# US 2008/0166589 A1 · Component having a coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0166589 A1
- Document ID: US20080166589A1
- Status: Published application
- Kind: A1
- Application number: 11/210,034
- Filed: 2005-08-23
- Published: 2008-07-10
- Earliest claimed: 2005-08-02
- Assignees: MTU Aero Engines AG
- Inventors: Anton Albrecht; Thomas Cosack; Thomas Dautl; Horst Pillhoefer
- Web page: https://patentgrep.com/patent/US20080166589A1

## CPC

- F01D 5/288: {Protective coatings for blades}
- C23C 10/16: more than one element being diffused in more than one step
- C23C 10/58: more than one element being diffused in more than one step
- C23C 28/042: {including a refractory ceramic layer, e.g. refractory metal oxides, ZrO2, rare earth oxides}
- C23C 28/048: {with layers graded in composition or physical properties}
- F05C 2201/0466: Nickel
- F05D 2300/121: Aluminium
- F05D 2300/143: Platinum group metals, i.e. Os, Ir, Pt, Ru, Rh, Pd
- Y10T 428/12611: Oxide-containing component
- Y10T 428/12618: Plural oxides
- Y10T 428/12736: Al-base component
- Y10T 428/1275: Next to Group VIII or IB metal-base component
- Y10T 428/12875: Platinum group metal-base component
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- F05C: INDEXING SCHEME RELATING TO MATERIALS, MATERIAL PROPERTIES OR MATERIAL CHARACTERISTICS FOR MACHINES, ENGINES OR PUMPS OTHER THAN NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A component having a corrosion-resistant and/or oxidation-resistant coating is provided that includes at least one platinum-aluminum substrate area is provided, the component having a substrate surface (11) and a substrate composition based on nickel, with a platinum-aluminum substrate area (12) formed in the area of the substrate surface of the component by precipitating platinum (Pt) and aluminum (Al) on the substrate surface. The platinum-aluminum substrate area (12) has a two-phase structure or duplex structure with finely dispersed platinum-aluminum deposits in a nickel-based mixed crystal in an outer zone (13), and a single-phase structure made of a nickel-based mixed crystal in an inner zone (14) located between the substrate surface (11) of the component and the outer zone (13).

## Claims

### Claim 1

A component having a corrosion-resistant and/or oxidation-resistant coating, comprising
a component having a substrate composition including nickel, the component having a substrate surface;
a platinum-aluminum substrate area formed by precipitating platinum (Pt) and aluminum (Al) on the substrate surface,
the platinum-aluminum substrate area having an inner zone and an outer zone, wherein:
the outer zone including a two-phase structure or duplex structure including finely dispersed platinum-aluminum deposits in a nickel-based mixed crystal, and
the inner zone including a single-phase structure of a nickel-based mixed crystal, and
the inner zone is located between the substrate surface of the component and the outer zone.

### Claim 2 (depends on 1)

The component as recited in claim 1, wherein the outer zone having the two-phase structure or duplex structure has finely dispersed, globulitic PtAl2 deposits between 0.1 μm and 3.0 μm in size in a mixed crystal of β-NiAl, the proportion of the two-phase structure or duplex structure being between 2.0% by volume and 40.0% by volume of the outer zone, and the aluminum proportion in the mixed crystal being greater than 20.0% by weight.

### Claim 3 (depends on 2)

The component as recited in claim 2, wherein the outer zone having the two-phase structure or duplex structure has finely dispersed, globulitic PtAl2 deposits between 0.1 μm and 1.0 μm in size in a mixed crystal of β-NiAl, the proportion of the two-phase structure or duplex structure being between 2.0% by volume and 20.0% by volume of the outer layer, and the Al proportion in the mixed crystal being greater than 25.0% by weight.

### Claim 4 (depends on 1)

The component as recited in claim 1, wherein the inner zone is a diffusion zone, and in the inner zone, the Al proportion in the nickel-based mixed crystal is a maximum of 15.0% by weight and the Pt proportion in the nickel-based mixed crystal is a maximum of 8.0% by weight.

### Claim 5 (depends on 4)

The component as recited in claim 4, wherein the inner zone is a diffusion zone, and wherein the maximum proportion of Al in the nickel-based mixed crystal is 10.0% by weight.

### Claim 6 (depends on 1)

The component as recited in claim 1, wherein the platinum-aluminum substrate area in the outer zone and/or in the inner zone has a maximum yttrium proportion of 1.5% by weight and/or a maximum hafnium proportion of 1.5% by weight.

