# US 2008/0236707 A1 · Method and Device For Producing a Mechanical Part, in Particular a Bearing Ring and a Part Produced By Said Method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0236707 A1
- Document ID: US20080236707A1
- Status: Published application
- Kind: A1
- Application number: 11/661,797
- Filed: 2005-09-02
- Published: 2008-10-02
- Earliest claimed: 2004-09-03
- Inventors: Gianfranco Passoni
- Web page: https://patentgrep.com/patent/US20080236707A1

## CPC

- F16C 33/64: Special methods of manufacture
- Y10S 29/006: Method or apparatus with centrifugal casting
- Y10T 29/49689: Race making
- Y10T 29/49705: Coating or casting
- Y10T 29/49989: Followed by cutting or removing material
- Y10T 29/5184: Casting and working
- F16C: SHAFTS; FLEXIBLE SHAFTS; ELEMENTS OR CRANKSHAFT MECHANISMS; ROTARY BODIES OTHER THAN GEARING ELEMENTS; BEARINGS
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A device and method for producing, by molding, a circular-shaped mechanical part made of a metal alloy. The device has a rotatable hollow mold for receiving a predetermined quantity of the metal alloy. The predetermined quantity of the metal alloy is defined by at least one segment of a metal alloy rod. An inductive heating device melts the metal alloy to a melting point. A blank of the mechanical part being formed by centrifuging the melted metal alloy. Cooling the blank in the hollow mold to a second temperature which corresponds to a desired malleability. Processing the blank with a shaping tool to obtain a desired internal profile. To harden and form the circular-shaped mechanical part, the blank is further cooled to a tempering temperature.

## Claims

### Claim at position 1

1-16. (canceled)

### Claim 17

A method of producing an annular-shaped mechanical part made of a metal alloy that can be subjected to at least one thermal hardening treatment, a blank of the mechanical part is produced by centrifugation in a rotating hollow mold from a predetermined volume of the metal alloy which is heated to a melting temperature (T1) and the blank is next cooled to a second temperature (T2) lower than the melting temperature (T1), the blank at the second temperature (T2) having a malleable consistency, wherein the predetermined volume of the metal alloy to be melted is determined from a metal alloy bar inserted into a vertical induction oven, which is open at a lower end above the hollow mold, the predetermined volume of metal alloy is heated to the melting temperature (T1), an interior profile of the mechanical part is formed using a machining tool brought into contact with an interior surface of the mechanical part when the blank has reached the second temperature (T2), the mechanical part is then extracted from the hollow mold and is cooled to a tempering temperature (T3) in a predetermined manner.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the metal alloy bar is circularly pre-notched to define bar segments, each of the bar segments correspond to one of the predetermined volume of the raw material required to produce the mechanical part and to a whole sub-multiple of the predetermined volume of the raw material.

### Claim 19 (depends on 17)

The method according to claim 17, wherein the predetermined volume of the metal alloy is introduced into the hollow mold in a form of at least one drop formed by at least one bar segment melted at the melting temperature (T1) in the vertical induction oven, the at least one drop being detached from the metal alloy bar inserted inside the vertical induction oven by a force of gravity.

### Claim 20 (depends on 17)

The method according to claim 17, wherein the predetermined volume of the metal alloy is inserted into the hollow mold in a form of at least one bar segment, the at least one bar segment being detached from the metal alloy bar by heating the metal alloy bar in areas where the metal alloy bar is pre-notched, the at least the bar segment is heated to the melting temperature (T1) by heating components at least partially surrounding the hollow mold.

