atom per molecule is present.

### Claim 22 (depends on 13)

The process of claim 13, wherein organosilicon compounds having silicon-bonded hydrogen (B) comprise silanes of the formula (III)
R3eHfSi (III)
where
R3 are identical or different monovalent radicals selected from the group consisting of —F, —Cl, —Br, —CN, —SCN, —NCO, alkoxy radicals, and Si—C-bonded, substituted or unsubstituted hydrocarbon radicals optionally interrupted by oxygen atoms or the —C(O)— group,
e is 1, 2 or 3 and
f is 1, 2 or 3,
with the proviso that the sum of e+f=4.

### Claim 23 (depends on 13)

The process of claim 13, wherein the desiccant comprises silicon tetrachloride.

### Claim 24

A process for hydrosilylating compounds (A) containing carbon-carbon double bonds or carbon-carbon triple bonds with organosilicon compounds (B) having silicon-bonded hydrogen by catalysis with a compound or complex of a noble metal of transition group VIII as a catalyst (C), comprising desiccating starting materials (A) and/or (B), and desiccating the such that the water content of the reaction mixture is not more than 500 ppm and the catalyst is added in liquid form to the reaction mixture, with the proviso that the noble metal concentration is not more than 50 ppm based on the entire reaction composition.