### Claim 7 (depends on 1)

The component as recited in claim 1, further comprising a ceramic layer deposited onto the platinum-aluminum substrate area, a thin aluminum oxide intermediate layer being formed between the platinum-aluminum substrate area and the ceramic layer.

### Claim 8 (depends on 7)

The component as recited in claim 7, wherein the aluminum oxide intermediate layer includes an Al2O3 intermediate layer having a minimum proportion of 90.0% by volume of alpha Al2O3 with a rhombohedral crystal lattice structure, and a maximum proportion of 10.0% by volume of gamma Al2O3 with a cubic crystal lattice structure.

### Claim 9 (depends on 7)

The component as recited in claim 7, wherein the ceramic layer includes a zirconium oxide layer with a maximum proportion of 8.0% by weight of yttrium oxide.

### Claim 10 (depends on 1)

The component as recited in claim 1, wherein the component includes a directionally solidified or a monocrystalline substrate composition including nickel, with a nickel proportion between 18.0% by weight and 48.0% by weight and an aluminum proportion between 1.0% by weight and 8.0% by weight.

### Claim 11

A corrosion-resistant and/or oxidation-resistant coating for a component, comprising:
a platinum-aluminum substrate area formed by precipitating platinum (Pt) and aluminum (Al),
the platinum-aluminum substrate area having an inner zone and an outer zone, wherein
the platinum-aluminum substrate area has a two-phase structure or duplex structure in the outer zone, the two-phase structure or duplex structure including finely dispersed platinum-aluminum deposits in a nickel-based mixed crystal, and
the platinum-aluminum substrate area has a single-phase structure of a nickel-based mixed crystal in the inner zone, and
the inner zone is located between the component and the outer zone.

### Claim 12 (depends on 1)

A method for producing the-corrosion-resistant and/or oxidation-resistant coating as recited in claim 1, comprising the steps of
precipitating platinum onto a surface of a substrate of the component;
then diffusing the platinum being into the substrate surface; and
then alitizating the substrate, said alitizating further comprising
precipitating aluminum thermochemically in a high-activity gas phase process, and thereafter,
diffusing aluminum into the substrate surface, such that a platinum-aluminum substrate area is formed.

### Claim 13 (depends on 12)

The method as recited in claim 12, wherein the platinum is precipitated onto the substrate surface such that the forming platinum layer has a thickness of 1.0 μm to 10.0 μm, preferably of 2.0 μm to 4.0 μm.

### Claim 14 (depends on 12)

The method as recited in claim 12, wherein the platinum is diffused at a temperature between 960° C. and 1,160° C., and at a holding time of between 5 minutes and 60 minutes.

### Claim 15 (depends on 12)

The method as recited in claim 12, wherein the platinum is diffused at a temperature between 1000° C. and 1,100° C., and at a holding time of between 5 minutes and 15 minutes.

### Claim 16 (depends on 12)

The method as recited in claim 12, wherein the thermochemical precipitation of aluminum is carried out with an atmosphere of aluminum monohalogenides.

### Claim 17 (depends on 16)

The method as recited in claim 16, wherein the atmosphere has a proportion of aluminum monohalogenides of at least 15% by volume, and the pressure when precipitating aluminum is 10 mbar to 800 mbar over ambient pressure.

### Claim 18 (depends on 12)

The method as recited in claim 12, wherein the diffusing of aluminum occurs at an activity level of the aluminum of at least 50 atom % in relation to pure nickel, at a temperature that is at least 10° C. below the platinum annealing temperature, and at a holding time of between 180 minutes and 360 minutes.

### Claim 19 (depends on 12)

The method as recited in claim 12, further comprising
depositing an aluminumoxide intermediate layer over the platinum-aluminum substrate area; and
depositing a ceramic layer over the aluminum oxide intermediate layer.

### Claim 20 (depends on 19)

The method as recited in claim 19, wherein the step of depositing the aluminum-oxide intermediate layer comprises depositing an Al2O3 intermediate layer, and wherein the depositing includes the steps of cleaning the platinum-aluminum substrate area, heating the aluminum substrate area under a high vacuum and then holding it at the heated temperature and at a low vacuum or partial vacuum, the atmosphere of the low vacuum or partial vacuum including 25% by volume to 60% by volume oxygen and 75% by volume to 40% by volume of argon or helium.

### Claim 21 (depends on 18)

The method as recited in claim 18, wherein the step of depositing the ceramic layer comprises precipitating a zirconium oxide layer with a maximum proportion of 8.0% by weight of yttrium dioxide onto the aluminum oxide intermediate layer.

### Claim 22 (depends on 1)

The component as recited in claim 1 wherein the inner zone includes aluminum and platinum.