# US 2008/0187661 A1 · High thermal conductivity metal matrix composites

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0187661 A1
- Document ID: US20080187661A1
- Status: Published application
- Kind: A1
- Application number: 11/868,664
- Filed: 2007-10-08
- Published: 2008-08-07
- Earliest claimed: 2003-10-02
- Assignees: Nano Materials International Corporation
- Inventors: Sion M. Pickard; James C. Withers; Raouf O. Loutfy
- Web page: https://patentgrep.com/patent/US20080187661A1

## CPC

- H10W 40/254: {Diamond}
- C22C 1/1073: {Infiltration or casting under mechanical pressure, e.g. squeeze casting}
- C22C 26/00: Alloys containing diamond {or cubic or wurtzitic boron nitride, fullerenes or carbon nanotubes}
- Y10T 428/12181: Composite powder [e.g., coated, etc.]
- Y10T 428/12903: Cu-base component
- Y10T 428/254: Polymeric or resinous material
- Y10T 428/259: Silicic material
- Y10T 428/30: Self-sustaining carbon mass or layer with impregnant or other layer
- Y10T 428/31678: Of metal
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Discontinuous diamond particulate containing metal matrix composites of high thermal conductivity and methods for producing these composites are provided. The manufacturing method includes producing a thin reaction formed and diffusion bonded functionally graded interactive SiC surface layer on diamond particles. The interactive surface converted SiC coated diamond particles are then disposed into a mold and between the particles and permitted to rapidly solidify under pressure. The surface conversion interactive SiC coating on the diamond particles achieves minimal interface thermal resistance with the metal matrix which translates into good mechanical strength and stiffness of the composites and facilitates near theoretical thermal conductivity levels to be attained in the composite. Secondary working of the diamond metal composite can be performed for producing thin sheet product.

## Claims

### Claim at position 1

1-4. (canceled)

### Claim 5

A method of forming a composite structure comprised essentially of a metal matrix having diamond particles dispersed therein, and wherein said diamond particles are characterized by the presence thereon of a surface layer of SiC chemically bonded thereto, comprising the steps of contacting the surface of said diamond particles with a source of Si under conditions whereby the Si is chemically reacted with C comprising the surface of the diamond particles, thereby forming said surface layer of SiC bonded to said diamond particles, wherein said composite structure is formed by assembling a plurality of said diamond particles in an array, and encapsulating the particles of said array with said metal in a molten state whereby the particles of said array bearing the surface layer of SiC are dispersed in a matrix of said metal when the molten metal hardens upon cooling to the solid state.

### Claim 6

(canceled)

### Claim 7 (depends on 5)

The method of claim 5, wherein the surface layer of SiC is formed on said diamond particles by contacting said diamond particles with the source of Si prior to or subsequent to assembling said particles in said array.

### Claim 8 (depends on 5)

The method of claim 5, wherein the array of diamond particles is encapsulated by the molten metal in the performance of a squeeze casting process to form said composite structure.

### Claim at position 6

9-11. (canceled)

### Claim 12 (depends on 7)

The method of claim 7, wherein the Si that contacts the diamond particles is provided by SiO gas that is introduced into the array of diamond particles.

### Claim 13

(canceled)

### Claim 14 (depends on 7)

The method of claim 7, wherein the Si that contacts the diamond particles includes Si powder.

### Claim 15

(canceled)

### Claim 16 (depends on 7)

The method of claim 7, wherein the Si powder is mixed with phenolic resin.

### Claim at position 12

17-20. (canceled)

### Claim 21

A process to coat diamond powder with a thin SiC surface coating, wherein the diamond particles comprising the diamond powder are contacted by a gaseous Si containing species under conditions causing chemical vapor reaction between the gaseous Si containing species and the solid particles comprising the diamond powder, said SiC coated diamond powder being suitable to be encapsulated in a metal matrix to form a very high thermal conductivity metal matrix composite.