### Claim 21

A production device for producing a circular-shaped mechanical part made of a metal alloy capable of undergoing at least one thermal hardening treatment, device comprising a rotating hollow mold (11, 41) positioned to receive a predetermined volume of the metal alloy, heating components to bring the metal alloy to a melting temperature (T1) and drive mechanisms to cause the hollow mold to rotate and produce a blank (26) of the mechanical part through centrifugation,
a means for determining the predetermined volume of the metal alloy to be melted from a metal alloy bar (20);
induction heating components to melt the predetermined volume of the metal alloy by bringing the predetermined volume of the metal alloy to the melting temperature (T1) in the hollow mold;
a means (30) for cooling the blank (26) which was obtained through centrifugation of the molten alloy metal in the hollow mold and for bringing the predetermined volume of the metal alloy to a temperature second (T2), lower than the melting temperature (T1), at which the blank (26) has a malleable consistency;
machining mechanisms to form an interior shape of the mechanical part (28);
a temperature regulation device to bring the mechanical part (28) obtained from this blank to a tempering temperature (T3); and
a means for tempering the mechanical part (28) after the mechanical part (28) is extracted from the hollow mold.

### Claim 22 (depends on 21)

The device according to claim 21, wherein the means for determining the predetermined volume of the metal alloy to be melted comprises preliminary circular notches made on the bar (20) to define bar segments (21), the notches corresponding to one of the predetermined volume of the metal alloy required to produce the mechanical part (28) and to a whole sub-multiple of the predetermined volume of the metal alloy.

### Claim 23 (depends on 21)

The device according to claim 21, wherein the induction heating components comprise a vertical induction oven (23) open at a lower end above the hollow mold into which a prenotched bar of the metal alloy is inserted.

### Claim 24 (depends on 21)

The device according to claim 21, wherein the induction heating components comprise a vertical induction oven (23) into which a prenotched bar (20) of the metal alloy is inserted and at least one induction coil (31) at least partially surrounding the hollow mold (11), the melting temperature (T1) in the induction oven (23) being defined to melt the pre-notched bar (20) only in pre-notched areas (21) allowing detachment of segments (21) necessary to obtain the predetermined volume of the metal alloy, the segments being melted in the hollow mold (11) and brought to the melting temperature (T1) by the at least one induction coil (31).

### Claim 25 (depends on 21)

The device according to claim 21, wherein the machining mechanisms comprise a rotating shaping tool (27) in communication with one or more mechanisms which cause the shaping tool (27) to rotate and a means of axial and lateral movement to bring the shaping tool (27) into contact with an interior face of the blank (26) to form an interior shape of the mechanical part.

### Claim 26 (depends on 21)

The device according to claim 21, wherein the hollow mold (11) is combined with a mask (15) that forms a casting wall of the mechanical part.

### Claim 27 (depends on 21)

The device according to claim 21, wherein the means for tempering the mechanical part (28) comprises at least a tempering bath.

### Claim 28 (depends on 21)

The device according to claim 21, wherein the hollow mold (41) consists of at least two radially mobile segments (42) positioned to allow opening of the hollow mold to extract the mechanical part.

### Claim 29 (depends on 21)

The device according to claim 21, wherein the hollow mold (11; 41) comprises a crucible (13) positioned to contain the predetermined volume of the metal alloy and a casting cavity (14) that communicates with the crucible (13).

### Claim 30 (depends on 21)

The device according to claim 21, wherein the means for cooling the blank (26) are located to cool one or more of exterior walls of the mold (11; 41) and a mask (15).

### Claim 31

A method of producing an annular-shaped mechanical part made of a metal alloy that can be subjected to at least one thermal hardening treatment the method comprising the steps of:
defining a volume of the metal alloy;
inserting the volume of the metal alloy in a vertical induction oven, the induction oven having an open lower end aligned with a hollow mold which is located below the open lower end heating the volume of the metal alloy to a melting temperature (T1);
allowing the molten metal alloy to fall into the hollow mold;
rotating the hollow mold such that the molten metal alloy is forced into a casting cavity portion of the hollow mold by centrifugal force;
cooling the metal alloy to a second temperature (T2), at which the metal alloy tempers, but remains malleable, to form the annular-shaped mechanical part,
shaping an interior surface of the annular-shaped mechanical part with a shaping part to form a desired internal profile; and
further cooling the annular-shaped mechanical part to a tempering temperature (T3).