Autoxidisable Architectural Coating Compositions
AssigneeImperial Chemical Industries PLC
InventorPhilip Louis Taylor
Life of this patent
Estimating the term…
Loading patent…
AssigneeImperial Chemical Industries PLC
InventorPhilip Louis Taylor
Estimating the term…
An autoxidisable architectural coating composition suitable for application to surfaces found in and around buildings at ambient temperatures and in natural daylight wherein surface autoxidation of the composition is promoted by a combination of low concentrations of metal ions (especially manganese or vanadium) and 2,2-dimethoxy 1,2-diphenylethan-1-one as photoinitiator. The composition avoids the need to use more than trace amounts cobalt ions which are rumoured to be carcinogenic yet achieves adequately fast rates of autoxidation. Preferably the use of cobalt is a avoided altogether. The use of the low concentrations of the other metal ions reduces discolouration of the compositions often to levels below what is achieved using conventional cobalt promoters. Also a modification in which surface autoxidation is promoted by a combination of 2,2-dimethoxy-1,2-diphenylethan-1-one and trace amounts of cobalt ions in the absence of other surface autoxidation promoting metal ions. Finally, a method for applying the autoxidisable coatings to surfaces under ambient temperatures in which they are subjected to natural daylight or similar low energy irradiation is disclosed.
An autoxidisable architectural coating composition suitable for application to surfaces at an ambient temperatures and in natural daylight which composition contains an autoxidisable binder polymer and a promoter system for promoting autoxidation of the autoxidisable binder polymer wherein the system comprises
A method for applying a dried coat of an architectural coating composition to a surface in which a liquid coating of the composition is applied to the surface at ambient temperatures wherein the composition contains an autoxidisable binder polymer and a system for promoting surface autoxidation of the autoxidisable binder polymer and wherein the system is as described in any one of the preceding claims and the coating composition is exposed to low energy irradiation by light of wavelength in the range 200 to 750 nm.
Dependencies are inferred from the claim text.