### Claim 22 (depends on 21)

The process described in claim 21, wherein the gaseous species of Si is generated by the reduction of SiO2 to form gaseous SiO.

### Claim 23

A process to coat the particles comprising a diamond powder with a thin, in-situ SiC coating obtained by depositing a Si containing preceramic polymer layer on the diamond particle that can be converted to SiC by heating to a suitably high temperature to initiate the conversion of the diamond surface to SiC, but at a time insufficient to convert the diamond structure to graphite, said SiC coated diamond powder being suitable to form very high thermal conductivity metal matrix composites.

### Claim 24 (depends on 23)

The process described in claim 23, wherein the conversion is carried out at a temperature of at least about 1500 degrees centigrade, preferably at least about 1600 degrees centigrade, more preferably at least about 1800 degrees centigrade.

### Claim at position 17

25-26. (canceled)

### Claim 27 (depends on 23)

The process described in claim 23, wherein the reaction time at maximum temperature is less than about 1 hour, preferably less than about ½ hour, more preferably less than about ⅛ hour, most preferably less than about 1/10 hour.

### Claim at position 19

28-30. (canceled)

### Claim 31

A process to coat the particles comprising a diamond powder with a thin SiC surface conversion coating, wherein the coating is obtained by passing a reactive gaseous mixture over the diamond particles, such that the reactive gas produces a silicon containing species at a temperature that causes reaction between the silicon containing species and the diamond, but at a time and temperature insufficient to convert the diamond structure to graphite, said SiC powder being suitable to form very high thermal conductive matrix composites.

### Claim 32 (depends on 31)

The process described in claim 31, wherein the reaction is carried out at a temperature of at least about 1100 degrees centigrade, preferably at least about 1500 degrees centigrade, more preferably at least about 1800 degrees centigrade.

### Claim at position 22

33-34. (canceled)

### Claim 35 (depends on 31)

The process described in claim 31, wherein the reaction time at maximum temperature is less than about 1 hour, preferably less than about ½ hour, more preferably less than about ⅛ hour, most preferably less than about 1/10 hour.

### Claim at position 24

36-39. (canceled)

### Claim 40

A process to coat the particles compressing a diamond powder with a thin SiC surface coating, wherein a preform of phenolic resin, Si powder, and diamond powder are heated to a temperature sufficient to cause the surface conversion reaction to occur, said SiC coated diamond powder being suitable to form very high thermal conductivity metal matrix composites.

### Claim at position 26

41-45. (canceled)

### Claim 46 (depends on 40)

The process described in claim 40, wherein the temperature to which the preform is heated is at least 1300 degrees centigrade, preferably at least 1400 degrees centigrade, more preferably at least 1500 degrees centigrade, even more preferably at least 1600 degrees centigrade, most preferably at least 1700 degrees centigrade.

### Claim at position 28

47-96. (canceled)

### Claim 97

A process for making a metal matrix composite with very high thermal conductivity, said composite comprising of metal matrix containing a powder formed of diamond particles dispersed therein, comprising the steps of:
(a) providing the respective diamond particles comprising the diamond powder with a thin layer of SiC by contacting the said diamond particles with a gaseous Si containing species while subjecting said particles to heat at a temperature sufficient to cause the Si of the gas to react with the surface carbon of the diamond particles thereby converting the surface layer of the claimed particles to a thin layer of SiC,
(b) placing the SiC layered particles comprising of the diamond powder in the die cavity squeeze casting apparatus
(c) covering the diamond powder with a sheet of alumina ceramic paper,
(d) introducing by pressure squeeze casting a molten metal selected to form the matrix into the die containing the coated diamond powder, under conditions appropriate to pressure infiltrate the diamond powder with the molten metal, and cooling the die.

### Claim 98 (depends on 97)

The process of claim 97, wherein the metal employed for the metal matrix is selected from the group consisting of aluminum, magnesium, copper and alloys of one or more of said metals.

