# US 2008/0175125 A1 · Optical recording medium and recording film material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0175125 A1
- Document ID: US20080175125A1
- Status: Published application
- Kind: A1
- Application number: 12/010,163
- Filed: 2008-01-22
- Published: 2008-07-24
- Earliest claimed: 2007-01-23
- Assignees: TDK Corporation
- Inventors: Hiroshi Shingai; Tatsuya Kato; Masanori Kosuda; Hiroshi Takasaki; Hideki Hirata; Hajime Utsunomiya
- Web page: https://patentgrep.com/patent/US20080175125A1

## CPC

- G11B 7/24038: Multiple laminated recording layers
- G11B 7/2433: Metals or elements of Groups 13, 14, 15 or 16 of the Periodic Table, e.g. B, Si, Ge, As, Sb, Bi, Se or Te
- G11B 7/2578: consisting essentially of inorganic materials
- G11B 7/259: based on silver
- G11B 2007/24312: {group 14 elements (e.g. Si, Ge, Sn)}
- G11B 2007/24314: {group 15 elements (e.g. Sb, Bi)}
- G11B 2007/24316: {group 16 elements (i.e. chalcogenides, Se, Te)}
- G11B 2007/25706: {containing transition metal elements (Zn, Fe, Co, Ni, Pt)}
- G11B 2007/25715: {containing oxygen}
- Y10T 428/21: Circular sheet or circular blank
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A next-generation optical recording medium has two or more information layers which include a translucent information layer. The translucent information layer has a recording film and an interface layer, provided adjacent to the recording film on the side of the light incident surface. The recording film is made of a phase change material having SbxTeyGez elements and elemental ratios. Y satisfies 5≦y≦15 and z satisfies 5≦z≦15. When In having an elemental ratio of a is further added and x+y+z+a=100 holds, a satisfies 4≦a≦15. The interface layer comprises of ZrO2—Cr2O3 film thickness of which is in a range of from 2 nm to 10 nm. When ZrO2:Cr2O3═C:D (mol %), the compositional ratios ZrO2 and Cr2O3 in the ZrO2—Cr2O3 film, holds, the C satisfies 20≦C≦90, and the D satisfies 10≦D≦80, and the C and the D satisfy C+D=100. The ZrO2 is stabilized ZrO2 which contains Y2O3, when ZrO2:Y2O3=(100-X):X (mol %), the compositional ratios ZrO2 and Y2O3 in the stabilized ZrO2, holds, the X satisfies 2≦X≦10.

## Claims

### Claim 1

An optical recording medium comprising:
a substrate;
a first information layer which is provided on the substrate on a side of a light incident surface on which a laser beam is incident; and
at least one translucent information layer which is provided further on the side of the light incident surface than the first information layer,
wherein the translucent information layer comprises a recording film which is made of a phase change material having SbxTeyGez elements and specific elemental ratios,
wherein the y holds 5≦y≦15, z holds 5≦z≦15,
wherein NA represents the numerical aperture of an objective lens, and λ represents a wavelength of the laser beam, the recording film is rewritable using an optical system of λ/NA≦650 nm, and
wherein, when x+y+z+a=100 holds by adding In with an elemental ratio of a, 4≦a≦15 holds.

### Claim 2 (depends on 1)

The optical recording medium according to claim 1, wherein when 77≦b≦84 holds, the elemental ratios x and a satisfy x=−0.713×a+b.

### Claim 3 (depends on 1)

The optical recording medium according to claim 1, wherein the recording film has a thickness in a range of from 3 nm to 7 nm both inclusive.

### Claim 4 (depends on 2)

The optical recording medium according to claim 2, wherein the recording film has a thickness in a range of from 3 nm to 7 nm both inclusive.

### Claim 5 (depends on 1)

The optical recording medium according to claim 1, wherein the translucent information layer comprises a reflective layer provided on an opposite side of a light incident surface of the recording film and the reflective layer has a thickness in a range of from 8 nm to 16 nm both inclusive.

### Claim 6 (depends on 2)

The optical recording medium according to claim 2, wherein the translucent information layer comprises a reflective layer provided on an opposite side of a light incident surface of the recording film and the reflective layer has a thickness in a range of from 8 nm to 16 nm both inclusive.

