# US 2008/0286908 A1 · Method of Producing a Semiconductor Element in a Substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0286908 A1
- Document ID: US20080286908A1
- Status: Published application
- Kind: A1
- Application number: 11/748,327
- Filed: 2007-05-14
- Published: 2008-11-20
- Earliest claimed: 2007-05-14
- Assignees: Infineon Technologies AG; Qimonda AG
- Inventors: Luis-Felipe Giles; Matthias Goldbach; Martin Bartels; Paul Kuepper
- Web page: https://patentgrep.com/patent/US20080286908A1

## CPC

- H10P 30/204: {into Group IV semiconductors}
- H10D 62/53: the imperfections being within the semiconductor body
- H10P 14/20: of semiconductor materials
- H10P 30/208: {of electrically inactive species}
- H10P 30/21: {of electrically active species}
- H10P 30/224: {of a cluster, e.g. using a gas cluster ion beam}
- H10P 30/225: {of a molecular ion, e.g. decaborane}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10P 95/405: {using cavities formed by hydrogen or noble gas ion implantation}
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/2926: {Crystal orientations}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3802: {Crystallisation or recrystallisation of non-monocrystalline semiconductor materials, e.g. regrowth}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of producing a semiconductor element in a substrate includes forming a plurality of micro-cavities in a substrate, creating an amorphization of the substrate to form crystallographic defects and a doping of the substrate with doping atoms, depositing an amorphous layer on top of the substrate, and annealing the substrate, such that at least a part of the crystallographic defects is eliminated using the micro-cavities. The semiconductor element is formed using the doping atoms.

## Claims

### Claim 1

A method of producing an integrated circuit, the method comprising:
forming a plurality of micro-cavities in a substrate;
creating an amorphization of the substrate to form crystallographic defects and a doping of the substrate with doping atoms;
depositing an amorphous layer over the substrate; and
annealing the substrate, such that at least a part of the crystallographic defects is eliminated using the micro-cavities;
wherein a semiconductor element is formed using the doping atoms.

### Claim 2 (depends on 1)

The method according to claim 1, wherein forming the plurality of micro-cavities comprises implanting ions into the substrate.

### Claim 3 (depends on 2)

The method according to claim 2, wherein implanting ions comprises implanting H2+-, He+-, F+-, Ne+-, Cl+-, or Ar+-ions.

### Claim 4 (depends on 2)

The method according to claim 2, wherein implanting ions comprises using an implantation dose of between approximately 1015 cm−2 and 1018 cm−2.

### Claim 5 (depends on 2)

The method according to claim 2, wherein implanting ions comprises implanting with an energy between 10 keV and 150 keV.

### Claim 6 (depends on 1)

The method according to claim 1, wherein annealing comprises annealing at a temperature lower than 650° C.

### Claim 7 (depends on 1)

The method according to claim 1, wherein creating the amorphization comprises amorphizing the substrate down to a depth lower than 500 nm.

### Claim 8 (depends on 1)

The method according to claim 1, wherein creating the amorphization of the substrate comprises using amorphization ions.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the amorphization ions comprise germanium ions and/or silicon ions.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the micro-cavities are near an interface between a crystalline region of the substrate and an amorphous region of the substrate formed by the amorphization of the substrate.

### Claim 11 (depends on 1)

The method according to claim 1, wherein creating the amorphization of the substrate to form a doping of the substrate comprises implanting one or more of boron atoms, phosphorus atoms, or arsenic atoms into the substrate.

### Claim 12 (depends on 11)

The method according to claim 11, wherein implanting comprises introducing boron ions into the substrate or introducing boron fluoride ions into the substrate or introducing boron clusters into the substrate.

### Claim 13 (depends on 1)

The method according to claim 1, wherein at least one region, within which region the doping atoms are implanted into the substrate, forms a shallow junction of the semiconductor element.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the semiconductor element comprises a transistor.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the semiconductor element comprises a field effect transistor.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the at least one region, within which region the doping atoms are implanted into the substrate, forms a source region or a drain region of the field effect transistor.

