# US 2008/0188046 A1 · Method and Apparatus For Manufacturing A Semiconductor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0188046 A1
- Document ID: US20080188046A1
- Status: Published application
- Kind: A1
- Application number: 11/671,158
- Filed: 2007-02-05
- Published: 2008-08-07
- Earliest claimed: 2007-02-05
- Assignees: Infineon Technologies North America Corp.; Samsung Electronics Co., Ltd.
- Inventors: Matthias Hierlemann; Ja-Hum Ku
- Web page: https://patentgrep.com/patent/US20080188046A1

## CPC

- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 30/792: {comprising applied insulating layers, e.g. stress liners}
- H10D 30/795: {being in lateral device isolation regions, e.g. STI}
- H10D 62/405: {Orientations of crystalline planes}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/0188: {Manufacturing their isolation regions}
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method and apparatus for crystallizing a semiconductor that includes a first layer having a first crystal lattice orientation and a second layer having a second crystal lattice orientation, comprising amorphizing at least a portion of the second layer, applying a stress to the second layer and heating the second layer above a recrystallization temperature.

## Claims

### Claim 1

A method for crystallizing a semiconductor, comprising:
providing a semiconductor substrate comprising a first layer having a first crystal lattice orientation and a second layer having a second crystal lattice orientation different from said first crystal lattice orientation;
amorphizing a portion of said second layer;
applying an external stress to said second layer; and
heating said second layer above a recrystallization temperature of said second layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein applying said external stress comprises applying a stress liner over said second layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein applying said external stress comprises bending said second layer.

### Claim 4 (depends on 1)

The method of claim 1, further comprising forming trenches in said substrate.

### Claim 5 (depends on 1)

The method of claim 1, further comprising removing said external stress.

### Claim 6 (depends on 5)

The method of claim 5, further comprising filling isolation trenches formed in said substrate after removing said external stress.

### Claim 7 (depends on 1)

The method of claim 1, wherein amorphizing said portion of said second layer comprises implanting ions in at least said portion of said second layer at a temperature above said recrystallization temperature of said second layer.

### Claim 8 (depends on 4)

The method of claim 4 wherein applying said external stress comprises applying stress in said trenches.

### Claim 9

An apparatus for orienting a crystal structure of a semiconductor substrate comprising a first layer having a first crystal lattice orientation and a second layer having a second crystal lattice orientation different from said first crystal lattice orientation, comprising:
means for amorphizing a first set of portions of said second layer, while not amorphizing a second set of portions of said second layer;
means for applying an external stress to said second layer; and
means for annealing said substrate.

### Claim 10 (depends on 9)

The apparatus of claim 9, further comprising means for removing said stress from said second layer.

### Claim 11 (depends on 9)

The apparatus of claim 9, further comprising:
means for forming trenches in said substrate, said trenches extending from a top surface of said second layer through a bottom surface of said second layer and at least partially into said first layer.

### Claim 12 (depends on 11)

The apparatus of claim 11, further comprising means for filling said trenches after said stress is removed.

### Claim 13 (depends on 12)

The apparatus of claim 12, wherein said crystal lattice of said second layer initially has 1-0-0 orientation and said crystal lattice of said first layer has 1-1-0 orientation, and wherein said crystal lattice of said first portions of said second layer are reoriented to said 1-1-0 orientation.

### Claim 14

A method of manufacturing semiconductor devices, comprising:
providing a semiconductor substrate comprising a first layer with a first crystal orientation and a second layer with a second crystal orientation different from said first orientation;
amorphizing a first region of said second layer;
applying an external stress to said second layer;
heating said second layer above a recrystallization temperature; and
forming a first device in said first region of said second layer and a second device in a second region of said second layer.

### Claim 15 (depends on 14)

The method of claim 14, further comprising forming at least one isolation trench within said second layer.

### Claim 16 (depends on 14)

The method of claim 14, wherein said first device is a p-channel transistor and said second device is an n-channel transistor.

### Claim 17 (depends on 15)

The method of claim 15, wherein applying said external stress comprises applying said stress in said at least one isolation trench.

### Claim 18

A method of fabricating semiconductor circuits, comprising:
providing a semiconductor substrate;
amorphizing a portion of said substrate;
applying stress to said substrate;
heating said substrate above a recrystallization temperature of said substrate; and
fabricating electronic devices in said substrate.

### Claim 19 (depends on 18)

The method of claim 18, wherein said substrate comprises a first layer having a first crystal lattice orientation and a second layer having a second crystal lattice orientation different from said first crystal lattice orientation, and wherein amorphizing said portion of said substrate and fabricating said electronic devices in said substrate are performed in said second layer.

### Claim 20 (depends on 18)

The method of claim 18, further comprising removing said stress after heating said substrate above said recrystallization temperature.