# US 2008/0280197 A1 · Spirally wound non-aqueous electrolyte secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0280197 A1
- Document ID: US20080280197A1
- Status: Published application
- Kind: A1
- Application number: 12/114,400
- Filed: 2008-05-02
- Published: 2008-11-13
- Earliest claimed: 2007-05-07
- Assignees: Sony Corporation
- Inventors: Masaki Machida
- Web page: https://patentgrep.com/patent/US20080280197A1

## CPC

- H01M 10/0587: of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/523: {for non-aqueous cells (H01M4/525 takes precedence)}
- H01M 4/623: {fluorinated polymers}
- H01M 10/0431: {Cells with wound or folded electrodes (H01M10/045 takes precedence)}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0565: Polymeric materials, e.g. gel-type or solid-type
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A spirally-wound non-aqueous electrolyte secondary battery including a staked electrode assembly is disclosed. The stacked electrode assembly has first and second current collectors facing region disposed at a winding start end and at a winding terminal end, respectively. A positive electrode current collector exposed portion and a negative electrode current collector exposed portion face each other through the separator in each of the first and second current collector facing regions. At least one of the positive or negative electrode current collector exposed portion has a first insulating member formed thereon in the first current collector facing region at the winding start end. At least one of the positive or negative electrode current collector exposed portion has a second insulating member formed thereon in the second current collector facing region at the winding terminal end. The second insulating member has a melting point lower than that of the first insulating member.

## Claims

### Claim 1

A spirally-wound non-aqueous electrolyte secondary battery, comprising:
a stacked electrode assembly which includes a positive electrode including a cathode active material layer formed on at least one side of a positive electrode current collector, a negative electrode including an anode active material layer formed on at least one side of a negative electrode current collector, and a separator disposed between the positive electrode and the negative electrode, the positive electrode, the negative electrode, and the separator being spirally wound together,
wherein the stacked electrode assembly has a first current collector facing region and a second current collector facing region disposed at a winding start end and at a winding terminal end, respectively,
wherein a positive electrode current collector exposed portion in which the positive electrode current collector is exposed and a negative electrode current collector exposed portion in which the negative electrode current collector is exposed face each other through the separator in each of the first and second current collector facing regions,
wherein at least one of the positive electrode current collector exposed portion or the negative electrode current collector exposed portion has a first insulating member formed thereon in the first current collector facing region at the winding start end,
wherein at least one of the positive electrode current collector exposed portion or the negative electrode current collector exposed portion has a second insulating member formed thereon in the second current collector facing region at the winding terminal end, and
wherein the second insulating member has a melting point lower than that of the first insulating member.

### Claim 2 (depends on 1)

The spirally-wound non-aqueous electrolyte secondary battery according to claim 1, wherein the difference between the melting point of the first insulating member and the melting point of the second insulating member is 20° C. or higher.

### Claim 3 (depends on 2)

The spirally-wound non-aqueous electrolyte secondary battery according to claim 2, wherein the first insulating member is formed of a material selected from the group consisting of a polypropylene resin, a polyethylene terephthalate resin, a polyethylene naphthalate resin, a polyphenylene sulfide resin, and a polyimide resin.

### Claim 4 (depends on 2)

The spirally-wound non-aqueous electrolyte secondary battery according to claim 2, wherein the second insulating member is formed of a material selected from the group consisting of a low density polyethylene resin, a high density polyethylene resin, a polypropylene resin, a polyethylene terephthalate resin, a polyethylene naphthalate resin, and a polyphenylene sulfide resin.

### Claim 5 (depends on 2)

The spirally-wound non-aqueous electrolyte secondary battery according to claim 2, wherein the difference between the melting point of the first insulating member and the melting point of the second insulating member is 100° C. or higher.

### Claim 6 (depends on 1)

The spirally-wound non-aqueous electrolyte secondary battery according to claim 1, wherein the first insulating member is formed on both sides of the positive electrode current collector exposed portion at the winding start end of the positive electrode, and the second insulating member is formed on both sides of the positive electrode current collector exposed portion at the winding terminal end of the positive electrode.

### Claim 7 (depends on 1)

The spirally-wound non-aqueous electrolyte secondary battery according to claim 1, wherein the first insulating member and the second insulating member are not formed in the negative electrode.

### Claim 8 (depends on 1)

The spirally-wound non-aqueous electrolyte secondary battery according to claim 1, wherein the first insulating member and second insulating member are formed so that the positive electrode current collector exposed portion and the negative electrode current collector exposed portion do not face each other through only the separator.

### Claim 9 (depends on 1)

The spirally-wound non-aqueous electrolyte secondary battery according to claim 1, wherein the first insulating member and second insulating member are formed at both ends of the negative electrode.

### Claim 10 (depends on 1)

The spirally-wound non-aqueous electrolyte secondary battery according to claim 1, wherein the first insulating member and second insulating member are individually formed on each of the positive electrode and the negative electrode.

### Claim 11 (depends on 1)