# US 2008/0277455 A1 · Method for joining components made of a high-strength aluminum material and heat exchanger assembled according to the method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0277455 A1
- Document ID: US20080277455A1
- Status: Published application
- Kind: A1
- Application number: 12/114,922
- Filed: 2008-05-05
- Published: 2008-11-13
- Earliest claimed: 2007-05-11
- Inventors: Hanskarl Hoffmann; Rahul Rajagopalan
- Web page: https://patentgrep.com/patent/US20080277455A1

## CPC

- B23K 1/0012: {Brazing of heat exchangers}
- B23K 2103/10: Aluminium or alloys thereof
- Y10T 29/49393: with metallurgical bonding
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention relates to a method for joining components made of a high-strength aluminum material, whereby at least two components of high-strength aluminum alloys are joined by soldering, both components separated from each other by at least one aluminum layer with a lower magnesium content compared with the contact surfaces before joining is carried out, and a heat exchanger produced according to this method.

## Claims

### Claim 1

A method of joining components, the method comprising the steps of:
(a) providing at least two components made of high strength aluminum alloys containing magnesium;
(b) placing a contact surface of each of the components to be joined adjacent each other;
(c) providing at least one aluminum layer having a low magnesium content between the contact surfaces of the components to separate the components; and
(d) soldering the components and the aluminum layer to connect the components.

### Claim 2 (depends on 1)

The method according to claim 1, wherein step (d) includes soldering the components and the aluminum layer using one of a controlled atmosphere brazing technique and flame soldering with one of a corrosive and non-corrosive fluxing agent.

### Claim 3 (depends on 1)

The method according to claim 1, wherein step (d) includes soldering the components and the aluminum layer using a controlled atmosphere brazing technique with a fluxing agent that contains cesium.

### Claim 4 (depends on 1)

The method according to claim 1, wherein step (c) includes applying an aluminum layer of a 1xxx or 3xxx alloy having a lower magnesium content than the components to at least one of the contact surfaces of the components to separate the components.

### Claim 5 (depends on 4)

The method according to claim 4, further comprising the step of disposing a solder on an edge of a solder gap, wherein the solder is one of a paste, a wire, and a ring.

### Claim 6 (depends on 4)

The method according to claim 4, further comprising the step of inserting the solder into the solder gap.

### Claim 7 (depends on 1)

The method according to claim 1, wherein step (c) includes inserting a molded part produced at least partially of aluminum having a lower magnesium content than the components into the solder gap to separate the components.

### Claim 8 (depends on 1)

The method according to claim 1, wherein step (c) includes inserting a molded part with a plurality of aluminum layers with at least one of a 4xxx, a 3xxx, and a 1xxx alloy, having a lower magnesium content than the components into the solder gap to separate the components.

### Claim 9 (depends on 1)

The method according to claim 1, wherein step (c) includes providing at least one aluminum layer on at least one of the components to be joined using a plasma supported vapor deposition process to separate the components.

### Claim 10 (depends on 1)

The method according to claim 1, wherein step (c) includes providing at least one aluminum layer on at least one of the components to be joined using one of a single sided and a double sided solder plating process to separate the components.

### Claim 11 (depends on 1)

The method according to claim 1, wherein step (c) includes providing at least one aluminum layer of 4xxx, 3xxx, and 1xxx on at least one of the contact surfaces to separate the components.

### Claim 12

A method of joining components, the method comprising the steps of:
(a) providing at least two components made of high strength aluminum alloys containing magnesium;
(b) placing a contact surface of each of the components to be joined adjacent each other;
(c) applying at least one aluminum layer of at least one of a 1xxx and a 3xxx alloy having a lower magnesium content compared to the components to at least one of the contact surfaces to separate the components; and
(d) soldering the components and the aluminum layer to connect the components.

### Claim 13 (depends on 12)

The method according to claim 12, wherein step (c) includes inserting a molded part having a plurality of aluminum layers of at least one of a 4xxx, a 3xxx and a 1xxx alloy having a lower magnesium content as compared with the components, into the solder gap, to separate the components.

### Claim 14 (depends on 12)

The method according to claim 12, wherein step (c) includes providing at least one aluminum layer to at least one of the components to be joined using a plasma supported vapor deposition process to separate the components.

### Claim 15 (depends on 12)

The method according to claim 12, wherein step (c) includes providing at least one aluminum layer to at least one of the components to be joined using one of a single sided and a double sided solder plating process to separate the components.

### Claim 16 (depends on 12)

The method according to claim 12, wherein step (c) includes providing a layer of at least one of a 4xxx, a 3xxx, and a 1xxx alloy to at least one of the contact surfaces to separate the components.

### Claim 17

A heat exchanger comprising:
a first heat exchanger component produced from a high strength aluminum alloy containing magnesium;
a second heat exchanger component produced from a high strength aluminum alloy containing magnesium; and
a solder connection disposed between said first heat exchanger component and said second heat exchanger component, wherein said solder connection includes at least one aluminum alloy layer having a lower magnesium content than said first heat exchanger component and said second heat exchanger component.

### Claim 18 (depends on 17)

The heat exchanger according to claim 17, wherein said first heat exchanger component is one of a collection tank, a connecting block, a distributor tube, and a distributor, and said second heat exchanger component is one of a collection tank, a connecting block, a distributor tube, and a distributor.

### Claim 19 (depends on 17)

The heat exchanger according to claim 17, wherein said solder connection includes at least one aluminum alloy layer having a lower magnesium content than said first heat exchanger component and said second heat exchanger component separating said components.

### Claim 20 (depends on 17)

The heat exchanger according to claim 17, wherein at least one of said first heat exchanger component and said second heat exchanger component includes at least one aluminum alloy layer provided by a plasma supported vapor deposition process.