# US 2008/0187781 A1 · Magnetic recording head and media overcoat

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0187781 A1
- Document ID: US20080187781A1
- Status: Published application
- Kind: A1
- Application number: 11/702,247
- Filed: 2007-02-05
- Published: 2008-08-07
- Earliest claimed: 2007-02-05
- Assignees: SAE Magnetics (H.K.) Ltd.
- Inventors: Shide Cheng; Zhu Feng; Ellis T. Cha
- Web page: https://patentgrep.com/patent/US20080187781A1

## CPC

- C23C 14/024: {Deposition of sublayers, e.g. to promote adhesion of the coating (C23C14/027 takes precedence)}
- C23C 14/0036: {Reactive sputtering}
- C23C 14/0605: {Carbon}
- C23C 14/0676: {Oxynitrides}
- G11B 5/3106: {where the integrated or assembled structure comprises means for conditioning against physical detrimental influence, e.g. wear, contamination (G11B5/3133 takes precedence)}
- G11B 5/7264: {Inorganic carbon protective coating, e.g. graphite, diamond like carbon or doped carbon}
- G11B 5/8408: {protecting the magnetic layer}
- G11B 5/40: Protective measures on heads, e.g. against excessive temperature (G11B5/31 takes precedence; protection against wear G11B5/255 {; protective structure of the head: see under structures, e.g. G11B5/3106})
- Y10T 428/115: Magnetic layer composition
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for forming a protective bilayer on a substrate that is a magnetic read/write head or a magnetic recording medium. The bilayer is formed as an adhesion enhancing and corrosion resistant underlayer and a protective diamond-like carbon (DLC) overlayer. The underlayer is formed of silicon oxynitride, having the general formula SiOxNy, where x can be within the range between 0.02 and 2.0 and y is in the range between approximately 0.01 and 1.5. By adjusting the values of x and y the underlayer contributes to such qualities as strong chemical bonding between the substrate and the DLC, wear and corrosion resistance, chemical and mechanical stability and low electrical conductivity. The underlayer may be formed by various methods such as reactive ion sputtering, plasma assisted chemical vapor deposition, reactive pulsed laser deposition, plasma surface treatment and plasma immersion ion implantation.

## Claims

### Claim 1

A protected magnetic read/write head or magnetic recording medium comprising:
the read/write head or recording medium;
a protective bilayer formed on said head or recording medium, the bilayer further comprising:
an underlayer formed as a layer of SiOxNy on an cleaned substrate surface of said head or recording medium;
a DLC outer layer formed on said underlayer.

### Claim 2 (depends on 1)

The protected read/write head or recording medium of claim 1 wherein x is in the range between approximately 0.02 and 2.0 and y is in the range between approximately 0.01 and 1.5.

### Claim 3 (depends on 1)

The protected read write head or recording medium of claim 1 wherein said underlayer is formed to a thickness less than approximately 50 angstroms.

### Claim 4 (depends on 1)

The protected read write head or recording medium of claim 1 wherein said underlayer is formed to a thickness less than approximately 20 angstroms.

### Claim 5 (depends on 1)

The protected read write head or recording medium claim 1 wherein x and y vary as a function of the underlayer thickness.

### Claim 6 (depends on 1)

The protected read/write head or recording medium of claim 1 wherein said underlayer is formed by a process of sputtering, plasma immersion ion implantation, plasma immersion ion implantation deposition, plasma enhanced chemical vapor deposition, electron cyclotron resonance plasma deposition, or reactive pulsed laser deposition.

### Claim 7 (depends on 1)

The protected read/write head or recording medium of claim 1 wherein said underlayer is both adhesion enhancing and corrosion resistant.

### Claim 8

A method of forming a protected read/write head, a plurality of protected read/write heads or a protected magnetic recording medium comprising:
providing the read/write head, the plurality thereof or the magnetic medium;
cleaning appropriate surfaces of the read/write head, the plurality thereof or the magnetic recording medium;
forming on said surfaces an underlayer having the general formula SiOxNy;
forming on said underlayer a DLC layer.

### Claim 9 (depends on 8)

The method of claim 8 wherein x is in the range between approximately 0.02 and 2.0 and y is in the range between approximately 0.01 and 1.5.

### Claim 10 (depends on 8)

The method of claim 8 wherein said underlayer is formed by a process comprising:
providing a vacuum deposition chamber that includes a rotatable holder, a sputtering target, an apparatus for injecting a beam of reactive ions at a chosen energy and directing said ions at said sputtering target, an apparatus for injecting various gases at chosen flow rates and maintaining said gases at desired relative concentrations within said chamber;
mounting said read/write head, said plurality of such heads or said magnetic recording medium on said holder;
directing said ion beam at a sputtering target of Si, SiO2, or Si3N4;
introducing O2 gas and N2 gas at relative concentrations x and y respectively while said reactive ions are impinging on said target, thereby forming an underlayer of SiOxNy on said read/write head or plurality thereof.

### Claim 11 (depends on 10)

The method of claim 10 wherein said reactive ion beam is a beam of Ar+ ions formed by sending said beam through a voltage of between approximately 600V to 1200V.

### Claim 12 (depends on 10)

The method of claim 10 wherein said reactive ion beam is a high energy scanning focused ion beam applied so as to avoid poisoning the sputtering target and to eliminate hysteresis.

### Claim 13 (depends on 10)

The method of claim 10 wherein said reactive ion beam is a high instantaneous power pulsed ion source applied so as to avoid poisoning the sputtering target.

### Claim 14 (depends on 10)

The method of claim 10 wherein x and y are made to vary as said underlayer is being formed.

### Claim 15 (depends on 10)

The method of claim 10 wherein said underlayer is formed to a thickness less than approximately 50 angstroms.

