# US 2008/0188101 A1 · Contact, Method For Manufacturing Contact, Connection Device Including Contact, And Method For Manufacturing Connection Device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0188101 A1
- Document ID: US20080188101A1
- Status: Published application
- Kind: A1
- Application number: 11/908,768
- Filed: 2006-03-07
- Published: 2008-08-07
- Earliest claimed: 2005-03-16
- Assignees: Alps Electric Co., Ltd.
- Inventors: Shin Yoshida; Shinichi Nagano
- Web page: https://patentgrep.com/patent/US20080188101A1

## CPC

- H01R 13/03: characterised by the material, e.g. plating, or coating materials
- H01R 13/2421: {using coil springs}
- Y10T 29/49002: Electrical device making
- H01R: ELECTRICALLY-CONDUCTIVE CONNECTIONS; STRUCTURAL ASSOCIATIONS OF A PLURALITY OF MUTUALLY-INSULATED ELECTRICAL CONNECTING ELEMENTS; COUPLING DEVICES; CURRENT COLLECTORS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

To provide a contact, formed in an amorphous state, having better spring properties as compared to conventional one; a method for manufacturing the contact; a connection device including the contact; and a method for manufacturing the connection device. The present invention provides a contact comprising an elastically deforming portion that includes at least one amorphous part. The elastically deforming portion includes an auxiliary elastic member 41 made of, for example, NiP (a P content of 15 atomic percent). In this case, an amorphous phase 50 is predominant in the auxiliary elastic member 41. This enhances spring properties such as a yield stress

## Claims

### Claim at position 1

1-25. (canceled)

### Claim 26

A contact comprising an elastically deforming portion, wherein the elastically deforming portion is three-dimensionally shaped under heating conditions at a temperature suitable for maintain at least one part of the elastically deforming portion in an amorphous state.

### Claim 27 (depends on 26)

The contact according to claim 26, wherein the elastically deforming portion includes at least one part made of Ni—X (where X is at least one selected from the group consisting of P, W, and B) and the Ni—X is amorphous.

### Claim 28 (depends on 27)

The contact according to claim 27, wherein the elastically deforming portion includes a conductive member and an auxiliary elastic member, the conductive member has a resistivity less than that of the auxiliary elastic member, and the auxiliary elastic member has a yield point and elastic modulus greater than those of the conductive member and is made of the Ni—X.

### Claim 29 (depends on 27)

The contact according to claim 27, further comprising ultra-fine precipitates, having a size of 1 nm or less, other than amorphous portions.

### Claim 30 (depends on 26)

The contact according to claim 26, wherein the elastically deforming portion has such a yield point that the load applied thereto is 19.6 mN or more and the distortion thereof is 0.1 mm or more.

### Claim 31 (depends on 26)

The contact according to claim 26, wherein the elastically deforming portion has a convex shape.

### Claim 32 (depends on 26)

The contact according to claim 26, wherein the elastically deforming portion has a conical, spiral shape.

### Claim 33 (depends on 26)

The contact according to claim 26, wherein the Ni—X is P.

### Claim 34

A method for manufacturing a contact including an elastically deforming portion, comprising:
(a) a step of forming at least one part of the elastically deforming portion using Ni—X (where X is at least one selected from the group consisting of P, W, and B); and
(b) a step of three-dimensionally shaping the elastically deforming portion under heating conditions,
wherein the heating temperature in the step (b) is suitable for maintaining the Ni—X in an amorphous state.

### Claim 35 (depends on 34)

The contact-manufacturing method according to claim 34, wherein the heating temperature in the step (b) is lower than the crystallization temperature of the Ni—X.

### Claim 36 (depends on 34)

The contact-manufacturing method according to claim 34, wherein the elastically deforming portion is three-dimensionally shape under heating conditions in such a manner that a stress in the plastic region of the Ni—X is applied to the elastically deforming portion.

### Claim 37 (depends on 35)

The contact-manufacturing method according to claim 35, wherein the heating temperature is 200° C. to 300° C.

### Claim 38 (depends on 35)

The contact-manufacturing method according to claim 35, wherein the heating temperature is 200° C. to 700° C.