# US 2008/0187746 A1 · Phosphor in Polycrystalline Ceramic Structure and a Light-Emitting Element Comprising Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0187746 A1
- Document ID: US20080187746A1
- Status: Published application
- Kind: A1
- Application number: 11/908,134
- Filed: 2006-03-10
- Published: 2008-08-07
- Earliest claimed: 2005-03-14
- Assignees: Koninklijke Philips Electronics N.V.
- Inventors: Jan De Graaf; Theo Arnold Kop
- Web page: https://patentgrep.com/patent/US20080187746A1

## CPC

- C04B 35/6455: {Hot isostatic pressing}
- C04B 35/6261: {Milling}
- C04B 35/62625: {Wet mixtures}
- C04B 35/63: using additives specially adapted for forming the products {, e.g.. binder binders}
- C04B 35/632: Organic additives
- C04B 38/0054: {the pores being microsized or nanosized}
- C09K 11/7774: {Aluminates}
- C04B 2111/807: {Luminescent or fluorescent materials}
- C04B 2235/3205: Alkaline earth oxides or oxide forming salts thereof, e.g. beryllium oxide
- C04B 2235/3222: Aluminates other than alumino-silicates, e.g. spinel (MgAl2O4)
- C04B 2235/3224: Rare earth oxide or oxide forming salts thereof, e.g. scandium oxide
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3229: Cerium oxides or oxide-forming salts thereof
- C04B 2235/3286: Gallium oxides, gallates, indium oxides, indates, thallium oxides, thallates or oxide forming salts thereof, e.g. zinc gallate
- C04B 2235/6022: Injection moulding
- C04B 2235/6023: Gel casting
- C04B 2235/6027: Slip casting
- C04B 2235/785: Submicron sized grains, i.e. from 0,1 to 1 micron
- C04B 2235/786: Micrometer sized grains, i.e. from 1 to 100 micron
- C04B 2235/80: Phases present in the sintered or melt-cast ceramic products other than the main phase
- H10H 20/8512: {Wavelength conversion materials}
- Y10T 428/26: Web or sheet containing structurally defined element or component, the element or component having a specified physical dimension
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention relates to a phosphor in a polycrystalline ceramic structure and a light-emitting element provided with the same comprising a Light-Emitting Diode (LED) in which a composite structure of phosphor particles is embedded in a matrix, characterized in that the matrix is a ceramic composite structure comprising a polycrystalline ceramic alumina material, hereafter called luminescent ceramic matrix composite. This luminescent ceramic matrix composite can be made by the steps of converting a powder mixture of ceramic phosphor particles and alumina particles into a slurry, shaping the slurry into a compact, and applying a thermal treatment, optionally in combination with hot isostatic pressing into a polycrystalline phosphor-containing ceramic alumina composite structure. The luminescent ceramic matrix composite further allows a method of tuning the light-diffusing properties by changing at least one of the fractions of phosphor particles and second ceramic particles, the grain size of the particles of the ceramic composite structure, the difference in the refractive index of the particles of the ceramic composite structure, and the porosity in the polycrystalline phosphor-containing ceramic composite structure.

## Claims

### Claim 1

A phosphor in a polycrystalline ceramic structure comprising a phosphor of the doted YAG type, characterized in that the phosphor is embedded in a ceramic matrix comprising non-luminescent polycrystalline alumina, wherein the ceramic matrix comprises 80 to 99.99 vol. % alumina and 0.01 to 20 vol. % phosphor.

### Claim 2 (depends on 1)

The phosphor in the polycrystalline ceramic structure of claim 1, wherein at least 90% of the pores of the ceramic matrix composite have an average pore size of 0 to 300 nm, preferably 0 to 100 nm.

### Claim 3 (depends on 1)

The phosphor in the polycrystalline ceramic structure of claim 1, wherein the phosphor is a doted YAG having the composition (Lu1−x−y−a−bYxGdy)3(Al1−zGaz)5O12:CeaPrb, with 0<x≦1; 0≦y<1; 0≦z≦0.1; 0≦a≦0.2 and 0≦b≦0.1, and a+b>0.

### Claim 4 (depends on 1)

The phosphor in the polycrystalline ceramic structure of claim 1, wherein the ceramic matrix comprises 90 to 99.9 vol. % alumina and 0.1 to 10 vol. % phosphor.

### Claim 5 (depends on 4)

The phosphor in the polycrystalline ceramic structure of claim 4, wherein the matrix comprises 95 to 99 vol. % alumina and 1 to 5 vol. % phosphor.

### Claim 6 (depends on 1)

The phosphor in the polycrystalline ceramic structure of claim 1, wherein the average grain size of the grains comprised in the ceramic matrix is 0.3 to 50 μm.

### Claim 7 (depends on 1)

A light-emitting element comprising a light-emitting diode (LED) and a phosphor of the doped YAG type according to claim 1.

### Claim 8 (depends on 7)

The light-emitting element according to claim 7, wherein the luminescent ceramic matrix composite is applied as a plate on top of or as a shaped cup over the LED and has a thickness between about 50 μm and about 1 mm.

### Claim 9 (depends on 7)

A light-emitting device comprising the element of claim 7.

### Claim 10 (depends on 1)

A method of making the phosphor in a polycrystalline ceramic structure of claim 1, comprising the steps of converting a powder of phosphor and alumina particles into a slurry, shaping the slurry into a polycrystalline phosphor-containing ceramic alumina composite structure, and applying a thermal treatment, optionally in combination with hot isostatic pressing into the ceramic matrix, after which the ceramic matrix is mounted to a LED.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the slurry is shaped into a polycrystalline phosphor-containing ceramic matrix by means of slip casting or injection molding so as to obtain a ceramic light-converting package, a collimating lens or collimating reflector, a coupling-out structure for light, or a heat-dissipating device.

### Claim 12 (depends on 1)

A method of tuning light-diffusing properties of the phosphor in a polycrystalline ceramic structure of claim 1 by changing at least one of:
the fractions of phosphor and alumina in the ceramic matrix;
the average particle size of the particles comprised in the ceramic matrix; and
the porosity of the ceramic matrix.

### Claim 13 (depends on 1)

A method of tuning light-emission properties of the phosphor in a polycrystalline ceramic structure of claim 1 by changing at least one of:
the fractions of the phosphor and the alumina in the ceramic matrix;
the ratio of Ce and/or Pr to YAG in the phosphor; and
the composition of the YAG.

### Claim 14

(canceled)