# US 2008/0185612 A1 · Semiconductor device and manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0185612 A1
- Document ID: US20080185612A1
- Status: Published application
- Kind: A1
- Application number: 12/026,917
- Filed: 2008-02-06
- Published: 2008-08-07
- Earliest claimed: 2007-02-07
- Assignees: Fujitsu Limited
- Inventors: Masahiro FUKUDA; Yosuke SHIMAMUNE
- Web page: https://patentgrep.com/patent/US20080185612A1

## CPC

- H10D 84/017: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/021: {Forming source or drain recesses by etching e.g. recessing by etching and then refilling}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3208: {Silicon carbide}
- H10P 14/3211: {Silicon, silicon germanium or germanium}
- H10P 14/3248: {consisting of two layers}
- H10P 14/3408: {Silicon carbide}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3441: {Conductivity type}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- Y10S 438/933: Germanium or silicon or Ge-Si on III-V
- Y10S 438/938: Lattice strain control or utilization
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A semiconductor device has a Si substrate, a gate insulating film over the Si substrate, a gate electrode over the gate insulating film, a source region and a drain region in the Si substrate, wherein each of the source region and the drain region includes a first Si layer including Ge, an interlayer over the first Si layer, and a second Si layer including Ge over the interlayer, wherein the interlayer is composed of Si or Si including Ge, and a Ge concentration of the interlayer is less than a Ge concentration of the first Si layer and a Ge concentration of the second Si layer.

## Claims

### Claim 1

A semiconductor device comprising:
a Si substrate;
a gate insulating film over the Si substrate;
a gate electrode over the gate insulating film;
a source region and a drain region in the Si substrate;
wherein each of the source region and the drain region includes a first Si layer including Ge, an interlayer over the first Si layer, and a second Si layer including Ge over the interlayer, wherein the interlayer is composed of Si or Si including Ge, and a Ge concentration of the interlayer is less than a Ge concentration of the first Si layer and a Ge concentration of the second Si layer.

### Claim 2 (depends on 1)

The semiconductor device according to claim 1, wherein the first Si layer is lattice matching to the Si substrate, the interlayer is lattice matching to the first Si layer, the second Si layer is lattice matching to the interlayer.

### Claim 3 (depends on 1)

The semiconductor device according to claim 1 further comprising a recess in the Si substrate, wherein the first Si layer, the interlayer, and the second Si layer are formed in the recess.

### Claim 4 (depends on 1)

The semiconductor device according to claim 1, wherein the Ge concentration of the first Si layer and the Ge concentration of the second Si layer is in the range from 20% to 40% in atomic %.

### Claim 5 (depends on 1)

The semiconductor device according to claim 1, wherein each of the source region and the drain region includes B as p-type impurity, and a concentration of B is in the range from 1×1019 cm−3 to 1×1021 cm−3.

### Claim 6

A semiconductor device comprising:
a Si substrate;
a gate insulating film over the Si substrate;
a gate electrode over the gate insulating film;
a source region and a drain region in the Si substrate;
wherein the each of the source region and the drain region includes a first Si layer including C over the Si substrate, an interlayer over the first Si layer, and a second Si layer including C over the interlayer, wherein the interlayer is composed of Si or Si including C, and a C concentration of the interlayer is less than a C concentration of the first Si layer and a C concentration of the second Si layer.

### Claim 7 (depends on 6)

The semiconductor device according to claim 6, wherein the first Si layer is lattice matching to the Si substrate, the interlayer is lattice matching to the first Si layer, the second Si layer is lattice matching to the interlayer.

### Claim 8 (depends on 6)

The semiconductor device according to claim 6, an interface between the first Si layer and the Si substrate is lower than the surface of the Si substrate.

### Claim 9 (depends on 6)

The semiconductor device according to claim 6, wherein the C concentration of the first Si layer and the C concentration of the second Si layer is in the range from 1% to 2% in atomic %.

### Claim 10 (depends on 6)

The semiconductor device according to claim 6, wherein each the source and the drain region includes P or As as n-type impurity, and the concentration of P or As is in the range from 1×1019 cm−3 to 1×1021 cm−3.

### Claim 11

A method of manufacturing a semiconductor device comprising:
forming a gate insulating film and a gate electrode over a Si substrate;
forming a recess in the Si substrate at both sides of the gate electrode;
forming a first Si layer including Ge in the recess;
forming an interlayer over the first Si layer;
forming a second Si layer including Ge over the interlayer;
wherein the interlayer is composed of Si or Si including Ge, and a Ge concentration of the interlayer is less than a Ge concentration of the first Si layer and a Ge concentration of the second Si layer.

### Claim 12 (depends on 11)

The method of manufacturing the semiconductor device according to claim 11, wherein the first Si layer is formed by epitaxial growth, the interlayer is formed by epitaxial growth, and the second Si layer is formed by epitaxial growth.

### Claim 13 (depends on 11)

The method of manufacturing the semiconductor device according to claim 11, wherein a thickness of each of the first Si layer, and the second Si layer is equal to or less than a critical film thickness.

### Claim 14 (depends on 11)

The method of manufacturing the semiconductor device according to claim 11, wherein the Ge concentration of the first Si layer and the Ge concentration of the second Si layer is in a range from 20% to 40% in atomic %.

### Claim 15 (depends on 11)

The method of manufacturing the semiconductor device according to claim 11, wherein each of the source and the drain region includes B as p-type impurity, and the concentration of B is in the range from 1×1019 cm−3 to 1×1021 cm−3.

### Claim 16

A method of manufacturing a semiconductor device comprising:
forming a gate insulating film and a gate electrode over a Si substrate;
forming a recess in the Si substrate at both sides of the gate electrode;
forming a first Si layer including C in the recess;
forming a interlayer over the first Si layer;
forming a second Si layer including C over the interlayer;
wherein the interlayer is composed of Si or Si including C, and a C concentration of the interlayer is less than a C concentration of the first Si layer and a C concentration of the second Si layer.

### Claim 17 (depends on 16)

The method of manufacturing the semiconductor device according to claim 16, wherein the first Si layer is formed by epitaxial growth, the interlayer is formed by epitaxial growth, and the second Si layer is formed by epitaxial growth.

### Claim 18 (depends on 16)

The method of manufacturing the semiconductor device according to claim 16, wherein the thickness of each of the first Si layer, and the second Si layer is equal to or less than a critical film thickness.

### Claim 19 (depends on 16)

The method of manufacturing the semiconductor device according to claim 16, wherein the C concentration of the first Si layer and the C concentration of the second Si layer is in the range from 1% to 2% in atomic %.

### Claim 20 (depends on 16)

The method of manufacturing the semiconductor device according to claim 16, wherein each of the source and the drain region includes P or As as n-type impurity, and the concentration of P or As is in the range from 1×1019 cm−3 to 1×1021 cm−3.