# US 2008/0188575 A1 · Process for the Preparation, Under Subcritical Conditions, of Monolithic Xerogels and Aerogels of Silica/Latex Hybrids, Modified with Alkoxysilane Groups

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0188575 A1
- Document ID: US20080188575A1
- Status: Published application
- Kind: A1
- Application number: 11/910,716
- Filed: 2006-04-04
- Published: 2008-08-07
- Earliest claimed: 2005-04-05
- Assignees: Instituto Superior Tecnico
- Inventors: Jose Manuel Gaspar Martinho; Laura Maria Ilharco De Almeida Santos; Jose Paulo Sequira Farinha; Alexandra Marina Abrantes Fidalgo; Pedro Oliveira Martinho
- Web page: https://patentgrep.com/patent/US20080188575A1

## CPC

- B01J 13/0091: {Preparation of aerogels, e.g. xerogels}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

The invention relates to a process for the preparation of monolithic xerogels and aerogels of silica/latex hybrids under subcritical conditions. In the two-stage synthesis of these alcogels in the presence of an acid-base catalyst, the hydrolysis and polycondensation of a silicon alkoxide are carried out in an organic medium containing excess water. A latex consisting of polybutyl methacrylate and polybutyl acrylate, modified with alkoxysilane groups, is first synthesized and then incorporated in the mixture either in the first stage in order to effect its co-hydrolysis with the silicon alkoxide, or in the second stage to effect its co-condensation with the previously hydrolysed colloidal silica. The resulting alcogels are aged, washed, and dried under subcritical conditions. This process gives hybrid products containing 0.1-50 wt-% of latex and having a density of 300-1300 kg/m3, a porosity of 40-85%, a specific surface area of 400-900 m2/g and a mean pore diameter of 2-12 nm. The products are resistant to atmospheric humidity and moisture, have better mechanical properties than the corresponding inorganic products, and can be used as thermal, acoustic and electrical insulators.

## Claims

### Claim 1

Process for the preparation of monolithic silica/latex hybrid xerogels and aerogels under subcritical conditions, comprising the following steps:
the hybrid gels are synthesized by the acid hydrolysis of a silicon alkoxide with excess water in an organic solvent, after which the hydrolysed sol obtained is subjected to polycondensation under alkaline conditions;
colloidal polymer particles containing alkoxysilane groups are prepared in the form of an aqueous dispersion and are incorporated in the above mixture, either in the first stage for co-hydrolysis with the silicon alkoxide, or in the second stage for co-condensation with the previously hydrolysed colloidal silica;
the gels thus obtained are aged, washed, and then dried under subcritical conditions in an atmosphere almost fully saturated with the solvent used for washing them;
the dry hybrid gels obtained have a density of 300-1300 kg/m3, a porosity of 40-85%, a specific surface area of 400-900 m2/g and a mean pore diameter of 2-12 nm;
the dry hybrid gels are resistant to atmospheric humidity and moisture, have better mechanical properties than the corresponding inorganic materials, and can be used as thermal, acoustic and electrical insulators.

### Claim 2 (depends on 1)

Process according to claim 1, characterized in that the silicon alkoxide is an alkoxysilane with a short alkyl chain, being for example tetraethoxysilane (TEOS) or tetramethoxysilane (TMOS).

### Claim 3 (depends on 2)

Process according to claim 2, characterized in that the amount of silicon alkoxide in the starting solution is 10-50 wt-%.

### Claim 4 (depends on 3)

Process according to claim 3, characterized in that the molar ratio between water and tetraethoxysilane is 2-10.

### Claim 5 (depends on 1)

Process according to claim 1, characterized in that the co-solvent is a polar protonic solvent, such as an alcohol or a mixture of alcohols chosen from amongst methanol, ethanol, propanol, isopropanol and butanol.

### Claim 6 (depends on 1)

Process according to claim 1, characterized in that the hydrolysis is catalysed by a strong acid, such as hydrochloric acid.

