# US 2008/0286949 A1 · Method of Forming a Rare-Earth Dielectric Layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0286949 A1
- Document ID: US20080286949A1
- Status: Published application
- Kind: A1
- Application number: 12/111,568
- Filed: 2008-04-29
- Published: 2008-11-20
- Earliest claimed: 2005-10-19
- Assignees: Translucent Photonics, Inc.
- Inventors: Petar Atanackovic
- Web page: https://patentgrep.com/patent/US20080286949A1

## CPC

- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- C30B 23/02: Epitaxial-layer growth
- C30B 29/16: Oxides
- H10D 64/01342: {by deposition, e.g. evaporation, ALD or laser deposition (H10D64/01344 takes precedence)}
- H10D 64/693: {the insulator comprising nitrogen, e.g. nitrides, oxynitrides or nitrogen-doped materials}
- H10P 14/69396: {the material containing at least one rare earth metal element, e.g. oxides of lanthanides, scandium or yttrium}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Methods for forming compositions comprising a single-phase rare-earth dielectric disposed on a substrate are disclosed. In some embodiments, the method forms a semiconductor-on-insulator structure. Compositions and structures that are formed via the method provide the basis for forming high-performance devices and circuits.

## Claims

### Claim at position 1

1-40. (canceled)

### Claim 41

A method comprising forming a first dielectric layer on a substrate, wherein said first dielectric layer comprises a rare-earth metal, and wherein said first dielectric layer is substantially alkaline earth metal-free, and further wherein said first dielectric layer has a substantially single-phase crystal structure.

### Claim 42 (depends on 41)

The method of claim 41 wherein said first dielectric layer is formed using atomic layer epitaxy.

### Claim 43 (depends on 41)

The method of claim 41 further comprising forming a template layer on said substrate prior to forming said first dielectric layer, wherein said template layer provides an energetically-favorable surface for the bonding of one of either cations or anions.

### Claim 44 (depends on 41)

The method of claim 41 further comprising forming a template layer on said substrate prior to forming said first dielectric layer, wherein said template layer changes a surface of said substrate from non-polar to polar.

### Claim 45 (depends on 41)

The method of claim 41 further comprising forming a template layer on said substrate prior to forming said first dielectric layer, wherein said template layer comprises an anion-rich/cation-rich superlattice structure.

### Claim 46 (depends on 41)

The method of claim 41 further comprising forming a template layer on said substrate prior to forming said first dielectric layer, wherein said template layer provides a means of ordering bixbyite oxygen vacancies in said first dielectric layer.

### Claim 47 (depends on 41)

The method of claim 41 further comprising providing said substrate, wherein said substrate comprises a silicon wafer, and wherein said silicon wafer has a crystal orientation selected from the group consisting of <111>, <100>, and <011>.

### Claim 48 (depends on 47)

The method of claim 47 further comprising providing said silicon wafer, wherein said silicon wafer is miscut from its crystal orientation by an angle that has a value within the range of 0 to 20 degrees.

### Claim 49 (depends on 1)

The method of claim 1 further comprising forming a active layer, wherein said active layer has a substantially single-phase crystal structure, and wherein said active layer comprises a material selected from the group consisting of silicon, germanium, silicon-germanium, gallium arsenide, indium phosphide, and silicon carbide.

### Claim 50 (depends on 49)

The method of claim 49 wherein said active layer is formed using atomic layer epitaxy.

### Claim 51 (depends on 49)

The method of claim 49 further comprising forming a wetting layer for changing a surface of said first dielectric layer from polar to non-polar.

### Claim 52 (depends on 49)

The method of claim 49 further comprising forming a wetting layer for providing a surface having surface energy greater than the sum of (1) the surface energy of said active layer, and (2) the interface energy, and wherein said wetting layer supports two-dimensional, layer-by-layer growth of said active layer.

### Claim 53 (depends on 49)

The method of claim 49 further comprising forming a wetting layer comprising a material selected from the group consisting of ytterbium monoxide and erbium nitride.

### Claim 54 (depends on 49)

The method of claim 49 further comprising forming a second dielectric layer, wherein said second dielectric layer comprises a rare-earth metal, and wherein said second dielectric layer has a substantially single-phase crystal structure, and further wherein said active layer is interposed between said first dielectric layer and said second dielectric layer.

### Claim 55 (depends on 54)

The method of claim 54 further comprising forming a template layer on said active layer prior to forming said second dielectric layer, wherein said template layer supports formation of said second dielectric layer.

### Claim 56

A method comprising forming a first dielectric layer on a substrate, wherein said first dielectric layer comprises a rare-earth metal, and wherein said first dielectric layer is substantially alkaline earth metal-free, and further wherein said rare-earth metal forms a cation having a radius less than 0.93 angstroms, and further wherein the crystal structure of said first dielectric layer is substantially single-phase.

### Claim 57 (depends on 56)

The method of claim 56 further comprising forming said first dielectric layer with a crystal structure that is bixbyite.

### Claim 58 (depends on 56)

The method of claim 56 further comprising forming said first dielectric layer with a crystal structure that is one of oxygen-rich bixbyite and oxygen-poor bixbyite.

