# US 2008/0186356 A1 · Nozzle plate, method of manufacturing nozzle plate, and image forming apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0186356 A1
- Document ID: US20080186356A1
- Status: Published application
- Kind: A1
- Application number: 12/023,984
- Filed: 2008-01-31
- Published: 2008-08-07
- Earliest claimed: 2007-02-02
- Assignees: FUJIFILM Corporation
- Inventors: Shuji Takahashi
- Web page: https://patentgrep.com/patent/US20080186356A1

## CPC

- B41J 2/1433: {Structure of nozzle plates}
- B41J 2/1606: {Coating the nozzle area or the ink chamber}
- B41J 2/162: {Manufacturing of the nozzle plates}
- B41J 2/1628: {dry etching}
- B41J 2/1629: {wet etching}
- B41J 2/1642: {thin film formation by CVD [chemical vapor deposition]}
- B41J 2/1645: {thin film formation by spincoating}
- B41J: TYPEWRITERS; SELECTIVE PRINTING MECHANISMS, i.e. MECHANISMS PRINTING OTHERWISE THAN FROM A FORME; CORRECTION OF TYPOGRAPHICAL ERRORS

## Abstract

The nozzle plate has a nozzle hole formed therethrough, the nozzle hole being defined in the nozzle plate with an inner surface including a first liquid-philic portion, a liquid-phobic portion and a second liquid-philic portion that are arranged in this order from a side near the nozzle mouth, the first and second liquid-philic portions having liquid-philicity, the liquid-phobic portion having liquid-phoblicity.

## Claims

### Claim 1

A nozzle plate having a nozzle hole formed through the nozzle plate, the nozzle hole having a nozzle mouth from which a liquid is ejected, the nozzle hole being defined in the nozzle plate with an inner surface including a first liquid-philic portion, a liquid-phobic portion and a second liquid-philic portion that are arranged in this order from a side near the nozzle mouth, the first and second liquid-philic portions having liquid-philicity, the liquid-phobic portion having liquid-phobicity.

### Claim 2 (depends on 1)

The nozzle plate as defined in claim 1, wherein:
the nozzle plate is constituted of an SOI substrate including a supporting layer, an active layer, and an oxide film layer interposed between the supporting layer and the active layer;
a portion of the inner surface defining the nozzle hole corresponding to the active layer serves as the first liquid-philic portion;
a portion of the inner surface defining the nozzle hole corresponding to the oxide film layer is covered with a liquid-phobic member that serves as the liquid-phobic portion;
a portion of the inner surface defining the nozzle hole corresponding to the supporting layer serves as the second liquid-philic portion; and
a surface energy Es1 of the first liquid-philic portion, a surface energy Eh of the liquid-phobic portion and a surface energy Es2 of the second liquid-philic portion have a relationship of Es2≧Es1>Eh.

### Claim 3 (depends on 1)

The nozzle plate as defined in claim 1, wherein a liquid-phobic film is formed on a surface of the nozzle plate on which the nozzle mouth opens, the liquid-phobic film having liquid-phobicity.

### Claim 4 (depends on 3)

The nozzle plate as defined in claim 3, wherein a surface energy Es1 of the first liquid-philic portion, a surface energy Eh of the liquid-phobic portion, a surface energy Es2 of the second liquid-philic portion and a surface energy Eo of the liquid-phobic film on the ejection surface have a relationship of Es2≧Es1>Eh≧Eo.

### Claim 5 (depends on 1)

The nozzle plate as defined in claim 1, wherein:
the inner surface defining the nozzle hole includes a plurality of the liquid-phobic portions; and
one of the liquid-phobic portions which is nearest to the nozzle mouth has a surface energy lower than any other of the liquid-phobic portions.

### Claim 6 (depends on 1)

An image forming apparatus comprising the nozzle plate as defined in claim 1.

### Claim 7

A method of manufacturing a nozzle plate through which a nozzle hole is formed, the method comprising the steps of:
forming the nozzle hole through an SOI substrate including a supporting layer, an active layer and an oxide film layer interposed between the supporting layer and the active layer, the nozzle hole having a nozzle mouth from which a liquid is ejected, the nozzle mouth opening on a surface on the active layer of the SOI substrate;
then forming a liquid-phobic film on at least an inner surface defining the nozzle hole in the SOI substrate, the liquid-phobic film having liquid-phobicity; and
then removing the liquid-phobic film other than a portion of the liquid-phobic film covering a portion of the inner surface defining the nozzle hole corresponding to the oxide film layer.

### Claim 8 (depends on 7)

The method as defined in claim 7, wherein, in the step of removing the liquid-phobic film, the SOI substrate is subjected to a removing liquid so that the liquid-phobic film other than the portion of the liquid-phobic film on the portion of the inner surface defining the nozzle hole corresponding to the oxide film layer is removed.

### Claim 9

A method of manufacturing a nozzle plate through which a nozzle hole is formed, the method comprising the steps of:
forming a first opening in an SOI substrate that includes a first active layer, a second active layer, a supporting layer, a first oxide film layer interposed between the first active layer and the second active layer, a second oxide film layer interposed between the second active layer and the supporting layer, by etching the first active layer, the first oxide film layer and the second active layer;
forming a first liquid-phobic film on at least an inner surface defining the first opening in the SOI substrate;
forming a second opening in the SOI substrate by etching the supporting layer and the second oxide film layer, the second opening connecting to the first opening to form the nozzle hole;
forming a second liquid-phobic film on at least an inner surface defining the second opening in the SOI substrate;
removing the first liquid-phobic film other than a portion of the first liquid-phobic film covering a portion of the inner surface defining the first opening corresponding to the first oxide film layer; and
removing the second liquid-phobic film other than a portion of the second liquid-phobic film covering a portion of the inner surface defining the second opening corresponding to the second oxide film layer,
wherein the first and second liquid-phobic films have liquid-phobicity, and the first liquid-phobic film has a surface energy lower than the second liquid-phobic film.