### Claim 7 (depends on 3)

The optical recording medium according to claim 3, wherein the translucent information layer comprises a reflective layer provided on an opposite side of a light incident surface of the recording film and the reflective layer has a thickness in a range of from 8 nm to 16 nm both inclusive.

### Claim 8 (depends on 4)

The optical recording medium according to claim 4, wherein the translucent information layer comprises a reflective layer provided on an opposite side of a light incident surface of the recording film and the reflective layer has a thickness in a range of from 8 nm to 16 nm both inclusive.

### Claim 9 (depends on 1)

The optical recording medium according to claim 1, wherein the translucent information layer comprises an interface layer provided adjacent to the recording film on the side of the light incident surface and the interface layer contains at least Cr and O.

### Claim 10 (depends on 2)

The optical recording medium according to claim 2, wherein the translucent information layer comprises an interface layer provided adjacent to the recording film on the side of the light incident surface and the interface layer contains at least Cr and O.

### Claim 11 (depends on 3)

The optical recording medium according to claim 3, wherein the translucent information layer comprises an interface layer provided adjacent to the recording film on the side of the light incident surface and the interface layer contains at least Cr and O.

### Claim 12 (depends on 4)

The optical recording medium according to claim 4, wherein the translucent information layer comprises an interface layer provided adjacent to the recording film on the side of the light incident surface and the interface layer contains at least Cr and O.

### Claim 13 (depends on 5)

The optical recording medium according to claim 5, wherein the translucent information layer comprises an interface layer provided adjacent to the recording film on the side of the light incident surface and the interface layer contains at least Cr and O.

### Claim 14 (depends on 6)

The optical recording medium according to claim 6, wherein the translucent information layer comprises an interface layer provided adjacent to the recording film on the side of the light incident surface and the interface layer contains at least Cr and O.

### Claim 15 (depends on 9)

The optical recording medium according to claim 9, wherein the translucent information layer contains a heat sink layer, a dielectric layer, the interface layer, and the recording film and comprises their stacked in this order from the light incident surface, and the heat sink layer comprises an AlN film.

### Claim 16 (depends on 9)

The optical recording medium according to claim 9, wherein the interface layer is made of ZrO2—Cr2O3 film, and the ZrO2—Cr2O3 film has a thickness in a range of from 2 nm to 10 nm both inclusive.

### Claim 17 (depends on 16)

The optical recording medium according to claim 16, wherein when ZrO2:Cr2O3═C:D (mol %), the compositional ratios ZrO2 and Cr2O3 in the ZrO2—Cr2O3 film, holds, the C satisfies 20≦C≦90, and the D satisfies 10≦D≦80, and the C and the D satisfy C+D=100.

### Claim 18 (depends on 16)

The optical recording medium according to claim 16, wherein the ZrO2 is stabilized ZrO2 which contains Y2O3, when ZrO2:Y2O3=(100-X):X (mol %), the compositional ratios ZrO2 and Y2O3 in the stabilized ZrO2, holds, the X satisfies 2≦X≦10.

### Claim 19

An optical recording medium comprising:
a substrate;
a first information layer which is provided on the substrate on a side of a light incident surface on which a laser beam is incident; and
at least one translucent information layer which is provided further on the side of said light incident surface than the first information layer,
wherein the translucent information layer comprises: a recording film which is rewritable using an optical system of λ/NA≦650 nm when NA represents the numerical number of an objective lens and λ represents a wavelength of the laser beam; and a protective layer adjacent to the recording film on the side of the substrate side, and
wherein the recording film is made of an Sb-based eutectic phase change material having Sb as a main composition and the protective layer contains at least Cr and O.

### Claim 20

A recording film material comprising a phase change material having SbxTeyGez elements and elemental ratios in which y satisfies 5≦y≦15 and z satisfies 5≦z≦15, the recording film material for making a recording film which is rewritable using an optical system of λ/NA≦650 nm when NA represents the numerical number of an objective lens and λ represents a wavelength of a laser beam, wherein
when In having an elemental ratio of a is further added and x+y+z+a=100 holds, the a satisfies 4≦a≦15.