# US 2008/0188630 A1 · One pot procedure for poly (glycidyl nitrate) end modification

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0188630 A1
- Document ID: US20080188630A1
- Status: Published application
- Kind: A1
- Application number: 11/553,752
- Filed: 2006-10-27
- Published: 2008-08-07
- Earliest claimed: 2006-10-27
- Assignees: Alliant Techsystems Inc.
- Inventors: Alexander J. Paraskos; Michael A. Dewey; Wayne Edwards
- Web page: https://patentgrep.com/patent/US20080188630A1

## CPC

- C06B 45/105: {The resin being a polymer bearing energetic groups or containing a soluble organic explosive}
- C06B: EXPLOSIVES OR THERMIC COMPOSITIONS (blasting F42D); MANUFACTURE THEREOF; USE OF SINGLE SUBSTANCES AS EXPLOSIVES (compounds in general C01, C07 or C08; {demolition agents based on cementitious or like materials C04B41/0009})

## Abstract

A method is provided in which PGN is end-modified in a process using a single solvent. The resulting end-modified PGN may be stably crosslinked using aliphatic polyisocyanates. Further provided are methods of producing energetic compositions comprising PGN which has been end-modified in a process using a single solvent. Such energetic compositions may be stably crosslinked using aliphatic polyisocyanates.

## Claims

### Claim 1

A method of end-modifying PGN, the method comprising:
end-modifying PGN in a single solvent to create the following chemical structure:

### Claim 2 (depends on 1)

The method according to claim 1, wherein end-modifying in a single solvent is conducted by end-modifying in tetrahydrafuran.

### Claim 3 (depends on 1)

The method according to claim 1, further comprising epoxidating PGN.

### Claim 4 (depends on 1)

The method according to claim 1, further comprising epoxidating PGN in the presence of a base.

### Claim 5 (depends on 4)

The method according to claim 4, further comprising selecting the base from the group consisting of KOH, NaOH, potassium t-butoxide, lithium diisopropyl amide, and potassium 2-methyl-2-butoxide.

### Claim 6 (depends on 3)

The method according to claim 3, further comprising washing a reaction product of epoxidating PGN.

### Claim 7 (depends on 16)

The method according to claim 16, further comprising washing a reaction product of epoxidating PGN in solution of sodium chloride or H2SO4.

### Claim 8 (depends on 3)

The method according to claim 3, further comprising washing a reaction product of epoxidating PGN until a residual nitrate level is less than 1%.

### Claim 9 (depends on 1)

The method according to claim 1 further comprising adjusting the pH end-modified PGN to about or below 7.

### Claim 10

A method for producing an energetic composition, the method comprising:
creating, in a single solvent, an end-modified PGN having the following chemical structure:
preparing an energetic formulation comprising the end-modified PGN.

### Claim 11 (depends on 10)

The method according to claim 10, further comprising cross-linking the energetic formulation comprising the end-modified PGN.

### Claim 12 (depends on 10)

The method according to claim 10, further comprising cross-linking the energetic formulation comprising the end-modified PGN with an aliphatic polyisocyanate.

### Claim 13 (depends on 10)

The method according to claim 10, further comprising selecting the single solvent to be tetrahydrafuran.

### Claim 14 (depends on 10)

The method according to claim 10, further comprising epoxidating PGN.

### Claim 15 (depends on 10)

The method according to claim 10, further comprising epoxidating PGN in the presence of a base.

### Claim 16 (depends on 15)

The method according to claim 15, further comprising selecting the base from the group consisting of KOH, NaOH, potassium t-butoxide, lithium diisopropyl amide, and potassium 2-methyl-2-butoxide.

### Claim 17 (depends on 14)

The method according to claim 14, further comprising washing a reaction product of epoxidating PGN.

### Claim 18 (depends on 17)

The method according to claim 17, further comprising washing a reaction product of epoxidating PGN in solution of sodium chloride or H2SO4.

### Claim 19 (depends on 14)

The method according to claim 14, further comprising washing a reaction product of epoxidating PGN until a residual nitrate level is less than 1%.

### Claim 20 (depends on 10)