# US 2008/0210299 A1 · Method of Fabricating Photocoltaic Cells

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0210299 A1
- Document ID: US20080210299A1
- Status: Published application
- Kind: A1
- Application number: 11/792,327
- Filed: 2005-12-08
- Published: 2008-09-04
- Earliest claimed: 2004-12-21
- Assignees: Solarforce
- Inventors: Christian Belouet; Claud Remy
- Web page: https://patentgrep.com/patent/US20080210299A1

## CPC

- H10F 71/1221: {comprising polycrystalline silicon}
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 71/139: {using temporary substrates}
- Y02E 10/546: Polycrystalline silicon PV cells
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The invention relates to a method of fabricating photovoltaic cells in which at least one layer of semiconductor material is deposited continuously on a carbon ribbon (10) to form a composite ribbon (20), said layer having a free face (22, 24) opposite from its face in contact with the carbon ribbon. According to the invention, at least one treatment (28) is applied to the layer of semiconductor material, from said free face (22, 24), in order to implement photovoltaic functions of the cells on said layer, prior to eliminating the carbon ribbon (10). The invention makes it possible to increase productivity in the fabrication of photovoltaic cells, which cells can be of very small thicknesses.

## Claims

### Claim at position 1

1-20. (canceled)

### Claim 21

A method of fabricating photovoltaic cells, said method comprising the steps of:
depositing at least one layer of semiconductor material continuously on a carbon ribbon to form a composite ribbon, said layer having a free face opposite from its face in contact with the carbon ribbon;
eliminating the carbon ribbon during said method; and
applying at least one treatment to said layer of semiconductor material, from said free face in order to implement photovoltaic functions of said cells on said layer, prior to eliminating the carbon ribbon.

### Claim 22 (depends on 21)

A method according to claim 21, wherein said treatment comprises creating a plurality of contact zones by depositing a precursor material on said free face, which face is the rear face of said cells, said precursor material including dopant elements that conserve the type of the doping, n or p of said semiconductor material.

### Claim 23 (depends on 21)

A method according to claim 21, wherein said treatment comprises creating a plurality of junction zones by depositing a precursor material on said free face, which is the rear face of said cells, said precursor material including dopant elements that change the type of the doping of the semiconductor material.

### Claim 24 (depends on 22)

A method according to claim 22, wherein said treatment comprises creating a plurality of zones that insulate said contact zones electrically from said junction zones.

### Claim 25 (depends on 24)

A method according to claim 24, wherein said insulating zones are created by depositing an oxidizing material on said free face.

### Claim 26 (depends on 21)

A method according to claim 21, wherein said treatment comprises creating a plurality of junction zones by depositing a precursor material on said free face, which is the front face of said cells, said precursor material including dopant elements that change the type of the doping of the semiconductor material.

### Claim 27 (depends on 21)

A method according to claim 21, wherein said treatment comprises piercing holes in said layer of semiconductor material, substantially perpendicularly to said free face, said holes passing through said layer of semiconductor material.

### Claim 28 (depends on 27)

A method according to claim 27, wherein said piercing is performed by laser.

### Claim 29 (depends on 21)

A method according to claim 21, wherein said treatment comprises ablating the semiconductor material covering the flanks of said composite ribbon.

### Claim 30 (depends on 29)

A method according to claim 29, wherein said semiconductor material is removed by one of the following methods: laser ablation; laser ablation assisted by water jet; plasma ablation.

### Claim 31 (depends on 21)

A method according to claim 21, wherein said carbon ribbon is eliminated by being burnt off after performing the treatment.

### Claim 32 (depends on 31)

A method according to claim 31, wherein the diffusion of the dopant(s) of the precursor into said semiconductor material is implemented during the burning off of said carbon ribbon.

### Claim 33 (depends on 21)

A method according to claim 21, wherein said method includes applying at least one operation on the face of the layer of semiconductor material that is opposite from the free face, after the carbon ribbon has been eliminated.

### Claim 34 (depends on 21)

A method according to claim 21, wherein said treatment is performed continuously.

### Claim 35 (depends on 21)

A method according to claim 21, wherein said composite ribbon is cut up to form composite strips of great length, said treatment being applied to said composite strips.

### Claim 36 (depends on 35)

A method according to claim 35, wherein strips of semiconductor material of great length are obtained by eliminating the carbon from said composite strips, and in that at least one of the following operations is performed on said strips of semiconductor material: texturing the front faces of the photovoltaic cells; implementing junction zones; depositing an antireflection layer on the front faces of the cells; depositing electric contacts on the front and rear faces of the cells.

### Claim 37 (depends on 35)

A method according to claim 35, wherein said strips are of a length lying in the range 1.0 m to 4.50 m.

### Claim 38 (depends on 21)

A method according to claim 21, wherein said semiconductor material is silicon.

### Claim 39 (depends on 21)

A method according to claim 21, wherein said composite ribbon is fabricated by the RGS method, said ribbon then comprising two layers of semiconductor material surrounding said carbon ribbon, each of the two layers of semiconductor material having a free face on which said treatment is applied.

### Claim 40 (depends on 22)

A method according to claim 22, wherein said precursor material is based on an oxide filled with boron if it is desired to increase p-type doping or filled with phosphorous if it is desired to increase n-type doping.

### Claim 41 (depends on 21)

A semiconductor product, wherein said product is obtained by using the method defined in claim 21.