# US 2008/0187456 A1 · Extruded material of a free-cutting aluminum alloy excellent in embrittlement resistance at a high temperature

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0187456 A1
- Document ID: US20080187456A1
- Status: Published application
- Kind: A1
- Application number: 12/059,904
- Filed: 2008-03-31
- Published: 2008-08-07
- Earliest claimed: 2005-09-30
- Assignees: Furukawa-Sky Aluminum Corp.
- Inventors: Kensuke Mori; Kazuo TAGUCHI
- Web page: https://patentgrep.com/patent/US20080187456A1

## CPC

- C22C 21/12: with copper as the next major constituent
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

An extruded material of a free-cutting aluminum alloy excellent in embrittlement resistance at a high temperature, containing from 3 to 6% by mass of Cu and from 0.9 to 3% by mass of Bi with the balance being Aluminum and inevitable impurities, wherein a temperature for reducing the Charpy impact test value to half of the value at room temperature is 180° C. or more.

## Claims

### Claim 1

An extruded material of a free-cutting aluminum alloy excellent in embrittlement resistance at a high temperature, comprising from 3 to 6% by mass of Cu and from 0.9 to 3% by mass of Bi with the balance being Aluminum and inevitable impurities, wherein a temperature for reducing the Charpy impact test value to half of the value at room temperature is 180° C. or more.

### Claim 2

The extruded material of a free-cutting aluminum alloy excellent in embrittlement resistance at a high temperature, further comprising one or two kinds of elements selected from Si in a proportion from 0.1 to 1.5% by mass and Fe in a proportion from 0.1 to 2.0% by mass.