### Claim at position 31

99-100. (canceled)

### Claim 101

A process for making a metal matrix composite with very high thermal conductivity, said composite comprising a metal matrix containing a powder formed of diamond particles dispersed therein, comprising the steps of:
(a) providing the respective particles comprising the selected diamond powder with a thin layer of SiC by preparing a mixture of phenolic resin, Si powder and said diamond powder, pressing said mixture to form a preform, and heating said preform to a temperature sufficient to cause a chemical reaction between the Si powder and the carbon surfaces of the respective diamond particles which results in the formation of a thin SiC surface conversion layer on the respective diamond particles,
(b) placing the SiC layered diamond particles in the die cavity of a squeeze casting
(c) and covering the diamond powder with a sheet of alumina ceramic paper,
(d) introducing molten metal selected to form the matrix into said die cavity under conditions of heat and pressure effective to pressure squeeze cast the molten metal in the die containing the SiC layered diamond powder, therefor pressure infiltrating the diamond powder with the molten metal, and cooling the die.

### Claim 102 (depends on 101)

The process of claim 101, wherein the metal employed for the metal matrix is selected from the group consisting of aluminum, magnesium, copper and an alloy of one or more of said metals.

### Claim at position 34

103-104. (canceled)

### Claim 105

A process for making a metal matrix composite with very high thermal conductivity, said composite comprising a metal matrix containing a powder formed of diamond particles dispersed therein, comprising the steps of:
(a) providing the respective particles comprising the diamond powder with a thin surface layer of SiC by reacting the carbon surfaces of said diamond particles with a gaseous Si containing species at a temperature sufficient to form SiC,
(b) forming a homogeneous mixture of the above SiC layered diamond particles with metal powder selected to form the matrix, and
(c) forming a dense composite by hot pressing the above mixture of SiC surface layered diamond particles and metal powder at a temperature, pressure and cycle time sufficient to fully densify the composite.

### Claim 106

A process for making a metal matrix composite with very high thermal conductivity, said composite comprising a metal matrix containing a powder formed of diamond particles dispersed therein, comprising the steps of:
(a) coating the respective particles comprising the diamond powder with a thin layer of SiC by reacting said diamond particles with a gaseous SiC containing species at a temperature sufficient to form SiC,
(b) forming a homogeneous mixture of the above SiC coated powder with metal powder, and
(c) forming a dense composite by hot isostatic pressing the above mixture of SiC coated diamond powder and metal powder at a temperature, pressure and cycle time sufficient to fully densify the composite.

### Claim at position 37

107-135. (canceled)

### Claim 136

A method of forming a composite structure comprised essentially of a metal matrix having diamond particles dispersed therein, and wherein said diamond particles are characterized by the presence thereon of a surface layer of SiC chemically bonded thereto, comprising the steps of contacting the surface of said diamond particles with a source of SiC under conditions whereby the SiC is deposited on the surface of the diamond particles, causing the deposited SiC to diffuse into the diamond particle on which it is deposited by subjecting to heat at a temperature and for a time adequate to cause such diffusion, thereby forming said surface layer of SiC bonded to said diamond particles, and forming said composite structure by encapsulating a plurity of said particles in array with said metal in a molten state, whereby the particles of said array bearing the surface layer of SiC are dispersed in a matrix of said metal when the molten metal hardens upon cooling to the solid state.

### Claim 137 (depends on 136)

The method of claim 136 wherein the source of SiC is a SiC organometallic gas, preferably a gas selected from the group consisting of methyltrichloro silane, dimethyldichlorosilane and triethylsilane.

### Claim 138

(canceled)

### Claim 139 (depends on 136)

The method of claim 136, wherein the array of diamond particles are enclosed in a non oxidizing atmosphere prior to being contacted by the SiC organometallic gas and whereas the diamond particles are heated to about 1600 degrees centigrade for about one (1) hour to cause the SiC to diffuse.