# US 2008/0277818 A1 · Composition and Method for Producing Continuous Basalt Fibre

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0277818 A1
- Document ID: US20080277818A1
- Status: Published application
- Kind: A1
- Application number: 12/063,796
- Filed: 2006-12-25
- Published: 2008-11-13
- Earliest claimed: 2006-05-19
- Inventors: Viktor F. Kibol; Sunao Nakanoo; Alexandr B. Biland; Roman V. Kibol
- Web page: https://patentgrep.com/patent/US20080277818A1

## CPC

- C03C 13/06: Mineral fibres, e.g. slag wool, mineral wool, rock wool
- C03C 1/024: {Chemical treatment of cullet or glass fibres}
- C03C 13/001: {Alkali-resistant fibres}
- Y10T 428/24355: Continuous and nonuniform or irregular surface on layer or component [e.g., roofing, etc.]
- Y10T 428/29: Coated or structually defined flake, particle, cell, strand, strand portion, rod, filament, macroscopic fiber or mass thereof
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The proposed inventions pertain to technology of continuous inorganic fibers manufacturing by way of drawing from melted minerals. Such continuous inorganic fibers may be used in production of heat-resistant threads, rovings, cut fibers, fabrics, composition materials and products based on such materials. The C contains the mixture of silicon (SiO2), aluminum (Al2O3), titan (TiO2), iron (Fe2O3 and FeO), calcium (CaO), magnesium (MgO), manganese (MnO) oxides and admixtures, and, according to the invention, this composition further contains potassium (K2O), sodium (Na2O), barium (BaO) oxides with the following components ratio (in mass %): Al2O3 15.90-18.10 TiO2 0.75-1.20 Fe2O3 + FeO 7.51-9.53 CaO 6.41-8.95 MgO 2.50-6.40 K2O 1.60-2.72 Na2O 3.30-4.10 P2O5 0.23-0.50 SO3 0.02-0.15 MnO 0.12-0.21 BaO 0.05-0.19 admixtures, up to 1.00 SiO2 the rest. The M comprises operations of the crushed composition loading into the melting furnace, melting, melt homogenization, subsequent stabilization of the melt in the melting furnace feeder, drawing, lubrication and winding the fiber onto the reel, and, according to the invention, the composition is held in alkaline solution during 15 to 20 minutes, then washed by running water during 20 to 30 minutes, dried and loaded into the melting furnace after such washing and drying. The feature of the proposed M is the use of sodium hydroxide (NaOH) and potassium hydroxide (KOH) solution in the range of about 0.1 to 0.5 N concentration as the alkaline solution. The inventions aim at providing the means for obtaining stronger and chemically more stable fibers by way of creating the conditions for decreasing the number of defects on the fiber surfaces.

## Claims

### Claim 1

Composition for production of continuous basalt fiber containing the mixture of silicon (SiO2), aluminum (Al2O3), titan (TiO2), iron (Fe2O3 and FeO), calcium (CaO), magnesium (MgO), manganese (MnO) oxides and admixtures, wherein this composition further contains potassium (K2O), sodium (Na2O), barium (BaO) oxides with the following components ratio (in mass %):
Al2O3
15.90-18.10
TiO2
0.75-1.20
Fe2O3 + FeO
7.51-9.53
CaO
6.41-8.95
MgO
2.50-6.40
K2O
1.60-2.72
Na2O
3.30-4.10
P2O5
0.23-0.50
SO3
0.02-0.15
MnO
0.12-0.21
BaO
0.05-0.19
admixtures,
up to 1.00
SiO2
the rest.

### Claim 2 (depends on 1)

Method of continuous basalt fiber production from the composition according to claim 1, comprising operations of the crushed composition loading into the melting furnace, melting, melt homogenization, subsequent stabilization of the melt in the melting furnace feeder, drawing, lubrication and winding the fiber onto the reel, wherein the composition is held in alkaline solution during 15 to 20 minutes, then washed by running water during 20 to 30 minutes, dried and loaded into the melting furnace after such washing and drying.

### Claim 3 (depends on 2)

Method of continuous basalt fiber production according to claim 2, wherein sodium hydroxide (NaOH) and potassium hydroxide (KOH) solution in the range of about 0.1 to 0.5 N concentration is used as the alkaline solution.