# US 2008/0286703 A1 · Reducing Sulfur Gas Emissions Resulting from the Burning of Carbonaceous Fuels

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0286703 A1
- Document ID: US20080286703A1
- Status: Published application
- Kind: A1
- Application number: 11/631,046
- Filed: 2005-04-08
- Published: 2008-11-20
- Earliest claimed: 2004-06-28
- Assignees: Nox II International, Ltd.
- Inventors: Douglas C. Comrie; Vincent A. Vellella
- Web page: https://patentgrep.com/patent/US20080286703A1

## CPC

- C10L 10/00: Use of additives to fuels or fires for particular purposes (additives for liquid carbonaceous fuels characterised by their chemical nature C10L1/10; using binders for briquetting solid fuels C10L5/10; using additives to improve the combustion of solid fuels C10L9/10)
- B01D 53/501: {by treating the gases with a solution or a suspension of an alkali or earth-alkali or ammonium compound}
- B01D 53/508: {by treating the gases with solids}
- B01D 53/64: Heavy metals or compounds thereof, e.g. mercury
- C10L 9/10: by using additives
- C10L 10/02: for reducing smoke development
- C10L 10/04: for minimising corrosion or incrustation
- F23J 7/00: Arrangement of devices for supplying chemicals to fire
- F23K 1/00: Preparation of lump or pulverulent fuel in readiness for delivery to combustion apparatus
- B01D 2251/304: of sodium
- B01D 2251/306: of potassium
- B01D 2251/404: of calcium
- B01D 2255/2047: Magnesium
- B01D 2255/20738: Iron
- B01D 2257/302: Sulfur oxides
- B01D 2257/602: Mercury or mercury compounds
- F23K 2201/505: with additives
- C10L: FUELS NOT OTHERWISE PROVIDED FOR; NATURAL GAS; SYNTHETIC NATURAL GAS OBTAINED BY PROCESSES NOT COVERED BY SUBCLASSES C10G OR C10K; LIQUIFIED PETROLEUM GAS; USE OF ADDITIVES TO FUELS OR FIRES; FIRE-LIGHTERS
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- F23J: REMOVAL OR TREATMENT OF COMBUSTION PRODUCTS OR COMBUSTION RESIDUES; FLUES (combustion apparatus for consuming smoke or fumes, e.g. exhaust gases, F23G7/06)
- F23K: FEEDING FUEL TO COMBUSTION APPARATUS (fuel feeders specially adapted for fluidised bed combustion apparatus F23C10/22)

## Abstract

A process for burning coal or other carbonaceous fuels captures sulfur and other undesirable compounds are captured and retained in non-reactive ceramic-like form after the combustion phase. The process involves addition of multiple element alkali powders and/or sorbents preferably containing oxidizing anions such as nitrates and nitrites, preferably based on calcium. In various embodiments, the remediation materials when applied in a complex powder and/or liquid containing multiple elements, result in higher sulfur capture than the materials would otherwise achieve on an individual basis. In a preferred embodiment, the sorbents contain elements that minimize or lower the melting point of the ash. This leads to lowered cohesiveness and toughness of the ash so that less ash builds up on the boiler and better heat transfer is obtained.

## Claims

### Claim 1

A method for reducing the amount of sulfur gases released into the atmosphere upon combustion of a sulfur-containing carbonaceous fuel, comprising:
applying a sorbent composition onto the carbonaceous fuel; and
combusting the carbonaceous fuel,
wherein the sorbent composition comprises calcium nitrate, calcium nitrite, or both.

### Claim 2 (depends on 1)

A method according to claim 1, wherein the sorbent composition comprises calcium nitrite and calcium nitrate.

### Claim 3 (depends on 1)

A method according to claim 1, wherein the sorbent composition further comprises calcium bromide.

### Claim 4 (depends on 1)

A method according to claim 1, comprising applying an aqueous solution comprising calcium nitrate and calcium nitrite onto the fuel.

### Claim 5 (depends on 1)

A method according to claim 1, comprising adding up to 6% dry weight of the sorbent composition onto the fuel.

### Claim 6 (depends on 1)

A method according to claim 1, comprising applying up to 3% dry weight of the sorbent composition onto the fuel.

### Claim 7 (depends on 1)

A method according to claim 1, comprising applying up to 1.5% dry weight of the sorbent composition onto the fuel.

### Claim 8 (depends on 1)

A method according to claim 1, wherein the sorbent composition further comprises silicon dioxide, aluminum oxide, calcium oxide, and iron oxide.

