# US 2008/0188609 A1 · Epoxy compositions having improved impact resistance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0188609 A1
- Document ID: US20080188609A1
- Status: Published application
- Kind: A1
- Application number: 12/035,274
- Filed: 2008-02-21
- Published: 2008-08-07
- Earliest claimed: 2005-08-24
- Assignees: Henkel AG & Co. KGaA; Loctite (R&D) Limited
- Inventors: Rajat Agarwal; Olaf Lammerschop; Rainer Schoenfeld; Hubert K. Schenkel; Barry N. Burns; Matthew J. Holloway; Mary B. Ward; Martin J. Fitzpatrick; Jonathan P. Wigham
- Web page: https://patentgrep.com/patent/US20080188609A1

## CPC

- C08L 51/04: grafted on to rubbers
- C08L 63/00: Compositions of epoxy resins; Compositions of derivatives of epoxy resins
- C09J 163/00: Adhesives based on epoxy resins; Adhesives based on derivatives of epoxy resins
- C08L 2666/02: Organic macromolecular compounds, natural resins, waxes or and bituminous materials
- C08L 2666/08: Homopolymers or copolymers according to C08L7/00 - C08L21/00; Derivatives thereof
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

This invention relates to compositions useful as adhesives and more particularly to the preparation of heat-cured epoxy-based adhesive compositions with improved impact resistance and good adhesion to oily metal substrates.

## Claims

### Claim 1

A composition comprising:
A) at least one epoxy resin;
B) rubber particles having a core-shell structure;
C) at least one auxiliary impact modifier/toughening agent; and
D) at least one heat-activated latent curing agent.

### Claim 2 (depends on 1)

The composition of claim 1 additionally comprising at least one filler selected from the group consisting of platy fillers, hollow glass microspheres and combinations thereof.

### Claim 3 (depends on 1)

The composition of claim 1 additionally comprising at least one chelate-modified epoxy resin.

### Claim 4 (depends on 1)

The composition of claim 1 in which the at least one epoxy resin is selected from the group consisting of diglycidyl ethers of bisphenol A and bisphenol F.

### Claim 5 (depends on 1)

The composition of claim 1 comprising from about 0.1 to about 3 weight percent of at least one chelate-modified epoxy resin.

### Claim 6 (depends on 1)

The composition of claim 1 comprising at least one substituted guanidine heat-activated latent curing agent.

### Claim 7 (depends on 1)

The composition of claim 1 comprising from about 5 to about 25 weight percent of said rubber particles having a core-shell structure.

### Claim 8 (depends on 1)

The composition of claim 1 wherein said rubber particles have a core comprised of a diene homopolymer, diene copolymer or polysiloxane elastomer.

### Claim 9 (depends on 1)

The composition of claim 1 wherein said rubber particles have a shell comprised of an alkyl (meth)acrylate homopolymer or copolymer.

### Claim 10 (depends on 1)

The composition of claim 1 wherein said rubber particles have an average diameter of from about 25 to about 200 nm.

### Claim 11 (depends on 1)

The composition of claim 1 wherein the weight ratio of epoxy resin: combined weight of auxiliary impact modifier/toughener and rubber particles having a core-shell structure is from about 0.2:1 to about 3:1.

### Claim 12 (depends on 1)

The composition of claim 1 wherein the weight ratio of auxiliary impact modifier/toughener: rubber particles is from about 0.2:1 to about 5:1.

### Claim 13 (depends on 1)

The composition of claim 1 additionally comprising at least one reactive diluent which is a mono-epoxide.

### Claim 14 (depends on 1)

The composition of claim 1 comprising from about 25 to about 55 weight percent of epoxy resin.

### Claim 15 (depends on 1)

The composition of claim 1 comprising from about 5 to about 40 weight percent of auxiliary impact modifier/toughener.

### Claim 16 (depends on 1)

The composition of claim 1 comprising from about 25 to about 55 weight percent epoxy resin, from about 5 to about 40 weight percent auxiliary impact modifier/toughener, and from about 5 to about 25 weight percent rubber particles having a core-shell structure, wherein the weight ratio of epoxy resin: combined weight of auxiliary impact modifier/toughener and rubber particles having a core-shell structure is from about 0.2:1 to about 3:1 and the weight ratio of auxiliary impact modifier/toughener: rubber particles is from about 0.2:1 to about 5:1.

### Claim 17 (depends on 1)

The composition of claim 1 wherein at least a portion of the rubber particles having a core-shell structure have an average diameter of from about 25 to about 200 nm and are stably dispersed in a masterbatch comprised of epoxy resin when combined with the other components of the composition, with said rubber particles having a core comprised of a polymer or copolymer of 1,4-butadiene having a glass transition temperature of not greater than −40° C.

### Claim 18 (depends on 1)

The composition of claim 1 wherein said at least one auxiliary impact modifier/toughening agent is selected from the group consisting of epoxy-based prepolymers obtained by reacting one or more amine-terminated polymers with one or more epoxy resins.

### Claim 19 (depends on 1)

The composition of claim 1 wherein said at least one auxiliary impact modifier/toughening agent is selected from the group consisting of reaction products of isocyanate-terminated prepolymers and hydroxyl-containing epoxides.

### Claim 20 (depends on 1)

The composition of claim 1 wherein said at least one auxiliary impact modifier/toughening agent is selected from the group consisting of reaction products of isocyanate-terminated prepolymers and compounds having one or more phenolic, benzyl alcohol, aminophenyl or benzylamino groups per molecule.

### Claim 21 (depends on 1)

The composition of claim 1 wherein said at least one auxiliary impact modifier/toughening agent is selected from the group consisting of polystyrene-1,4-polybutadiene-polymethylmethacrylate block copolymers.

### Claim 22 (depends on 1)

The composition of claim 1 wherein said at least one auxiliary impact modifier/toughening agent is selected from the group consisting of adducts of dimeric fatty acids with epoxy resins.

### Claim 23 (depends on 1)

The composition of claim 1 wherein said at least one auxiliary impact modifier/toughening agent is a polymeric or oligomeric material having a glass transition temperature below −30 C and containing one or more functional groups selected from the group consisting of epoxy groups, carboxylic acid groups, amino groups and hydroxyl groups.

### Claim 24 (depends on 1)

A method of making a composite article which comprises: contacting a surface with the composition of claim 1 and curing the composition in contact with the surface to prepare a composite article.

### Claim 25 (depends on 24)

The method of claim 24 in which the surface is metal.

### Claim 26 (depends on 24)

The method of claim 24 in which at least two surfaces are contacted with the composition and cured in contact therewith.

### Claim 27 (depends on 24)

The method of claim 24 wherein the surface is contaminated with at least one oily substance and the composition additionally comprises at least one chelate-modified epoxy resin.