# US 2008/0277808 A1 · Method of manufacturing a lens presenting a graded tint

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0277808 A1
- Document ID: US20080277808A1
- Status: Published application
- Kind: A1
- Application number: 12/114,148
- Filed: 2008-05-02
- Published: 2008-11-13
- Earliest claimed: 2002-05-02
- Assignees: Bnl Eurolens
- Inventors: Didier CLERC
- Web page: https://patentgrep.com/patent/US20080277808A1

## CPC

- B29C 45/16: Making multilayered or multicoloured articles {(B29C45/0062 takes precedence; feeding colouring materials into the injection unit B29C45/1816)}
- B29K 2995/002: Coloured
- B29L 2011/0016: {Lenses}
- Y10S 425/808: Lens mold
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method of manufacturing a lens presenting a graded tint, the lens comprising first and second layers each of which is made of a thermoplastic material, with only one of the layers being colored in the tint concerned, the method including the steps of: injecting the thermoplastic material of the first layer into a first mold cavity in order to form the first layer; and placing the first layer in a second mold cavity and injecting therein the thermoplastic material of the second layer so as to form the second layer on the first layer.

## Claims

### Claim 1

A method of manufacturing a lens presenting a graded tint lens comprising first and second layers each of which is made of a thermoplastic material, with only one of the layers being colored in the tint concerned, the method comprising the step of:
injecting the thermoplastic material of the first layer into a first mold cavity in order to form the first layer, wherein:
the first layer is the layer colored in the tint concerned and occupies a front face of a lens,
said first layer being of varying thickness along a vertical direction and presenting on the top edge a thickness which is at least superior or equal to about 1.5 mm and on the bottom edge a thickness which is at least inferior or equal to about 0.8 mm;
said variation of the thickness of the first layer from the top to the bottom of the lens providing a graded vertical tinting effect to the lens, which presents the great variation of transmission (Tv), along a vertical direction, into a space comprised from about 20 to 25 mm above and below the geometric centre of said lens along a horizontal direction,
said first layer being of constant thickness as measured along a horizontal direction to provide along this horizontal direction a constant horizontal tinting effect to the lens; and
placing the first layer in a second mold cavity and injecting therein the thermoplastic of the second layer so as to form the second layer on the first layer,
the second layer occupying a rear face of the lens,
said second layers being of varying thickness along a vertical direction from a top edge of the lens to a bottom edge of the lens, in a substantially complementary manner with the first layer to provide a lens which presents on the top edge and on the bottom edge a thickness at least superior to 1.5 mm said second layer being of varying thickness as measured along a horizontal direction to provide the optical property to the lens.

### Claim 2 (depends on 1)

The method of manufacture according to claim 1, wherein the second layer is not tinted.

### Claim 3 (depends on 1)

The method of manufacture according to claim 1, wherein the second layer is colored in a tint different from the tint of the first layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein, the first and second lens are molded using an injection molding installation and comprising the sequential steps of:
placing a first concave shape (7) which faced a second convex shape (8) so as to define a first mold cavity for the first layer, with the first and second shapes arranged such that the first layer has a thickness that decrease, along a vertical direction, going from a top edge towards a bottom edge, and a constant thickness along a horizontal direction,
injecting a colored thermoplastic material between the first and second shapes to form the first layer, the first and second shapes being heated to a temperature over the glass transition temperature of the colored thermoplastic material being injected;
spacing the first and second shapes apart from each other, with the thus-formed first layer remaining in position in the concave first shape, said first shape being maintained to the temperature used during the first injecting step;
facing the concave first shape towards a convex third shape (9) so that a concave face (10) of the first layer co-operates with the convex third shape (9) to define a cavity for forming the second layer;
injecting a non-colored thermoplastic material into a cavity formed between the concave face of the first layer and the convex third shape, said third shape being heated to a temperature over the glass transition temperature of the non-colored thermoplastic material being injected, to form the second layer with a thickness that varies in a manner complementary to the thickness of the first layer so that the combined thickness of the first and second layer remains constant along a vertical direction.