# US 2008/0185075 A1 · HIGH-STRENGHT Co-BASED ALLOY WITH ENHANCED WORKABILITY AND PROCESS FOR PRODUCING THE SAME

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0185075 A1
- Document ID: US20080185075A1
- Status: Published application
- Kind: A1
- Application number: 12/098,746
- Filed: 2008-04-07
- Published: 2008-08-07
- Earliest claimed: 2006-10-11
- Assignees: Japan Science and Technology Agency
- Inventors: Kiyohito ISHIDA; Kiyoshi YAMAUCHI; Ryosuke KAINUMA; Yuji SUTOU; Toshihiro OMORI
- Web page: https://patentgrep.com/patent/US20080185075A1

## CPC

- C22C 19/07: based on cobalt
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A Co-based alloy being useful as a spiral spring, common spring, wire, cable guide, steel belt, build-up material, guide wire, stent, catheter, etc. There is provided a Co-based alloy having a composition of Co—Al binary system containing 3-13% Al loaded with at least one workability enhancing element selected from among 001 to 50% Ni, 0.01 to 40% Fe and 0.01 to 30% Mn and having a lamellar structure wherein f.c.c. structure α-phase and β(B2)-phase are repeated in layers. The lamellar structure is so regulated that the occupancy ratio of the whole structure is 30 vol. % or above and the layer spacing is 100 μm or less. The Co-based alloy may contain at least one optional component selected from among Ga, Cr, V, Ti, Mo, Nb, Zr, W, Ta, Hf, Si, Rh, Pd, Ir, Pt, Au, B, C and P may be added in a total amount of 0.01 to 60%.

## Claims

### Claim 1

A high-strength Co-based alloy comprising: a fundamental composition which comprises, on the basis of mass percent, one or more of 0.01 to 60% of workability enhancing elements selected from 0.01 to 50% of Ni, 0.01 to 40% of Fe and 0.01 to 30% of Mn, and 3 to 13% of Al, and the balance being cobalt and impurities; and a metallic structure having a lamellar structure wherein a f.c.c. structure α-phase and β(B2)-phase with an interlayer spacing of 100 μm or less are repeated in layers and the occupancy ratio is 30% by volume or more.

### Claim 2

The high-strength Co-based alloy, comprising a composition which comprises, on the basis of mass ratio, 3 to 13% of Al and 0.01 to 60% of workability enhancing element, and further comprises one or more members selected from the following:
0.01 to 40% of Cr, 0.01 to 30% of Mo, 0.01 to 5% of Si, 0.01 to 30% of W, 0.01 to 10% of Zr, 0.01 to 15% of Ta, 0.01 to 10% of Hf, 0.01 to 20% of Ga, 0.01 to 20% of V, 0.01 to 12% of Ti, 0.01 to 20% of Nb, 0.001 to 3% of C, 0.01 to 20% of Rh, 0.01 to 20% of Pd, 0.01 to 20% of Ir, 0.01 to 20% of Pt, 0.01 to 10% of Au, 0.001 to 1% of B, and 0.001 to 1% of P in a total of 0.001 to 60%, and the balance being cobalt without incidental impurities; and the lamellar structure wherein the f.c.c. structure α-phase and β(B2)-type phase, a L12-type γ′ phase, a D019-type precipitate, and/or a M23C6-type carbide with an interlayer spacing of 100 μm or less are repeated in layers and the occupancy ratio of the lamellar structure to the whole metallic structure is 30% by volume or more.

### Claim 3 (depends on 1, 2)

A process for producing the high-strength co-based alloy, comprising the steps of: dissolving the Co-based alloy having the composition according to claim 1 or 2; cooling and solidifying with an average cooling rate: 500° C./min or less in the range of 1500 to 600° C.; and crystallizing the f.c.c. structure α-phase and β(B2)-type phase, the L12-type γ′ phase,

### Claim 4 (depends on 1)

The process for producing the high-strength co-based alloy, comprising the steps of: performing solution treatment at 900 to 1400° C. the co-based alloys having the composition according to claim 1; and precipitating the f.c.c. structure α-phase and β(B2)-type phase, the L12-type γ′ phase, the D019-type precipitate, and/or the M23C6-type carbide so as to form the lamellar structure by aging treatment at 500 to 900° C.

### Claim 5 (depends on 3)

The process for producing the high-strength co-based alloy according to claim 3, wherein the Co-based alloy after formation of the lamellar structure is subjected to cold working at a working ratio of 10% or more.