### Claim 16 (depends on 8)

The method of claim 8 wherein said underlayer is formed by a process comprising:
providing a vacuum deposition chamber that includes a rotatable holder, a sputtering target, a laser for directing a high energy pulsed beam of electromagnetic radiation at said sputtering target, an apparatus for introducing various gases at chosen flow rates and maintaining said gases at desired relative concentrations within said chamber;
mounting said read/write head, said plurality of such heads or said magnetic recording medium on said holder;
directing said electromagnetic radiation at a sputtering target of Si;
injecting O2 gas and N2 gas at selected concentrations, while said electromagnetic radiation impinges on said target, thereby forming an underlayer of SiOxNy on said read/write head or plurality thereof.

### Claim 17 (depends on 16)

The method of claim 16 wherein Ar is used as a carrier gas during the O2 and N2 injection process.

### Claim 18 (depends on 16)

The method of claim 16 wherein x and y are made to vary as said underlayer is being formed.

### Claim 19 (depends on 16)

The method of claim 16 wherein said underlayer is formed to a thickness less than approximately 50 angstroms.

### Claim 20 (depends on 16)

The method of claim 16 wherein said laser is a CO2 laser or an excimer laser.

### Claim 21 (depends on 16)

The method of claim 16 wherein said high energy beam of radiation has an energy fluence between approximately 2 and 5 J/cm2.

### Claim 22 (depends on 8)

The method of claim 8 wherein said underlayer is formed by a process comprising:
providing a vacuum deposition chamber that includes a rotatable holder, a sputtering target, an apparatus for injecting a beam of reactive ions at a chosen energy and directing said ions at said sputtering target, an apparatus for forming a plasma within said chamber said plasma being formed of a mixture of O2 gas and N2 gas at selected concentrations;
mounting said read/write head, a plurality of such heads or a magnetic recording medium on said holder;
directing said reactive ion beam at a sputtering target of Si and forming, thereby, a Si layer on said read/write head, plurality thereof or magnetic recording medium; then
forming, subsequent to the formation of said Si layer, said plasma of O2 gas and N2 gas at selected concentrations, said Si layer being immersed in said plasma for a selected time duration and thereby forming an underlayer of SiOxNy on said read/write head or plurality thereof.

### Claim 23 (depends on 22)

The method of claim 22 wherein Ar is used as a carrier gas during the O2 and N2 plasma formation process.

### Claim 24 (depends on 22)

The method of claim 22 wherein said reactive ion beam is a beam of Ar+ ions formed by sending said beam through a voltage of between approximately 600V to 1200V.

### Claim 25 (depends on 22)

The method of claim 22 wherein said plasma is applied as a sequence comprising an application of an Ar/O2 plasma followed by an application of an Ar/N2 plasma, each application being at a different time duration or as a sequence comprising an application of an Ar/N2 plasma followed by an application of an Ar/O2 plasma, each application being at a different time duration.

### Claim 26 (depends on 22)

The method of claim 22 wherein said plasma is an ion beam plasma, an ECR plasma, an ICP, or a CCP.

### Claim 27 (depends on 8)

The method of claim 8 wherein said underlayer is formed by a process comprising:
providing a vacuum deposition chamber that includes a rotatable holder, a sputtering target, an apparatus for injecting a beam of reactive ions at a chosen energy and directing said ions at said sputtering target, an apparatus for forming a plasma within said chamber said plasma being formed of a mixture of O2 gas and N2 gas at selected concentrations;
mounting said read/write head, said plurality of such heads or said magnetic recording medium on said holder;
directing said reactive ion beam at a sputtering target of Si and forming, thereby, a Si layer on said read/write head or plurality thereof;
forming said plasma of O2 gas and N2 gas, at selected concentrations, said Si layer being immersed in said plasma while said layer is being formed and thereby forming an underlayer of SiOxNy on said read/write head, said plurality thereof or said magnetic recording medium.

### Claim 28 (depends on 27)

The method of claim 27 wherein Ar is used as a carrier gas during the O2 and N2 plasma formation process.

### Claim 29 (depends on 27)

The method of claim 27 wherein said reactive ion beam is a beam of Ar+ ions formed by sending said beam through a voltage of between approximately 600V to 1200V.

### Claim 30 (depends on 27)

The method of claim 27 wherein said plasma is an ion beam plasma, an ECR plasma, an ICP, or a CCP.

### Claim 31 (depends on 8)

The method of claim 8 wherein said underlayer is formed by a process comprising:
providing a vacuum deposition chamber that includes a rotatable holder, a sputtering target, an apparatus for injecting a beam of reactive ions at a chosen energy and directing said ions at said sputtering target, an apparatus for injecting various gases and maintaining an atmosphere of said gases at selected relative concentrations within said chamber;
mounting said read/write head, said plurality of such heads or a magnetic recording medium on said holder;
directing said reactive ion beam at a sputtering target of Si and forming, thereby, a Si layer on said read/write head, said plurality of such heads or said magnetic recording medium; then
forming an atmosphere of O2 gas and N2 gas at selected relative concentrations, using Ar as a carrier gas, whereby said O2 gas oxidizes said Si layer and said N2 gas nitridizes said Si layer, thereby forming an underlayer of SiOxNy on said read/write head, said plurality of such heads or said magnetic recording medium.

### Claim 32 (depends on 31)

The method of claim 31 wherein said reactive ion beam is a beam of Ar+ ions formed by sending said beam through a voltage of between approximately 600V to 1200V.

### Claim 33 (depends on 8)

The method of claim 8 wherein the DLC layer is formed by IBD, PECVD or FCVA.

### Claim 34 (depends on 8)

The method of claim 8 wherein said underlayer is both adhesion enhancing and corrosion resistant.