# US 2008/0188163 A1 · Method of polishing a substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0188163 A1
- Document ID: US20080188163A1
- Status: Published application
- Kind: A1
- Application number: 12/055,621
- Filed: 2008-04-23
- Published: 2008-08-07
- Earliest claimed: 2005-09-19
- Assignees: Rohm and Haas Electronic Materials CMP Holdings, Inc.
- Inventors: Chau H. Duong
- Web page: https://patentgrep.com/patent/US20080188163A1

## CPC

- B24B 37/24: characterised by the composition or properties of the pad materials
- C08L 75/04: Polyurethanes
- C08K 7/22: Expanded, porous or hollow particles
- C08L 33/06: of esters containing only carbon, hydrogen and oxygen, which oxygen atoms are present only as part of the carboxyl radical
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A method for polishing a substrate using a pad comprising, a polymeric matrix having microspheres dispersed therein, the polymeric matrix being formed of a water-based polymer or blends thereof, wherein the polymeric matrix is applied on a permeable substrate, and wherein the polishing pad exhibits reduced defectivity and improved polishing performance are provided.

## Claims

### Claim 1

A chemical mechanical planarization method comprising: providing a chemical mechanical polishing pad comprising,
a permeable substrate having a thickness of 2-100 mils; and
a polishing layer comprising a polymeric matrix having microspheres dispersed therein, wherein the polymeric matrix is formed of a water-based polymer blend, wherein the polishing layer is applied on the permeable substrate, wherein the polymeric matrix comprises a blend of 3:1 to 1:3 (by weight) of an aqueous urethane dispersion and an acrylic dispersion, wherein the microspheres are gas filled, wherein the polymeric matrix contains at least 0.3 volume percent microspheres, wherein the microspheres have a weight average diameter of 10-100 μm, wherein the polishing layer has grooves formed therein; and, wherein the chemical mechanical polishing pad exhibits improved defectivity.

### Claim 2 (depends on 1)

The method of claim 1, wherein the polymeric matrix penetrates and binds to the permeable substrate.

### Claim 3 (depends on 1)

The method of claim 1, wherein the permeable substrate is a woven or a non-woven web.

### Claim 4 (depends on 1)

The method of claim 1, wherein the polymeric matrix comprises a blend of 3:1 (by weight) of an aqueous urethane dispersion and an acrylic dispersion.

### Claim 5

A chemical mechanical planarization method comprising: providing a chemical mechanical polishing pad comprising,
a permeable substrate having a thickness of 2-100 mils; and
a polishing layer comprising a polymeric matrix having microspheres dispersed therein, wherein the polymeric matrix is formed of a water-based polymer blend, wherein the polishing layer is applied on the permeable substrate, wherein the polymeric matrix comprises a blend of 3:1 to 1:3 (by weight) of an aqueous urethane dispersion and an acrylic dispersion, wherein the microspheres are gas filled, wherein the polymeric matrix contains at least 0.3 volume percent microspheres, wherein the microspheres have a weight average diameter of 10-100 μm, wherein the polishing layer has grooves formed therein; and, wherein the chemical mechanical polishing pad exhibits improved defectivity, where the chemical mechanical polishing pad creates less than 300 total defects on the surface of a copper sheet wafer when the chemical mechanical polishing pad is used to polish the copper sheet wafer on a polishing machine, under downforce conditions of 1.5 psi, a polishing solution flow rate of 150 cc/min, a platen speed of 120 RPM and a carrier speed of 114 RPM to polish copper sheet wafers.

### Claim 6 (depends on 5)