# US 2008/0187454 A1 · Heat-resistant magnesium alloy for casting heat-resistant magnesium alloy cast product, and process for producing heat-resistant magnesium alloy cast product

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0187454 A1
- Document ID: US20080187454A1
- Status: Published application
- Kind: A1
- Application number: 11/975,381
- Filed: 2007-10-18
- Published: 2008-08-07
- Earliest claimed: 2003-01-31
- Assignees: Kabushiki Kaisha Toyota Jidoshokki
- Inventors: Motoharu Tanizawa; Kyoichi Kinoshita; Eiji Kishi; Katsufumi Tanaka; Yuki Okamoto; Takayuki Kato
- Web page: https://patentgrep.com/patent/US20080187454A1

## CPC

- C22C 23/00: Alloys based on magnesium
- C22C 23/02: with aluminium as the next major constituent
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A heat-resistant magnesium alloy is for casting, and includes Ca in an amount of from 1 to 15% by mass, Al in a summed amount of from 4 to 25% by mass with the amount of Ca, and the balance being Mg and inevitable impurities when the entirety is taken as 100% by mass. The heat-resistant magnesium alloy is not only inexpensive, but also effects an advantage that cracks are inhibited from occurring when being cast. For example, a process for producing heat-resistant magnesium alloy cast product includes the step of pressure pouring an alloy molten metal, which has a target composition around Mg-3% Ca-3% Al-from 0.2 to 0.3% Mn, into a cavity of metallic die, which is preheated to a die temperature of from 130 to 140° C. in advance. The process makes it possible to produce die-cast products, which are free from cast cracks.

## Claims

### Claim 1

A heat-resistant magnesium alloy for casting, the magnesium alloy being good in terms of the castability and heat resistance, and comprising:
calcium (Ca) in an amount of from 1 to 15% by mass;
aluminum (Al) in a summed amount of from 4 to 25% by mass with the amount of Ca; and
the balance being magnesium (Mg) and inevitable impurities when the entirety is taken as 100% by mass (hereinafter simply referred to as “%”).

### Claim 2 (depends on 1)

The heat-resistant magnesium alloy set forth in claim 1, further comprising manganese (Mn) in an amount of from 0.1 to 1%.

### Claim 3 (depends on 1)

The heat-resistant magnesium alloy set forth in claim 1, wherein a mass ratio of the Ca amount with respect to the Al amount, Ca/Al by mass, is 1 or more.

### Claim 4 (depends on 1)

The heat-resistant magnesium alloy set forth in claim 1, wherein a solidification temperature width, a temperature difference between a liquidus temperature at which a molten metal starts solidifying and a solidus temperature at which the molten metal completes solidifying, is 110° C. or less.

### Claim 5 (depends on 1)

The heat-resistant magnesium alloy set forth in claim 1 being free from a rare-earth element.

### Claim 6 (depends on 1)

A heat-resistant magnesium alloy cast product being good in terms of the heat resistance, and produced by a process comprising the steps of:
pouring a molten alloy into a mold, the molten alloy comprising the heat-resistance aluminum alloy set forth in claim 1; and
solidifying the molten alloy by cooling it after the pouring step.

### Claim 7 (depends on 6)

The heat-resistant magnesium alloy cast product set forth in claim 6 being free from a rare-earth element.

### Claim 8 (depends on 6)

The heat-resistant magnesium cast product set forth in claim 6 whose average crystalline grain diameter indexing the structural roughness is 18 μm or less.

### Claim 9

A process for producing heat-resistant magnesium alloy cast product, the process comprising the steps of: preparing an alloy molten metal including calcium (Ca), aluminum (Al), manganese (Mn) and magnesium (Mg); pouring the alloy molten metal into a preheated casting die; and solidifying the alloy molten metal undergone the pouring step by cooling;
the casting die comprises a metallic die with a cavity provided therein;
the pouring step comprises a step of pressure pouring the alloy molten metal into the cavity of the metallic die, which is preheated to a die temperature of from 130 to 140° C.; and thereby
a heat-resistant magnesium alloy cast product is obtainable, the heat-resistant magnesium alloy cast product comprising: from 2.5 to 3.5%-by-mass Ca; from 2.5 to 3.5%-by-mass Al; from 0.1 to 0.5%-by-mass Mn; and the balance being Mg as well as inevitable impurities and/or trace-amount reforming elements being effective for improving characteristics; when the entirety is taken as 100% by mass (hereinafter simply referred to as “%”).

### Claim 10 (depends on 9)

The process set forth in claim 9, wherein a temperature of the alloy molten metal prior to the pouring step falls in a range of from 620 to 640° C.

### Claim 11

A process for producing heat-resistant magnesium alloy cast product, the process comprising the steps of: preparing an alloy molten metal including Ca, Al, Mn and Mg; pouring the alloy molten metal into a preheated casting die; and solidifying the alloy molten metal undergone the pouring step by cooling;
the casting die comprises a metallic die with a cavity provided therein;
the pouring step comprises a step of gravity pouring the alloy molten metal into the cavity of the metallic die, which is preheated to a die temperature of from 30 to 450° C.; and thereby
a heat-resistant magnesium alloy cast product is obtainable, the heat-resistant magnesium alloy cast product comprising: from 2.5 to 3.5% Ca; from 2.5 to 3.5% Al; from 0.1 to 0.5% Mn; and the balance being Mg as well as inevitable impurities and/or trace-amount reforming elements being effective for improving characteristics; when the entirety is taken as 100%.

### Claim 12 (depends on 11)

The process set forth in claim 11, wherein a temperature of the alloy molten metal prior to the pouring step falls in a range of from 630 to 750° C.

### Claim 13

A process for producing heat-resistant magnesium alloy cast product, the comprising the steps of: preparing an alloy molten metal including Ca, Al, Mn and Mg; pouring the alloy molten metal into a preheated casting die; and solidifying the alloy molten metal undergone the pouring step by cooling;
the casting die comprises a sand die with a cavity provided therein;
the pouring step comprises a step of gravity pouring the alloy molten metal into the cavity of the sand die, which is preheated to a die temperature of from 30 to 350° C.; and thereby
a heat-resistant magnesium alloy cast product is obtainable, the heat-resistant magnesium alloy cast product comprising: from 2.5 to 3.5% Ca; from 2.5 to 3.5% Al; from 0.1 to 0.5% Mn; and the balance being Mg as well as inevitable impurities and/or trace-amount reforming elements being effective for improving characteristics; when the entirety is taken as 100%.

### Claim 14 (depends on 13)

The process set forth in claim 13, wherein a temperature of the alloy molten metal prior to the pouring step falls in a range of from 630 to 750° C.