# US 2008/0185118 A1 · Reduced friction molds for injection molded solder processing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0185118 A1
- Document ID: US20080185118A1
- Status: Published application
- Kind: A1
- Application number: 11/670,080
- Filed: 2007-02-01
- Published: 2008-08-07
- Earliest claimed: 2007-02-01
- Assignees: International Business Machines Corporation
- Inventors: Mark D. Schultz
- Web page: https://patentgrep.com/patent/US20080185118A1

## CPC

- H05K 3/3465: Application of solder
- H05K 2203/0113: Female die used for patterning or transferring, e.g. temporary substrate having recessed pattern
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

A process of reducing friction, which is encountered in molds utilized in injection molded, solder processing, and wherein glass mold plates have mold pits etched therein. The mold pates are subjected to a heat treatment so as to smooth or round-off sharp edges along the periphery of the mold pits.

## Claims

### Claim 1

A method of modifying mold plates having mold pits etched in the upper surfaces of said mold plates, said mold plates being utilized in implementing injection molded solder processing, said method comprising:
smoothing the peripheral edges of each of said mold pits from an initially sharp condition into a rounded-off or smoothly radiused configuration.

### Claim 2 (depends on 1)

A method as claimed in claim 1, wherein said mold plates are subjected in at least the upper surface regions thereof to a heat treatment so as to cause the initially sharp peripheral edge of each of said mold pits to deform into said rounded-off or smoothly radiused configuration extending into said upper surfaces of the mold plates.

### Claim 3 (depends on 2)

A method as claimed in claim 2, wherein said heat treatment of said mold plates is implemented throughout the thickness of each of said mold plates.

### Claim 4 (depends on 1)

A method as claimed in claim 1, wherein said mold plates are constituted of a glass material, and said heat treatment comprises heating said glass material mold plates to a temperature which is closely below the softening temperature of said glass material.

### Claim 5 (depends on 4)

A method as claimed in claim 4, wherein said glass material mold plates are heated to a temperature at approximately 60° C. below the softening temperature of said glass material.

### Claim 6 (depends on 4)

A method as claimed in claim 4, wherein said heat treatment comprises heating said glass material mold plates to a temperature of about 760° C.

### Claim 7 (depends on 4)

A method as claimed in claim 4, wherein said heat treatment of the glass material is maintained over at least one temperature cycle for a predetermined period of time.

### Claim 8 (depends on 6)

A method as claimed in claim 6, wherein said predetermined period of time of said at least one temperature cycle for said heat treatment is for a duration of about 10 minutes.

### Claim 9 (depends on 4)

A method as claimed in claim 4, wherein said mold pit edges are deformed from the initial sharp edge into the rounded-off edge configuration by said glass material being softened during the heat treatment.

### Claim 10 (depends on 4)

A method as claimed in claim 4, wherein said mold plates have backside surfaces thereof supported on a substrate having a planar surface in contact therewith during at least the heat treatment of said glass material mold plates.

### Claim 11 (depends on 10)

A method as claimed in claim 10, wherein said substrate is constituted of quartz.

### Claim 12 (depends on 10)

A method as claimed in claim 10, wherein said substrate is constituted of graphite plate.

### Claim 13 (depends on 10)

A method as claimed in claim 10, wherein the surface area of said substrate and the backside surface of said mold plates have a coating layer of a material interposed so as to inhibit sticking between said mold plates and said substrate.

### Claim 14 (depends on 13)

A method as claimed in claim 13, wherein said coating layer is selected from the group of materials consisting of graphite, refectory powders or kiln wash.

### Claim 15 (depends on 13)

A method as claimed in claim 13, wherein said coating layer is permanently applied to the lower surface of said mold plates.

### Claim 16 (depends on 13)

A method as claimed in claim 13, wherein said coating layer comprises a sacrificial layer of material which is temporarily applied to the surface of said substrate for the duration of the heat treatment of the mold plates.

### Claim 17

A mold plate having mold pits etched in an upper surface thereof, wherein said molt plate is utilized in injection molded processing, wherein said mold plate is subjected in at least the upper surface regions thereof to a heat treatment so as to cause an initially sharp peripheral edge of each of said mold pits to deform into a rounded-off or smoothly radiused configuration extending into said upper surface of the mold plate.

### Claim 18 (depends on 17)

A mold plate as claimed in claim 17, wherein said heat treatment of said mold plate is implemented throughout the thickness of said mold plate.

### Claim 19 (depends on 17)

A mold plate as claimed in claim 17, wherein said mold plate is constituted of a glass material, and said heat treatment comprises heating said glass material mold plate to a temperature which is closely below the softening temperature of said glass material.

### Claim 20 (depends on 19)

A mold plate as claimed in claim 19, wherein said glass material mold plate is heated to a temperature at approximately 60° C. below the softening temperature of said glass material.

### Claim 21 (depends on 19)

A mold plate as claimed in claim 19, wherein said heat treatment comprises heating said glass material mold plate to a temperature of about 760° C.

### Claim 22 (depends on 19)

A mold plate as claimed in claim 19, wherein said heat treatment of the glass material is maintained over at least one temperature cycle for a predetermined period of time.

### Claim 23 (depends on 22)

A mold plate as claimed in claim 22, wherein said predetermined period of time for the at least one temperature cycle of said heat treatment is for a duration of about 10 minutes.

### Claim 24 (depends on 19)

A mold plate as claimed in claim 19, wherein said mold pit edges are deformed from the initial sharp edge into the rounded-off edge configuration by said glass material being softened during the heat treatment.

### Claim 25 (depends on 19)

A mold plate as claimed in claim 19, wherein said mold plate has the backside surface thereof supported on a substrate having a planar surface in contact therewith during at least the heat treatment of said glass material mold plate.

### Claim 26 (depends on 24)

A mold plate as claimed in claim 24, wherein said substrate is constituted of quartz.

### Claim 27 (depends on 25)

A mold plate as claimed in claim 25, wherein said substrate is constituted of graphite.

### Claim 28 (depends on 25)

A mold plate as claimed in claim 25, wherein the surface area of said substrate and the backside surface of said mold plate have a coating layer of a material interposed so as to inhibit sticking between said mold plate and said substrate.

### Claim 29 (depends on 28)

A mold plate as claimed in claim 28, wherein said coating layer is selected from the group of materials consisting of graphite and refectory powder or wash.

### Claim 30 (depends on 28)

A mold plate as claimed in claim 28, wherein said coating layer is permanently applied to the backside surface of said mold plate.

### Claim 31 (depends on 28)

A mold plate as claimed in claim 28, wherein said coating layer comprises a sacrficial layer of material which is temporarily applied to the surface of said substrate for the duration of the heat treatment of the mold plate.