### Claim 9 (depends on 8)

A method according to claim 8, wherein the sorbent further comprises magnesium oxide.

### Claim 10 (depends on 8)

A method according to claim 8, comprising adding a powder composition comprising silicon oxide, aluminum oxide, calcium oxide, and iron oxide onto the carbonaceous fuel.

### Claim 11 (depends on 10)

A method according to claim 10, wherein the powder composition comprises Portland cement.

### Claim 12 (depends on 10)

A method according to claim 10, wherein the powder composition comprises a dolomitic material selected from the group consisting of dolomite and burnt dolomite.

### Claim 13 (depends on 10)

A method according to claim 10, comprising applying an aqueous solution comprising calcium nitrate and calcium nitrite onto particulate carbonaceous fuel, and adding the powder composition onto the wetted fuel.

### Claim 14 (depends on 1)

A method according to claim 1, wherein the fuel comprises lignite coal.

### Claim 15 (depends on 1)

A method according to claim 1, wherein the fuel comprises bituminous coal.

### Claim 16 (depends on 1)

A method according to claim 1, wherein the fuel comprises anthracite coal.

### Claim 17

A method for reducing the amount of sulfur gases released into the atmosphere upon combustion of a sulfur-containing carbonaceous fuel, comprising:
applying a sorbent composition onto the carbonaceous fuel; and
combusting the carbonaceous fuel,
wherein the sorbent composition comprises
20-50% by weight Portland cement
20-40% by weight calcium oxide
15-25% by weight of a dolomitic material selected from the group consisting of dolomite and burnt dolomite, and
5-15% by weight of an aluminosilicate clay.

### Claim 18 (depends on 17)

A method according to claim 17, wherein the clay comprises calcium montmorillonite, kaolin, or a combination thereof.

### Claim 19 (depends on 17)

A method according to claim 17, wherein the sorbent composition comprises about 30% by weight Portland cement, about 40% by weight calcium oxide, about 20% by weight dolomite, and about 10% by weight clay.

### Claim 20 (depends on 17)

A method according to claim 17, wherein the sorbent composition further comprises at least one oxidizing salt selected from the group consisting of calcium nitrate and calcium nitrite.

### Claim 21 (depends on 20)

A method according to claim 20, comprising applying the at least one oxidizing salt in an aqueous solution.

### Claim 22 (depends on 17)

A method according to claim 17, wherein the carbonaceous fuel comprises coal.

### Claim 23 (depends on 22)

A method according to claim 22, wherein the coal comprises <4% by weight sulfur.

### Claim 24 (depends on 22)

A method according to claim 22, wherein the coal comprises <3% by weight sulfur.

### Claim 25 (depends on 22)

A method according to claim 22, wherein the coal comprises <2% by weight sulfur.

### Claim 26 (depends on 22)

A method according to claim 22, wherein the coal comprises >4% by weight sulfur.

### Claim 27 (depends on 17)

A method according to claim 17, comprising applying up to 6% weight of the sorbent composition onto the fuel.

### Claim 28 (depends on 27)

A method according to claim 27, further comprising applying a liquid sorbent comprising water and solids, the solids comprising at least one of calcium nitrate and calcium nitrite.

### Claim 29 (depends on 28)

A method according to claim 28, comprising applying up to 3% weight of the powder composition and up to 1.5% weight of the solids in the liquid sorbent, based on the weight of the carbonaceous fuel.

### Claim 30

A method for reducing sulfur gases and/or mercury released into the atmosphere upon combustion of coal containing sulfur and/or mercury comprising:
applying a powder sorbent composition onto the carbonaceous fuel, and
combusting the carbonaceous fuel,
wherein the sorbent composition comprises
Portland cement,
at least one water soluble chlorine containing inorganic compound,
calcium oxide,
optionally an aluminosilicate clay, and
an alkali metal salt selected from the group consisting of sodium silicate, potassium silicate, sodium hydroxide, potassium hydroxide, sodium oxide, and potassium oxide.

### Claim 31 (depends on 30)

A method according to claim 30, wherein the at least one chlorine containing inorganic compound comprises a soluble salt selected from the group consisting of sodium chloride, potassium chloride, sodium chlorate, and potassium chlorate.

### Claim 32 (depends on 30)

A method according to claim 30, wherein the clay comprises metakaolin.

