# US 2008/0188074 A1 · Peeling-free porous capping material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0188074 A1
- Document ID: US20080188074A1
- Status: Published application
- Kind: A1
- Application number: 11/728,623
- Filed: 2007-03-27
- Published: 2008-08-07
- Earliest claimed: 2007-02-06
- Inventors: I-I Chen; Fang Wen Tsai; Zhen-Cheng Wu; Tien-I Bao; Shwang-Ming Jeng; Chen-Hua Yu
- Web page: https://patentgrep.com/patent/US20080188074A1

## CPC

- H10W 20/46: comprising air gaps
- H10W 20/071: {of dielectric parts thereof}
- H10W 20/072: {of dielectric parts comprising air gaps}
- H10W 20/074: {of dielectric parts comprising thin functional dielectric layers, e.g. dielectric etch-stop, barrier, capping or liner layers}
- H10W 20/47: comprising two or more dielectric layers having different properties, e.g. different dielectric constants
- H10W 20/48: Insulating materials thereof
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming a cap layer for an interconnect structure is provided. The method includes providing a substrate; depositing a low-k dielectric layer comprising a first porogen over the substrate; depositing a low-k cap layer comprising a second porogen on the low-k dielectric layer; and curing the low-k dielectric layer and the low-k cap layer simultaneously to remove the first and the second porogens, so that a first porosity in the low-k dielectric layer and a second porosity in the low-k cap layer are created. The second porosity is preferably less than the first porosity. Preferably, the low-k dielectric layer and the low-k cap layer comprise a common set of precursors and porogens, and are in-situ performed.

## Claims

### Claim 1

A method for forming a dielectric structure, the method comprising:
providing a substrate;
depositing a first low-k dielectric layer comprising a first porogen over the substrate;
depositing a second low-k dielectric layer comprising a second porogen on the first low-k dielectric layer; and
curing the first and the second low-k dielectric layers simultaneously to remove the first and the second porogens and to create a first porosity in the first low-k dielectric layer and a second porosity in the second low-k dielectric layer, wherein the second porosity is less than the first porosity.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first and the second porogens comprise same materials, and wherein the deposition of the first low-k dielectric layer and the second low-k dielectric layer comprise a common set of precursors.

### Claim 3 (depends on 2)

The method of claim 2, wherein a porogen percentage in the second low-k dielectric layer is less than a porogen percentage in the first low-k dielectric layer by greater than about 5 percent.

### Claim 4 (depends on 1)

The method of claim 1, wherein the step of depositing the first low-k dielectric layer comprises a higher porogen-to-precursor ratio than the step of depositing the second low-k dielectric layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first and the second low-k dielectric layers are formed by a chemical vapor deposition method.

### Claim 6 (depends on 1)

The method of claim 1, wherein the step of curing the first and the second low-k dielectric layers is performed using a method selected from the group consisting essentially of ultraviolet curing, eBeam curing, thermal curing, SCCO2 curing, and combinations thereof.

### Claim 7 (depends on 1)

The method of claim 1 further comprising an additional ultraviolet curing process.

### Claim 8 (depends on 1)

The method of claim 1, wherein the step of curing is performed in an environment containing a bond-repairing material.

### Claim 9 (depends on 8)

The method of claim 8, wherein the bond repairing material comprises a carbon-containing gas.

### Claim 10 (depends on 1)

The method of claim 1, wherein the first low-k dielectric layer has a k value of less than about 2.5, and the second low-k dielectric layer has a k value of less than about 2.7.

### Claim 11 (depends on 1)

The method of claim 1, wherein the first low-k dielectric layer has a porosity of less than about 25 percent, and the second low-k dielectric layer has a porosity of less than about 35 percent.

### Claim 12 (depends on 1)

The method of claim 1, wherein the first low-k dielectric and the second low-k dielectric layer have over 85 percent materials in common.

### Claim 13

A method for forming a dielectric structure, the method comprising:
providing a substrate;
depositing a low-k dielectric layer comprising a porogen over the substrate;
in-situ depositing a low-k cap layer comprising the porogen on the low-k dielectric layer, wherein the low-k dielectric layer and the low-k cap layer are formed of substantially same precursors; and
curing the low-k dielectric layer and the low-k cap layer simultaneously to remove the porogen and to create a first porosity in the low-k dielectric layer and a second porosity in the low-k cap layer, wherein the second porosity is less than the first porosity.

### Claim 14 (depends on 13)

The method of claim 13, wherein the step of depositing the low-k dielectric layer uses a higher RF power than the step of depositing the low-k cap layer.

### Claim 15 (depends on 13)

The method of claim 13, wherein the step of depositing the low-k dielectric layer has a higher porogen-to-precursor ratio than the step of depositing the low-k cap layer.

### Claim 16 (depends on 13)

The method of claim 13, wherein the step of curing the low-k dielectric layer and the low-k cap layer comprises a first curing and a second curing.

### Claim 17 (depends on 16)

The method of claim 16, wherein the first curing is a UV curing using a radiation having a longer wavelength than the second curing.

### Claim 18 (depends on 16)

The method of claim 16, wherein the first curing uses a wavelength of between about 250 nm and about 280 nm, and the second curing uses a wavelength of between about 200 nm and about 300 nm.

### Claim 19 (depends on 13)

The method of claim 13, wherein the step of curing is performed in an ambient comprising CxHy.

### Claim 20 (depends on 19)

The method of claim 19, wherein CxHy comprises a material selected from the group consisting essentially of C2H4, C3H6, HMDS, and combinations thereof.

### Claim 21

A semiconductor structure comprising:
a substrate;
a low-k dielectric layer over the substrate; and
a low-k cap layer on the low-k dielectric layer, wherein the low-k dielectric layer and the low-k cap layer comprise substantially similar materials, and wherein a first porosity in the low-k dielectric layer is greater than a second porosity in the low-k cap layer.

### Claim 22 (depends on 21)

The semiconductor structure of claim 21, wherein the low-k dielectric layer has a k value less than a k value of the low-k cap layer.

### Claim 23 (depends on 22)

The semiconductor structure of claim 22, wherein the low-k dielectric layer has a k value of less than about 2.5 and the low-k cap layer has a k value of less than about 2.7.

### Claim 24 (depends on 21)

The semiconductor structure of claim 21, wherein the low-k dielectric layer has a porosity of less than about 35 percent and the low-k cap layer has a porosity of less than about 25 percent.

### Claim 25 (depends on 21)

The semiconductor structure of claim 21, wherein a hardness of the low-k cap layer is greater than a hardness of the low-k dielectric layer by about 10 percent.

### Claim 26 (depends on 21)

The semiconductor structure of claim 21, wherein a porosity of the low-k cap layer is less than a porosity of the low-k dielectric layer by about 1.2 percent.

### Claim 27 (depends on 21)

The semiconductor structure of claim 21, wherein the low-k dielectric layer and the low-k cap layer comprises organosilicate glass.

### Claim 28 (depends on 21)

The semiconductor structure of claim 21, wherein the low-k dielectric layer and the low-k cap layer comprise a carbon-containing material.

### Claim 29 (depends on 21)

The semiconductor structure of claim 21 further comprising a metal feature extending from a top surface of the low-k cap layer to a bottom surface of the low-k dielectric layer.

### Claim 30 (depends on 21)