### Claim 17 (depends on 16)

The method according to claim 16,
wherein a first region, within which the doping atoms are implanted into the substrate, forms a source region of the field effect transistor; and
wherein a second region, within which the doping atoms are implanted into the substrate, forms a drain region of the field effect transistor.

### Claim 18 (depends on 1)

The method according to claim 1, wherein the substrate comprises a silicon substrate.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the substrate is a (100) silicon substrate or a (111) silicon substrate.

### Claim 20 (depends on 1)

The method according to claim 1, wherein depositing an amorphous layer comprises depositing at a temperature lower than 500° C.

### Claim 21 (depends on 1)

The method according to claim 1, wherein depositing of an amorphous layer comprises depositing silicon.

### Claim 22 (depends on 1)

The method according to claim 1, wherein depositing an amorphous layer comprises depositing the amorphous layer to a thickness between 5 nm and 100 nm.

### Claim 23 (depends on 1)

The method according to claim 1, further comprising performing a TEOS and a nitride spacer deposition after the annealing.

### Claim 24 (depends on 1)

The method according to claim 1, wherein creating an amorphization comprises forming a buried crystallographic defect layer near a region of the plurality of micro-cavities.

### Claim 25

A method of producing an integrated circuit, the method comprising:
forming a plurality of micro-cavities in a substrate;
creating an amorphization of the substrate to form crystallographic defects and a doping of the substrate with doping atoms; and
annealing the substrate at a temperature lower than 600° C., such that at least a part of the crystallographic defects is eliminated using the micro-cavities;
wherein the semiconductor element is formed using the doping atoms.

### Claim 26 (depends on 25)

The method according to claim 25, wherein forming the plurality of micro-cavities comprises implanting ions into the substrate.

### Claim 27 (depends on 25)

The method according to claim 25, wherein creating the amorphization of the substrate is performed such that the substrate is amorphized down to a depth lower than 500 nm.

### Claim 28 (depends on 25)

The method according to claim 25, wherein creating the amorphization of the substrate comprises using amorphization ions.

### Claim 29 (depends on 28)

The method according to claim 28, wherein the amorphization ions comprise germanium ions and/or silicon ions.

### Claim 30 (depends on 25)

The method according to claim 25, wherein creating the amorphization of the substrate to form the doping of the substrate comprises implanting one of boron atoms, phosphorous atoms, or arsenic atoms into the substrate.

### Claim 31 (depends on 25)

The method according to claim 25, wherein the implanting comprises introducing boron ions into the substrate or introducing boron fluoride ions into the substrate or introducing boron clusters into the substrate.

### Claim 32 (depends on 25)

The method according to claim 25, wherein at least one region, within which region the doping atoms are implanted into the substrate, forms a shallow junction of the semiconductor element.

### Claim 33 (depends on 25)

The method according to claim 25, wherein the semiconductor element comprises a transistor.

### Claim 34 (depends on 33)

The method according to claim 33, wherein the semiconductor element comprises a field effect transistor.

### Claim 35 (depends on 34)

The method according to claim 34, wherein at least one region, within which region the doping atoms are implanted into the substrate, forms a source region or a drain region of the field effect transistor.

### Claim 36 (depends on 35)

The method according to claim 35,
wherein a first region, within which the doping atoms are implanted into the substrate, forms a source region of the field effect transistor; and
wherein a second region, within which the doping atoms are implanted into the substrate, forms a drain region of the field effect transistor.

### Claim 37 (depends on 25)

The method according to claim 25, wherein the substrate is a silicon substrate.

### Claim 38 (depends on 25)

The method according to claim 25, further comprising depositing a TEOS and a nitride spacer after the annealing.

### Claim 39 (depends on 25)

The method according to claim 25, wherein the amorphization is performed such that a buried crystallographic defect layer near the region of the plurality of micro-cavities is formed.