### Claim 7 (depends on 6)

Process according to claim 6, characterized in that the hydrolysis is carried out at a pH lower than 2.7.

### Claim 8 (depends on 7)

Process according to claim 7, characterized in that the duration of the hydrolysis is limited to 60 minutes.

### Claim 9 (depends on 1)

Process according to claim 1, characterized in that the polycondensation is catalysed by an alkaline catalyst, such as ammonia (NH4OH).

### Claim 10 (depends on 9)

Process according to claim 9, characterized in that the polycondensation is carried out at a pH of 5-8.

### Claim 11 (depends on 1)

Process according to claim 1, characterized in that 0.1-50 wt-% of colloidal polymer particles are incorporated in the hybrid material.

### Claim 12 (depends on 1)

Process according to claim 1, characterized in that colloidal polymer particles that have a core-and-crown structure and a mean diameter of 30-1000 nm are prepared and incorporated in the hybrid material.

### Claim 13 (depends on 12)

Process according to claim 12, characterized in that the colloidal polymer particles prepared and incorporated in the hybrid material consist of a polymer, a copolymer or a mixture of polymers with a glass transition temperature close to or below room temperature, such as for example n-butyl methacrylate-n-butyl acrylate copolymer.

### Claim 14 (depends on 13)

Process according to claim 13, characterized in that the colloidal polymer particles prepared and incorporated in the hybrid material have cross-linked core and crown.

### Claim 15 (depends on 14)

Process according to claim 14, characterized in that the outer crown of the colloidal polymer particles prepared and incorporated in the hybrid material is modified with alioxysilane groups that are covalently linked to the polymer.

### Claim 16 (depends on 1)

Process according to claim 1, characterized in that an aqueous dispersion of the colloidal polymer particles is added to the mixture of silicon alkoxide, water and co-solvent before the introduction of the acid catalyst.

### Claim 17 (depends on 1)

Process according to claim 1, characterized in that the aqueous dispersion of the colloidal polymer particles is added to the previously hydrolysed mixture immediately before, simultaneously with, or immediately after the introduction of a base used as a catalyst.

### Claim 18 (depends on 16)

Process according to claim 16, characterized in that the gels are synthesized at a temperature between room temperature and a value close to the boiling point of the solvent.

### Claim 19 (depends on 1)

Process according to claim 1, characterized in that the gel is aged in a suitable medium, which may be the residual sol, a mixture of the residual sol, water and a solvent, or a mixture of the residual sol, silicon alkoxide, water and a solvent, used in various proportions.

### Claim 20 (depends on 19)

Process according to claim 19, characterized in that the gel is aged in two stages: first in the residual solution and then in a mixture of the residual solution, silicon alkoxide, water and a solvent.

### Claim 21 (depends on 20)

Process according to claim 20, characterized in that the ageing is carried out at a temperature that leaves the hybrid gel intact.

### Claim 22 (depends on 21)

Process according to claim 21, characterized in that the aged gel is washed with a C1-C5 monohydric, dihydric or trihydric aliphatic alcohol.

### Claim 23 (depends on 22)

Process according to claim 22, characterized in that the washing is carried out at a temperature that leaves the hybrid gel intact.

### Claim 24 (depends on 23)

Process according to claim 23, characterized in that the subsequent drying of the alcogel is carried out under subcritical conditions.

### Claim 25 (depends on 24)

Process according to claim 24, characterized in that the drying is carried out in an atmosphere that is almost fully saturated with the washing solvent and at a temperature that is between room temperature and a value close to the boiling point of the washing solvent.

### Claim 26 (depends on 1)

Use of the alcogels and their hybrids, prepared according to claim 1, characterized in that they are employed as thermal insulators.

### Claim 27 (depends on 1)

Use of the alcogels and their hybrids, prepared according to claim 1, characterized in that they are employed as sound insulators.

### Claim 28 (depends on 1)

Use of the alcogels and their hybrids, prepared according to claim 1, characterized in that they are employed as electrical insulators.