# US 2008/0185030 A1 · Methods of depositing epitaxial thermoelectric films having reduced crack and/or surface defect densities and related devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0185030 A1
- Document ID: US20080185030A1
- Status: Published application
- Kind: A1
- Application number: 12/024,475
- Filed: 2008-02-01
- Published: 2008-08-07
- Earliest claimed: 2007-02-02
- Assignees: Nextreme Thermal Solutions, Inc.
- Inventors: Jonathan Pierce; Robert P. Vaudo
- Web page: https://patentgrep.com/patent/US20080185030A1

## CPC

- H10N 10/01: Manufacture or treatment
- H10N 10/17: characterised by the structure or configuration of the cell or thermocouple forming the device
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

A substrate is provided including a growth surface that is offcut relative to a plane defined by a crystallographic orientation of the substrate at an offcut angle of about 5 degrees to about 45 degrees. A thermoelectric film is epitaxially grown on the growth surface. A crystallographic orientation of the thermoelectric film may be tilted about 5 degrees to about 30 degrees relative to the growth surface. The growth surface of the substrate may also be patterned to define a plurality of mesas protruding therefrom prior to epitaxial growth of the thermoelectric film. Related methods and thermoelectric devices are also discussed.

## Claims

### Claim 1

A method of fabricating a thermoelectric device, the method comprising:
providing a substrate including a growth surface that is offcut relative to a plane defined by a crystallographic orientation of the substrate at an offcut angle in a range of about 5 degrees to about 45 degrees; and then
epitaxially growing a thermoelectric film on the growth surface.

### Claim 2 (depends on 1)

The method of claim 1, wherein the plane defined by the crystallographic orientation of the substrate is a {100} plane, and wherein the growth surface comprises a vicinal growth surface that is offcut from the {100} plane toward a <110> direction.

### Claim 3 (depends on 2)

The method of claim 2, wherein the offcut angle is in a range of about 5 degrees to about 30 degrees.

### Claim 4 (depends on 3)

The method of claim 3, wherein the offcut angle is in a range of about 10 degrees to about 20 degrees.

### Claim 5 (depends on 3)

The method of claim 3, wherein the offcut angle is about 15 degrees relative to the {100} plane toward the <110> direction.

### Claim 6 (depends on 1)

The method of claim 1, wherein a crystallographic orientation of the thermoelectric film is tilted at an angle in a range of about 5 degrees to about 30 degrees relative to the growth surface.

### Claim 7 (depends on 6)

The method of claim 6, wherein a plane defined by the crystallographic orientation of the thermoelectric film is a (0015) plane.

### Claim 8 (depends on 6)

The method of claim 6, wherein the crystallographic orientation of the thermoelectric film is tilted at an angle in a range of about 10 degrees to about 25 degrees.

### Claim 9 (depends on 8)

The method of claim 8, wherein the crystallographic orientation of the thermoelectric film is tilted at an angle of about 18 degrees to about 24 degrees relative to the growth surface.

### Claim 10 (depends on 8)

The method of claim 8, wherein the crystallographic orientation of the thermoelectric film is tilted at an angle of about 20 degrees relative to the growth surface.

### Claim 11 (depends on 1)

The method of claim 1, wherein the thermoelectric film comprises a compound comprising bismuth (Bi), antimony (Sb), lead (Pb), tellurium (Te), and/or selenium (Se).

### Claim 12 (depends on 1)

The method of claim 1, wherein the substrate comprises gallium arsenide (GaAs), silicon (Si), barium fluoride (BaF), silicon carbide (SiC), gallium nitride (GaN), aluminum nitride (AlN), sapphire, and/or glass.

### Claim 13 (depends on 1)

The method of claim 1, further comprising the following prior to epitaxially growing the thermoelectric film:
patterning the growth surface of the substrate to define a plurality of mesas protruding therefrom.

### Claim 14 (depends on 1)

The method of claim 1, further comprising the following prior to epitaxially growing the thermoelectric film:
forming a mask pattern on the growth surface of the substrate to expose a plurality of portions thereof,
wherein epitaxially growing the thermoelectric film comprises epitaxially growing the thermoelectric film on the plurality of exposed portions of the growth surface.

### Claim 15 (depends on 14)

The method of claim 14, further comprising:
epitaxially growing a thermoelectric film seed layer on the growth surface prior to forming the mask pattern thereon.

### Claim 16 (depends on 1)

The method of claim 1, wherein the thermoelectric film has a crack density of less than about 1 crack per millimeter (mm).

### Claim 17 (depends on 16)

The method of claim 16, wherein epitaxially growing the thermoelectric film comprises epitaxially growing the thermoelectric film to a thickness in a range of about 5 micrometers (μm) to about 100 μm.

### Claim 18 (depends on 17)

The method of claim 17, wherein epitaxially growing the thermoelectric film comprises epitaxially growing the thermoelectric film to a thickness of about 40 μm or less.

### Claim 19 (depends on 16)

The method of claim 16, wherein the thermoelectric film has a crack density of less than about 1 crack per centimeter (cm).

### Claim 20 (depends on 1)

The method of claim 1, further comprising:
forming at least one intermediate layer on the growth surface of the substrate prior to epitaxially growing the thermoelectric film thereon.

