# US 2008/0268172 A1 · Layer forming method using plasma discharge

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0268172 A1
- Document ID: US20080268172A1
- Status: Published application
- Kind: A1
- Application number: 12/156,337
- Filed: 2008-05-30
- Published: 2008-10-30
- Earliest claimed: 2000-12-12
- Assignees: Konica Corporation
- Inventors: Kazuhiro Fukuda; Yoshikazu Kondo; Takashi Murakami; Shunichi Iwamaru; Yumi Muramatsu; Toshio Tsuji
- Web page: https://patentgrep.com/patent/US20080268172A1

## CPC

- G02B 1/11: Anti-reflection coatings
- C23C 4/10: Oxides, borides, carbides, nitrides or silicides; Mixtures thereof
- C23C 4/18: After-treatment
- C23C 16/402: {Silicon dioxide}
- C23C 16/405: {of refractory metals or yttrium}
- C23C 16/509: using internal electrodes
- C23C 16/5093: {Coaxial electrodes}
- C23C 16/545: {for coating elongated substrates}
- G02B 1/10: Optical coatings produced by application to, or surface treatment of, optical elements (G02B1/08 takes precedence)
- G02B 1/115: Multilayers
- G02B 1/14: Protective coatings, e.g. hard coatings
- G02B 1/16: having an anti-static effect, e.g. electrically conducting coatings
- G02B 1/18: Coatings for keeping optical surfaces clean, e.g. hydrophobic or photo-catalytic films (G02B1/16 takes precedence)
- H01J 37/32532: {Electrodes}
- Y02T 50/60: Efficient propulsion technologies, e.g. for aircraft
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

A layer forming method is disclosed which relies on reactive gas in a plasma state. The method includes steps of supplying power of not less than 1 W/cm2 at a high frequency voltage exceeding 100 kHz across a gap between a first electrode and a second electrode opposed to each other at atmospheric pressure or at approximately atmospheric pressure to induce a discharge, generating a reactive gas in a plasma state by the charge, and exposing a substrate to the reactive gas in a plasma state to form a layer on the substrate.

## Claims

### Claim 1

A layer forming method comprising the steps of:
supplying power of not less than 1 W/cm2 at a high frequency voltage exceeding 100 kHz across a gap formed between a first electrode and at least one second electrode opposed to each other at approximately atmospheric pressure to induce a discharge, and thereby generating a reactive gas in a plasma state by the discharge; and
exposing a substrate to the reactive gas in a plasma state to form a layer on the substrate;
wherein the total power supplied between the first electrode and the second electrode or the second electrodes exceeds 15 kW.

### Claim 2 (depends on 1)

The method of claim 1 wherein the total power supplied is not less than 30 kW.

### Claim 3 (depends on 1)

The method of claim 1 wherein the total power supplied is not less than 50 kW.

### Claim 4 (depends on 1)

The method of claim 1 wherein the total power supplied is not more than 300 kW.

### Claim 5 (depends on 1)

The method of claim 1 wherein the power is supplied at not less than 1.2 W/cm2 at a high frequency voltage not less than 200 kHz.

### Claim 6 (depends on 5)

The method of claim 5 wherein the total power is not less than 50 kW and not more than 300 kW.

### Claim 7 (depends on 6)

The method of claim 6 wherein the approximately atmospheric pressure is 93 kPa to 104 kPa.

### Claim 8 (depends on 5)

The method of claim 5 wherein the high frequency voltage is not less than 800 kHz.

### Claim 9 (depends on 1)

The method of claim 1 wherein the step of exporting the substrate to reactive gas forms a layer of 1 nm to 1000 nm.

### Claim 10 (depends on 1)

The method of claim 1 wherein the total power is not less than 50 kW and not more than 300 kW.

### Claim 11 (depends on 1)

The method of claim 1 wherein the approximately atmospheric pressure is 93 kPa to 104 kPa.