# US 2008/0287598 A1 · Method of preparing aramid polymers incorporating carbon nanotubes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0287598 A1
- Document ID: US20080287598A1
- Status: Published application
- Kind: A1
- Application number: 11/605,541
- Filed: 2006-11-29
- Published: 2008-11-20
- Earliest claimed: 2006-11-29
- Inventors: Kiu-Seung Lee
- Web page: https://patentgrep.com/patent/US20080287598A1

## CPC

- C08J 5/005: {Reinforced macromolecular compounds with nanosized materials, e.g. nanoparticles, nanofibres, nanotubes, nanowires, nanorods or nanolayered materials}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- C08K 3/041: {Carbon nanotubes}
- C08J 2377/10: Polyamides derived from aromatically bound amino and carboxyl groups of amino carboxylic acids or of polyamines and polycarboxylic acids
- C08K 2201/004: Additives being defined by their length
- C08K 2201/016: Additives defined by their aspect ratio
- C08L 77/06: Polyamides derived from polyamines and polycarboxylic acids (C08L77/10 takes precedence)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The invention relates to a method of preparing an aramid polymer solution having carbon nanotubes dispersed therein, providing a first dispersion comprising carbon nanotubes and a carrier polymer in a first solvent; providing a first solution comprising an aromatic diamine having an electron affinity lower than that of the carrier polymer and, optionally, a second solvent; adding the first solution to the first dispersion to form a second dispersion; adding an aromatic diacid or aromatic diacid chloride to the second dispersion; polymerizing the aromatic diacid or aromatic diacid chloride with the aromatic diamine to form a carbon nanotube containing aramid polymer or co-polymer in a first aramid solution; isolating the carbon nanotube-containing aramid polymer or co-polymer; and dissolving the carbon nanotube-containing aramid polymer or co-polymer in a third solvent to form a second aramid solution.

## Claims

### Claim 1

A method of preparing an aramid polymer solution comprising:
providing a first dispersion comprising carbon nanotubes and a carrier polymer in a first solvent;
providing a first solution comprising an aromatic diamine having an electron affinity lower than that of the carrier polymer and, optionally, a second solvent;
adding the first solution to the first dispersion to form a second dispersion;
adding an aromatic diacid or aromatic diacid chloride to the second dispersion;
polymerizing the aromatic diacid or aromatic diacid chloride with the aromatic diamine to form a carbon nanotube containing aramid polymer or co-polymer in a first aramid solution;
isolating the carbon nanotube-containing aramid polymer or co-polymer;
dissolving the carbon nanotube-containing aramid polymer or co-polymer in a third solvent to form a second aramid solution.

### Claim 2 (depends on 1)

The method of claim 1, wherein the aromatic diamine comprises a diamine selected from the list consisting of para-phenylene diamine, meta-phenylene diamine, 4,4′diphenyldiamine, 3,3′diphenyldiamine, 3,4′-diphenyldiamine, 4-4′-oxydiphenyldiamine, 3,3′-oxydiphenyldiamine, 3,4′-oxydiphenyldiamine, and 4,4′-sulfonyldiphenyldiamine and mixtures thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein the aromatic diacid or diacid chloride comprises at least one of terephthalic acid, isophthalic acid, 2,6-naphthalenedicarboxylic acid, 2,6-naphthalenedicarboxylic acid chloride, isophthaloyl chloride, terephthaloyl chloride, or compounds of the formula:
where Z is OH or Cl and Y is —O— or —SO2—.

### Claim 4 (depends on 3)

The method of claim 3 wherein the diacid or diacid chloride comprises at least one of terephthalic acid, isophthalic acid, 2,6-naphthalenedicarboxylic acid, 4,4′-oxydibenzoic acid, 3,3′-oxydibenzoic acid, 4,4′-sulfonyldibenzoic acid, 3,3′-sulfonyldibenzoic acid, 3,4′-sulfonyldibenzoic acid, 4.4′-dibenzoic acid, 3,3′-dibenzoic acid, 3,4′-dibenzoic acid, 2,6-naphthalenedicarboxylic acid chloride, terephthaloyl chloride, isophthaloyl chloride, 4,4′-oxydibenzoyl chloride, 3,3′-oxydibenzoyl chloride, 4,4′-sulfonyldibenzoyl chloride, 3,3′-sulfonyldibenzoyl chloride, 3,4′-sulfonyldibenzoyl chloride, 4,4′-dibenzoyl chloride, 3,3′-dibenzoyl chloride, and 3,4′-dibenzoyl chloride.

### Claim 5 (depends on 1)

The method of claim 1, wherein the aramid polymer or co-polymer comprises para-phenylene diamine.

### Claim 6 (depends on 1)

The method of claim 1, wherein the carbon nanotubes comprise 50 to 100 percent multi-walled carbon nanotubes.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first and second solvents are N-methyl-2-pyrrolidinone, N,N-dimethylacetamide, or N,N,N′,N′-tetramethylurea.

### Claim 8 (depends on 1)

The method of claim 1, wherein the nanotubes incorporated into the polymer have an average aspect ratio greater than 100:1.

### Claim 9 (depends on 1)

The method of claim 1, wherein the average length of the carbon nanotubes is greater than 50 nanometers.

### Claim 10 (depends on 1)

The method of claim 1, wherein the carbon nanotubes are present in a concentration less than the percolation threshold.

### Claim 11 (depends on 1)

The method of claim 1, wherein the third solvent is sulfuric acid or methanesulfonic acid.

### Claim 12 (depends on 1)

The method of claim 1, wherein the first and second solvents are n-methyl-2-pyrrolidinone and the third solvent is sulfuric acid.

### Claim 13 (depends on 1)

The method of claim 1 wherein the aramid is poly(p-phenylene terephthalamide).

### Claim 14 (depends on 1)

A composition made by the method of claim 1.

### Claim 15 (depends on 14)

The composition of claim 14 wherein the aramid is poly(p-phenylene terephthalamide).

### Claim 16 (depends on 14)

The composition of claim 14 wherein the aromatic diacid is terephthalic acid.

### Claim 17 (depends on 14)

The composition of claim 14 wherein the aromatic diamine is para-phenylene diamine.

### Claim 18 (depends on 14)

The composition of claim 14 wherein the aromatic diacid is terephthalic acid and the aromatic diamine is para-phenylene diamine.

### Claim 19 (depends on 14)

The composition of claim 14 wherein the carbon nanotubes have an average aspect ratio greater than 100:1

### Claim 20 (depends on 14)

An article comprising a composition of claim 14.