### Claim 59 (depends on 56)

The method of claim 56 further comprising forming an active layer, wherein the crystal structure of said active layer is substantially single-phase, and wherein said active layer comprises a material selected from the group consisting of silicon, germanium, silicon-germanium, gallium arsenide, indium phosphide, and silicon carbide.

### Claim 60 (depends on 59)

The method of claim 59 further comprising a second dielectric layer comprising a rare-earth metal, wherein the crystal structure of said second dielectric layer is substantially single-phase.

### Claim 61 (depends on 60)

The method of claim 60 wherein said first dielectric layer, said active layer, and second dielectric layer are formed using atomic layer epitaxy.

### Claim 62 (depends on 56)

The method of claim 56 further comprising forming a rare-earth nitride layer, wherein the crystal structure of said rare-earth nitride layer is substantially single-phase.

### Claim 63 (depends on 56)

The method of claim 56 wherein said substrate comprises a material selected from the group consisting of silicon, germanium, silicon-germanium, gallium arsenide, indium phosphide, and silicon carbide.

### Claim 64 (depends on 56)

The method of claim 56 wherein said rare-earth metal is selected from the group consisting of erbium, ytterbium, dysprosium, holmium, thulium, and lutetium.

### Claim 65

A method comprising forming a first dielectric layer on a substrate, wherein said first dielectric layer comprises a rare-earth metal, and wherein said first dielectric layer is substantially alkaline earth metal-free, and further wherein said rare-earth metal has an atomic number greater than or equal to 66, and further wherein the crystal structure of said first dielectric layer is substantially single-phase.

### Claim 66 (depends on 65)

The method of claim 65 further comprising forming said first dielectric layer with a crystal structure that is bixbyite.

### Claim 67 (depends on 65)

The method of claim 65 further comprising forming said first dielectric layer with a crystal structure that is one of oxygen-rich bixbyite and oxygen-poor bixbyite.

### Claim 68 (depends on 65)

The method of claim 65 further comprising forming said first dielectric layer such that said rare-earth metal is bonded in an ionization state that is triply ionized (3+).

### Claim 69 (depends on 65)

The method of claim 65 further comprising forming an active layer, wherein the crystal structure of said active layer is substantially single-phase, and wherein said active layer comprises a material selected from the group consisting of silicon, germanium, silicon-germanium, gallium arsenide, indium phosphide, and silicon carbide.

### Claim 70

A method comprising forming a first dielectric layer on a substrate, wherein said first dielectric layer comprises a rare-earth metal, and wherein said first dielectric layer is substantially alkaline earth metal-free, and wherein the crystal structure of said first dielectric layer is that of an oxygen-vacancy-derived fluorite crystal, and further wherein the crystal structure of said first dielectric layer is single-phase.

### Claim 71 (depends on 70)

The method of claim 70 further comprising forming said first dielectric layer such that said first dielectric layer comprises oxygen vacancies that are aligned in the <111> crystal plane.

### Claim 72 (depends on 70)

The method of claim 70 further comprising forming an active layer having a crystal structure that is substantially single-phase, wherein said active layer comprises a material selected from the group consisting of silicon, germanium, silicon-germanium, gallium arsenide, indium phosphide, and silicon carbide.

### Claim 73

A method comprising:
providing a substrate, wherein said substrate comprises a silicon wafer having crystal orientation that is selected from the group consisting of <001>, <111>, and <011>, and wherein said silicon wafer is miscut from its crystal orientation by an angle that has a value within the range of 0 to 20 degrees; and
forming a first dielectric layer, wherein said first dielectric layer comprises a dielectric comprising a rare-earth metal, and wherein said first dielectric layer is substantially alkaline earth metal-free, and further wherein said first dielectric layer has a crystal structure that is substantially that of an oxygen-vacancy-derived fluorite crystal.

### Claim 74 (depends on 73)

The method of claim 73 further comprising forming a superlattice layer, wherein said superlattice layer is interposed between said substrate and said first dielectric layer.

### Claim 75 (depends on 73)

The method of claim 73 further comprising forming an active layer having a crystal structure that is substantially single-phase, wherein said active layer comprises a material selected from the group consisting of silicon, germanium, silicon-germanium, gallium arsenide, indium phosphide, and silicon carbide.

### Claim 76 (depends on 73)

The method of claim 73 wherein said first dielectric layer and said semiconductor layer are formed using atomic layer epitaxy.

### Claim 77

A method comprising:
providing a substrate having a first surface that is non-polar;
forming a template layer for providing a second surface that is polar, wherein said template layer is formed using an epitaxial growth method; and
forming a first dielectric layer, wherein said first dielectric layer comprises a rare-earth metal, and further wherein said first dielectric layer has a substantially single-phase crystal structure.

### Claim 78 (depends on 77)

The method of claim 77 further comprising forming a wetting layer for providing a third surface that is non-polar, wherein said wetting layer is formed using an epitaxial growth method.

### Claim 79 (depends on 77)

The method of claim 77 further comprising forming an active layer having a crystal structure that is substantially single-phase, wherein said active layer comprises a material selected from the group consisting of silicon, germanium, silicon-germanium, gallium arsenide, indium phosphide, and silicon carbide.

### Claim 80 (depends on 79)

The method of claim 79 wherein said template layer, said first dielectric layer, said wetting layer, and said active layer are formed using atomic layer epitaxy.