# US 2008/0258131 A1 · Light Emitting Diode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0258131 A1
- Document ID: US20080258131A1
- Status: Published application
- Kind: A1
- Application number: 12/065,465
- Filed: 2006-09-29
- Published: 2008-10-23
- Earliest claimed: 2005-09-30
- Assignees: Seoul Opto Device Co., Ltd.
- Inventors: Kyoung Hoon Kim
- Web page: https://patentgrep.com/patent/US20080258131A1

## CPC

- H10H 20/825: containing nitrogen, e.g. GaN
- B82Y 20/00: Nanooptics, e.g. quantum optics or photonic crystals
- H10H 20/812: within the light-emitting regions, e.g. having quantum confinement structures
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

The present invention relates to a light emitting diode. More specifically, the present invention relates to a light emitting diode comprising an N-type semiconductor layer formed on a substrate, an active layer formed on the N-type semiconductor layer and a P-type semiconductor layer formed on the active layer, wherein the active layer is formed to have either a quantum well structure in which an AlxGa1-xN (0≦x<1) well layer and an AlN barrier layer are alternately laminated or a quantum well structure in which a well layer and a barrier layer are formed of a compound semiconductor layer containing phosphorous (P) and are alternately laminated. Accordingly, far-ultraviolet light can be easily emitted and the optical power of the light emitting diode can also be improved.

## Claims

### Claim 1

A light emitting diode, comprising:
an N-type semiconductor layer formed on a substrate;
an active layer formed on the N-type semiconductor layer; and
a P-type semiconductor layer formed on the active layer,
wherein the active layer is formed to have a quantum well structure in which an AlxGa1-xN (0≦x≦1) well layer and an AlN barrier layer are alternately laminated.

### Claim 2

A light emitting diode, comprising:
an N-type semiconductor layer formed on a substrate;
an active layer formed on the N-type semiconductor layer; and
a P-type semiconductor layer formed on the active layer,
wherein the active layer is formed to have a quantum well structure in which a well layer and a barrier layer are formed of a compound semiconductor layer containing phosphorous (P) and are alternately laminated.

### Claim 3 (depends on 1)

The light emitting diode as claimed in claim 1, wherein each of the well layer and the barrier layer is formed to a thickness of 5 to 1,000 Å.

### Claim 4 (depends on 1)

The light emitting diode as claimed in claim 1, wherein the AlxGa1-xN well layer is formed at a growth rate of 0.01 to 10 μm/hour using a gallium source, an aluminum source and a nitrogen source at a temperature of 900 to 1,300° C. and a pressure of 30 to 760 torr.

### Claim 5 (depends on 4)

The light emitting diode as claimed in claim 4, wherein the AlxGa1-xN well layer has a mole ratio of aluminum and gallium to nitrogen of 1:50 to 1:50,000.

### Claim 6 (depends on 1)

The light emitting diode as claimed in claim 1, wherein the AlN barrier layer is formed at a growth rate of 0.01 to 10 μm/hour using an aluminum source and a nitrogen source at a temperature of 900 to 1,300° C. and a pressure of 30 to 760 torr.

### Claim 7 (depends on 6)

The light emitting diode as claimed in claim 6, wherein the AlN barrier layer has a mole ration of aluminum to nitrogen of 1:50 to 1:50,000.

### Claim 8 (depends on 2)

The light emitting diode as claimed in claim 2, wherein the well layer is formed of AlNxP1-x and the barrier layer is formed of AlNyP1-y, wherein 0<x, y<1, and y>x.

### Claim 9 (depends on 8)

The light emitting diode as claimed in claim 8, wherein the well layer and the barrier layer are formed at a growth rate of 0.01 to 10 μm/hour using an aluminum source, a nitrogen source and a phosphorous source at a temperature of 400 to 1,200° C. and a pressure of 20 to 760 torr.

### Claim 10 (depends on 9)

The light emitting diode as claimed in claim 9, wherein each of the well layer and the barrier layer has a mole ration of aluminum to nitrogen and phosphorous of 1:50 to 1:50,000.

### Claim 11 (depends on 1)

The light emitting diode as claimed in claim 1, wherein the AlxGa1-xN well layer and the AlN barrier layer are alternately laminated two to one thousand times.

### Claim 12 (depends on 2)

The light emitting diode as claimed in claim 2, wherein the well layer and the barrier layer are alternately laminated two to one thousand times.

### Claim 13 (depends on 1, 2)

The light emitting diode as claimed in claim 1 or 2, further comprising a buffer layer formed between the substrate and the N-type semiconductor layer.

### Claim 14 (depends on 1, 2)

The light emitting diode as claimed in claim 1 or 2, further comprising an N-type clad layer formed between the N-type semiconductor layer and the active layer, and a P-type clad layer formed between the P-type semiconductor layer and the active layer.