# US 2008/0185747 A1 · Injection mold and partial compression molding method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0185747 A1
- Document ID: US20080185747A1
- Status: Published application
- Kind: A1
- Application number: 12/022,387
- Filed: 2008-01-30
- Published: 2008-08-07
- Earliest claimed: 2007-02-05
- Assignees: Canon Kabushiki Kaisha
- Inventors: Teruaki Uezaki; Takashi Arai; Yoshihiro Iitsuka
- Web page: https://patentgrep.com/patent/US20080185747A1

## CPC

- B29C 45/0025: {Preventing defects on the moulded article, e.g. weld lines, shrinkage marks (preventing defects on the preformed parts or layers B29C45/14836)}
- B29C 45/561: {Injection-compression moulding}
- B29C 45/572: {using movable mould wall or runner parts}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

In an injection mold, a compression pin is placed at a cavity surface by the pressing force of a biasing member, and is moved rearward by the pressure of filled resin so as to form a compression boss. After the completion of filling, the compression boss is compressed by the compression pin.

## Claims

### Claim 1

An injection mold comprising:
a stationary mold section;
a movable mold section that forms a cavity between the movable mold section and the stationary mold section;
a compression pin extending through the movable mold section and having a front end face that forms a part of a cavity surface;
a biasing member provided in the compression pin so that the front end face of the compression pin is caused to retreat from the cavity by the pressure of resin; and
a driving unit configured to advance the retreating front end face of the compression pin toward the cavity.

### Claim 2 (depends on 1)

The injection mold according to claim 1, further comprising:
an ejector pin and an ejector plate configured to push out an article molded in the cavity.

### Claim 3 (depends on 2)

The injection mold according to claim 2, wherein the compression pin has a flange portion, and the flange portion is movably stored in a large-diameter opening provided in the ejector plate.

### Claim 4 (depends on 3)

The injection mold according to claim 3, wherein the front end face of the compression pin is pushed toward the cavity by biasing the flange portion by the biasing member.

### Claim 5 (depends on 1)

The injection mold according to claim 1, wherein the biasing member includes a spring or an elastic member.

### Claim 6

A partial compression molding method comprising the steps of:
forming a surface of a cavity by a stationary mold section, a movable mold section, and a front end face of a compression pin;
filling the cavity with molten resin;
forming a compression boss by causing the front end face of the compression pin to retreat from the cavity surface by the pressure of the filled resin; and
moving the resin in the compression boss into the cavity by advancing the compression pin toward the cavity after filling of the resin is completed.