# US 2008/0185079 A1 · Lubricant for elevated temperature forming

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0185079 A1
- Document ID: US20080185079A1
- Status: Published application
- Kind: A1
- Application number: 11/671,495
- Filed: 2007-02-06
- Published: 2008-08-07
- Earliest claimed: 2007-02-06
- Assignees: GM Global Technology Operations LLC
- Inventors: Paul E. Krajewski; Yang T. Cheng
- Web page: https://patentgrep.com/patent/US20080185079A1

## CPC

- C22F 1/04: of aluminium or alloys based thereon
- B21D 22/201: {Work-pieces; preparation of the work-pieces, e.g. lubricating, coating}
- B21D 22/205: {Hydro-mechanical deep-drawing}
- B21D 22/208: {by heating the blank or deep-drawing associated with heat treatment (C21D takes precedence)}
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- B21D: WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS OR PROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL (working or processing of wire B21F)

## Abstract

The hot stretch forming of sheet metal alloys, such as highly deformable aluminum alloy materials, is improved by using a lubricant comprising bismuth between the forming tool and the engaged surface of the sheet metal. A precursor of bismuth, such as bismuth subsalicylate, may be dispersed in a liquid and applied to the sheet metal before the sheet is heated to its forming temperature. Other lubricants such as boron nitride may be combined with the bismuth precursor. The precursor compound is decomposed to bismuth (or bismuth and carbon in the case of bismuth subsalicylate) which lubricates contact between the surface(s) of the sheet and the forming tool during forming and removal of the formed part from the tool.

## Claims

### Claim 1

A method of forming sheet metal alloys at elevated temperatures, the method comprising:
applying a lubricant coating to at least a first side of a metal alloy sheet, the lubricant coating comprising bismuth, the sheet having an opposing side;
heating the metal alloy sheet with the lubricant coating to a forming temperature;
forming the sheet into a desired configuration by stretching the first side of the sheet with the lubricant into conformance with a heated forming surface of a forming tool.

### Claim 2 (depends on 1)

A method as set forth in claim 1 further comprising:
suspending particles of a bismuth precursor material in a liquid;
applying a coating of the suspension to at least a first side of a metal alloy sheet;
heating the coating to remove liquid and heating the metal alloy sheet with the lubricant coating to a forming temperature, the bismuth precursor material decomposing to bismuth prior to or during forming of the metal alloy sheet.

### Claim 3 (depends on 2)

A method as set forth in claim 2 wherein the bismuth precursor material is suspended in a liquid comprising at least one of water, an alcohol, or a ketone.

### Claim 4 (depends on 2)

A method as set forth in claim 2 wherein the lubricant as applied comprises bismuth subsalicylate suspended in a liquid.

### Claim 5 (depends on 1)

A method as set forth in claim 1 wherein said metal alloy sheet is an aluminum alloy.

### Claim 6 (depends on 1)

A method as set forth in claim 1 wherein application of said lubricant coating comprises spraying a liquid suspension comprising bismuth-precursor particles.

### Claim 7 (depends on 1)

A method as set forth in claim 1 wherein said lubricant coating further comprises boron nitride.

### Claim 8 (depends on 1)

A method as set forth in claim 1 further comprising:
suspending particles of a bismuth precursor material with particles of boron nitride in a liquid;
applying a coating of the suspension to at least a first side of a metal alloy sheet;
heating the coating to remove liquid and heating the metal alloy sheet with the lubricant coating to a forming temperature, the bismuth precursor material decomposing to bismuth prior to or during forming of the metal alloy sheet.

### Claim 9

A method of forming aluminum alloy sheet material at an elevated temperature, the method comprising:
providing an internally heated forming tool comprising a forming surface at a forming temperature for an aluminum alloy sheet metal workpiece;
providing an aluminum alloy sheet metal workpiece having a first surface for engagement with the forming surface of the forming tool, and an opposing surface;
applying a lubricant coating comprising bismuth to at least one of the forming surface of the forming tool or the first surface of the sheet metal workpiece;
heating the aluminum alloy sheet metal workpiece to a forming temperature in excess of 200° C.; and
producing a shape in the aluminum alloy sheet metal workpiece by applying a pressurized working gas to the opposing surface of the sheet metal workpiece so that the first surface of the sheet metal workpiece is deformed into conformance with said forming surface, the bismuth-containing lubricant acting between the first surface of the metal sheet and the forming surface of the tool.

### Claim 10 (depends on 9)

A method as set forth in claim 9 further comprising:
suspending particles of a bismuth precursor material in a liquid;
applying a coating of the suspension to at least a first side of a metal alloy sheet;
heating the coating to remove liquid; and
further heating the metal alloy sheet with the lubricant coating to a forming temperature, the bismuth precursor material decomposing to bismuth prior to or during forming of the metal alloy sheet.

### Claim 11 (depends on 9)

A method as set forth in claim 9 further comprising: suspending particles of a bismuth precursor material with particles of boron nitride in a liquid;
applying a coating of the suspension to at least a first side of a metal alloy sheet;
heating the coating to remove liquid; and
further heating the metal alloy sheet with the lubricant coating to a forming temperature, the bismuth precursor material decomposing to bismuth prior to or during forming of the metal alloy sheet.