# US 2008/0185951 A1 · Highly emissive cavity for discharge lamp and method and material relating thereto

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0185951 A1
- Document ID: US20080185951A1
- Status: Published application
- Kind: A1
- Application number: 11/702,919
- Filed: 2007-02-06
- Published: 2008-08-07
- Earliest claimed: 2007-02-06
- Assignees: General Electric Company
- Inventors: Deeder Aurongzeb
- Web page: https://patentgrep.com/patent/US20080185951A1

## CPC

- H01J 61/0732: {characterised by the construction of the electrode}
- H01J 9/042: {Manufacture, activation of the emissive part}
- H01J 61/526: {heating or cooling of electrodes}
- H01K 1/14: characterised by the shape
- H01K 3/02: Manufacture of incandescent bodies
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H01K: ELECTRIC INCANDESCENT LAMPS (details, apparatus or processes for manufacture applicable to both discharge devices and incandescent lamps H01J; light sources using a combination of incandescent and other types of light generation H01J61/96, H05B35/00)

## Abstract

The invention relates to an electrode having a nano-hollow array on the surface thereof, the nano-hollow array comprising a plurality of nano-pores or nano-balls, each pore having a diameter of less than 500 nm, formed by a process comprising depositing a uniform metal film on the electrode structure surface at a rate of 2 Å per second or less, annealing the metal film under rapid anneal conditions at a temperature within about 100 degrees of the melting point of the metal film and without subjecting the metal film to a temperature ramp-up to create metal droplets, and anodizing and over-anodizing the metal droplets in the presence of an anodization agent for the metal at from 20 to 200 volts at 0.1 to 2 amps to create nano-pores in the metal droplets or nano-balls to, creating increased surface area and increased electric field around the electrode which enhances speed of fill gas ionization.

## Claims

### Claim 1

An electrode having a nano-hollow array on the surface thereof, the nano-hollow array comprising a plurality of nano-pores, each pore having a diameter of from 10 nm to 500 nm and having side walls that are rough in nature, and formed from a metal film deposited on the electrode surface.

### Claim 2 (depends on 1)

The electrode of claim 1 wherein the metal film comprises a metal or an alloy of a metal having a low melting point below about 700° C.

### Claim 3 (depends on 1)

The electrode of claim 1 wherein the metal film has a thickness of from about 2 nm to about 50 nm prior to formation of the nano-hollow array.

### Claim 4 (depends on 1)

The electrode of claim 1 wherein the nano-hollow array does not cover more than about 10% of the electrode surface.

### Claim 5 (depends on 1)

The electrode of claim 1 wherein the nano-hollow array is formed by subjecting a low melting point metal film deposited on the electrode surface to rapid annealing, anodizing, and over-anodizing.

### Claim 6

A process for creating a nano-hollow array on an electrode structure comprising:
depositing a uniform metal film on the electrode structure surface at a rate of 2 Å per second or less;
annealing the metal film under rapid anneal conditions at a temperature within about 300 degrees of the melting point of the metal film, and without subjecting the metal film to a temperature ramp-up, to create metal droplets;
anodizing the metal droplets in the presence of an anodization agent for the metal at from 20 to 200 volts at 0.1 to 2 amps to create pores in the metal droplets having pore diameters of from about 10 nm to about 500 nm; and
over-anodizing the metal droplets to extend the pores into the electrode structure.

### Claim 7 (depends on 6)

The process of claim 6 wherein the over-anodizing step is replaced by exposing the anodized droplets to an electrolyte to extend the pores into the electrode structure.

### Claim 8 (depends on 6)

The process of claim 6 wherein the over-anodizing step is accomplished using the same or another suitable anodizing agent for the metal droplets.

### Claim 9 (depends on 6)

The process of claim 6 wherein the nano-hollow array covers about 10% of the electrode structure surface.

### Claim 10 (depends on 6)

The process of claim 6 wherein the electrode structure bears a tube or a coil, and the metal film is deposited on the tube or the coil.

### Claim 11 (depends on 10)

The process of claim 10 wherein the metal film comprises at least one of osmium, molybdenum, rhenium and hafnium, has a thickness of from about 3 to about 7 nm, and is annealed at a temperature in excess of half of the melting point of the metal film to create metal nano-balls having diameters less than about 500 nm.

### Claim 12 (depends on 11)

The process of claim 11 including the further step of over-coating the metal nano-balls with a high-temperature metal oxide, carbide or nitride to increase stability.

### Claim 13 (depends on 6)

The process of claim 6 wherein the over-anodizing step is replaced by exposing the anodized droplets to a plasma etching process to extend the pores into the electrode structure.

### Claim 14

A process for decreasing the operating temperature of an electrode in a high intensity lamp by increasing electrode surface area, the process comprising creating a nano-hollow array on the surface of the electrode by first depositing a low melting point metal film on at least a portion of the surface of the electrode, then subjecting the metal film to rapid anneal processing followed by anodizing to generate metal droplets from the metal film, the droplets having pore structures with rough side walls, and further processing the anodized surface to extend the pore structures into the electrode.

### Claim 15 (depends on 14)

The process of claim 14 wherein the electrode bears a coil, and the nano-hollow array is generated on the coil surface.

### Claim 16 (depends on 15)

The process of claim 15 wherein the droplets are replaced by metal nano-balls.

### Claim 17 (depends on 14)

The process of claim 14 wherein the electrode bears a coil and the nano-hollow array is generated on the electrode surface and on the coil surface.

### Claim 18 (depends on 14)

The process of claim 14 wherein the anodizing is conducted in the presence of an anodizing agent for the metal film at from 20 to 200 volts at 0.1 to 2 amps to create pores having pore diameters of from about 10 nm to about 500 nm.

### Claim 19 (depends on 14)

The process of claim 14 wherein the pore structures are extended into the electrode by a process selected from over-anodizing the anodized surface, exposing the anodized surface to an electrolyte, and plasma etching.