### Claim 33 (depends on 30)

A method according to claim 30, wherein the powder composition comprises
20-30% by weight Portland cement,
2-5% by weight of the water soluble chlorine containing inorganic compound,
20-40% by weight calcium oxide
20-30% by weight clay, and
1-9% by weight of the alkali metal salt.

### Claim 34 (depends on 30)

A method according to claim 30, wherein the sorbent composition further comprises at least one oxidizing salt selected from the group consisting of alkali metal nitrates, alkali metal nitrites, alkaline earth metal nitrates, and alkaline earth metal nitrites.

### Claim 35 (depends on 34)

A method according to claim 34, wherein the oxidizing salt comprises calcium nitrate, calcium nitrite, or a combination thereof.

### Claim 36 (depends on 30)

A method according to claim 30, further comprising applying a liquid sorbent onto the carbonaceous fuel, the liquid sorbent comprising at least one oxidizing salt selected from the group consisting of alkali metal nitrates, alkali metal nitrites, and alkaline earth metal nitrates, and alkaline earth metal nitrites.

### Claim 37 (depends on 36)

A method according to claim 36, wherein the oxidizing salt is selected from the group consisting of calcium nitrate, calcium nitrite, and combinations thereof.

### Claim 38 (depends on 30)

A method according to claim 30, further comprising applying a liquid sorbent to the carbonaceous fuel, the liquid sorbent comprising water and at least one alkali metal salt selected from the group consisting of potassium silicate, sodium silicate, potassium hydroxide, and sodium hydroxide.

### Claim 39 (depends on 30)

A method according to claim 30, comprising applying up to 6% by weight of the powder composition based on the weight of the carbonaceous fuel.

### Claim 40 (depends on 30)

A method according to claim 30, wherein the carbonaceous fuel comprises coal.

### Claim 41 (depends on 40)

A method according to claim 40, wherein the coal comprises lignite coal.

### Claim 42 (depends on 40)

A method according to claim 40, wherein the coal comprises bituminous coal.

### Claim 43 (depends on 40)

A method according to claim 40, wherein the coal comprises anthracite coal.

### Claim 44 (depends on 40)

A method according to claim 40, wherein the coal comprises greater than or equal to 2% by weight sulfur.

### Claim 45 (depends on 40)

A method according to claim 40, wherein the coal comprises greater than or equal to 3% by weight sulfur.

### Claim 46 (depends on 40)

A method according to claim 40, wherein the coal comprises greater than or equal to 4% by weight sulfur.

### Claim 47

A method for reducing the sulfur gases released in the atmosphere upon combustion of sulfur-containing coal, comprising
applying a liquid sorbent onto the coal, wherein the sorbent comprises water and solids, the solids comprising at least one soluble salt selected from the group consisting of soluble metal nitrates and soluble metal nitrites; and
applying a powder sorbent composition comprising calcium onto the coal,
wherein upon combustion of the coal to release its stored energy, the amount of sulfur gases in the combustion product is reduced and the amount of sulfur in the ashes increased relative to the amounts that would be produced by combustion of the coal without applying the liquid sorbent and powder sorbent.

### Claim 48 (depends on 47)

A method according to claim 47, wherein the liquid sorbent comprises alkaline metal nitrates, alkaline metal nitrites, alkaline metal earth nitrates, alkaline metal nitrites, or combinations thereof.

### Claim 49 (depends on 47)

A method according to claim 47, wherein the liquid sorbent comprises calcium nitrate and calcium nitrite.

### Claim 50 (depends on 47)

A method according to claim 47, comprising applying up to 6% weight of the solids and up to 6% weight of the powder sorbent.

### Claim 51 (depends on 47)

A method according to claim 47, comprising applying up to 3% weight of the solids and up to 3% weight of the powder sorbent.

### Claim 52 (depends on 47)

A method according to claim 47, wherein the powder sorbent composition comprises silicon, aluminum, calcium, iron, and magnesium.

### Claim 53 (depends on 47)

A method according to claim 47, wherein the powder sorbent composition comprises:
Portland cement;
calcium oxide;
optionally an aluminosilicate clay; and
dolomitic material selected from the group consisting of dolomite and burnt dolomite.

### Claim 54 (depends on 47)

A method according to claim 47, wherein the powder sorbent composition comprises
Portland cement;
calcium oxide;
at least one water soluble chlorine containing inorganic compound;
aluminosilicate clay; and
at least one alkali metal salt selected from the group consisting of potassium silicate, sodium silicate, potassium hydroxide, sodium hydroxide, potassium oxide, and sodium oxide.