### Claim 21 (depends on 20)

The method of claim 20, wherein the intermediate layer comprises a strained layer superlattice.

### Claim 22 (depends on 20)

The method of claim 20, wherein the intermediate layer comprises a graded layer having a lattice constant between that of the substrate and the thermoelectric film.

### Claim 23

A method of fabricating a thermoelectric device, the method comprising:
patterning a substrate to define a growth surface having a plurality of mesas protruding therefrom; and then
epitaxially growing a thermoelectric film on the growth surface.

### Claim 24 (depends on 23)

The method of claim 23, wherein epitaxially growing the thermoelectric film comprises epitaxially growing the thermoelectric film including a plurality of mesas protruding from the growth surface.

### Claim 25 (depends on 24)

The method of claim 24, wherein the plurality of mesas of the thermoelectric film are elliptical or rectangular in plan view.

### Claim 26 (depends on 25)

The method of claim 25, wherein the plurality of mesas of the thermoelectric film comprise elongated rectangular mesas extending in a direction substantially parallel to at least one crack in the thermoelectric film.

### Claim 27 (depends on 25)

The method of claim 25, wherein the plurality of mesas of the thermoelectric film have a diameter or width of about 200 micrometers (μm) or less.

### Claim 28 (depends on 24)

The method of claim 24, wherein a mesa of the thermoelectric film has a crack density of less than about 1 crack per millimeter (mm).

### Claim 29 (depends on 24)

The method of claim 24, wherein a crystallographic orientation of the thermoelectric film is tilted at an angle in a range of about 5 degrees to about 30 degrees relative to the growth surface.

### Claim 30 (depends on 29)

The method of claim 29, wherein the plurality of mesas of the thermoelectric film have a diameter or width of about 400 micrometers (μm) or less.

### Claim 31 (depends on 29)

The method of claim 29, wherein the plurality of mesas of the thermoelectric film have a diameter or width of about 300 micrometers (μm) or less.

### Claim 32 (depends on 29)

The method of claim 29, wherein the substrate comprises a vicinal growth surface that is offcut relative to a plane defined by a crystallographic orientation of the substrate at an offcut angle in a range of about 5 degrees to about 45 degrees.

### Claim 33 (depends on 32)

The method of claim 32, wherein the plane defined by the crystallographic orientation of the substrate is a {100} plane, and wherein the vicinal growth surface is offcut from the {100} plane toward a <110> direction.

### Claim 34 (depends on 33)

The method of claim 33, wherein the offcut angle is in a range of about 5 degrees to about 30 degrees.

### Claim 35 (depends on 23)

The method of claim 23, further comprising:
epitaxially growing a thermoelectric film seed layer on the substrate prior to patterning the substrate.

### Claim 36

A thermoelectric device, comprising:
a thermoelectric element comprising a thermoelectric film having a crystallographic orientation that is tilted at an angle in a range of about 5 degrees to about 30 degrees relative to a surface of the thermoelectric film.

### Claim 37 (depends on 36)

The device of claim 36, wherein the crystallographic orientation of the thermoelectric film is tilted at an angle in a range of about 10 degrees to about 25 degrees relative to a surface of the thermoelectric film.

### Claim 38 (depends on 36)

The device of claim 36, wherein the thermoelectric film comprises a compound comprising bismuth (Bi), antimony (Sb), lead (Pb), tellurium (Te), and/or selenium (Se).

### Claim 39 (depends on 36)

The device of claim 36, wherein the thermoelectric film has a thickness in a range of about 5 micrometers (μm) to about 100 μm.

### Claim 40 (depends on 39)

The device of claim 39, wherein the thermoelectric film has a thickness of about 40 μm or less.

### Claim 41 (depends on 36)

The device of claim 36, wherein the thermoelectric film has a crack density of less than about 1 crack per millimeter (mm).

### Claim 42 (depends on 36)

The device of claim 36, further comprising:
a second thermoelectric element comprising a second thermoelectric film having a crystallographic orientation that is tilted at an angle in a range of about 5 degrees to about 30 degrees relative to a surface of the second thermoelectric film, wherein the first and second thermoelectric elements have different conductivity types; and
first and second headers,
wherein the first and second thermoelectric elements are electrically coupled in series and are thermally coupled in parallel between the first and second headers.

### Claim 43

A thermoelectric film, comprising:
a thermoelectric material layer having a thickness of less than about 100 micrometers (μm) and a crack density of less than about 1 crack per millimeter (mm).

### Claim 44 (depends on 43)

The thermoelectric film of claim 43, wherein a crystallographic orientation of the thermoelectric material layer is tilted at an angle in a range of about 5 degrees to about 30 degrees relative to a surface of the thermoelectric material layer.

### Claim 45 (depends on 44)

The method of claim 44, wherein a plane defined by the crystallographic orientation of the thermoelectric material layer is a (0015) plane.

### Claim 46 (depends on 43)

The thermoelectric film of claim 43, wherein the thermoelectric material layer has a thickness in a range of about 5 micrometers (μm) to about 100 μm and comprises a compound comprising bismuth (Bi), antimony (Sb), lead (Pb), tellurium (Te), and/or selenium (Se).