# US 2008/0166578 A1 · Wear Resistant Lead Free Alloy Bushing and Method of Making

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0166578 A1
- Document ID: US20080166578A1
- Status: Published application
- Kind: A1
- Application number: 11/830,913
- Filed: 2007-07-31
- Published: 2008-07-10
- Earliest claimed: 2007-01-05
- Assignees: Federal-Mogul World Wide, Inc.
- Inventors: David M. Saxton; James M. Carpenter; Gregory W. Sevenski; Holger Schmitt; Gerd Andler
- Web page: https://patentgrep.com/patent/US20080166578A1

## CPC

- F16C 33/14: Special methods of manufacture; Running-in
- B22F 7/08: with one or more parts not made from powder {(B22F7/062 takes precedence)}
- C22C 9/02: with tin as the next major constituent
- C22C 32/0047: {with carbides, nitrides, borides or silicides as the main non-metallic constituents}
- F16C 33/121: {Use of special materials}
- B22F 2998/10: Processes characterised by the sequence of their steps
- F16C 2204/10: Alloys based on copper
- F16C 2204/12: with tin as the next major constituent
- F16C 2220/20: by sintering pulverised material, e.g. powder metallurgy
- F16C 2223/32: by attaching pre-existing layers, e.g. resin sheets or foils by adhesion to a substrate; Laminating
- Y02T 10/86: Optimisation of rolling resistance, e.g. weight reduction
- Y10T 428/12014: having metal particles
- Y10T 428/12049: Nonmetal component
- Y10T 428/12056: Entirely inorganic
- Y10T 428/12063: Nonparticulate metal component
- Y10T 428/1209: Plural particulate metal components
- F16C: SHAFTS; FLEXIBLE SHAFTS; ELEMENTS OR CRANKSHAFT MECHANISMS; ROTARY BODIES OTHER THAN GEARING ELEMENTS; BEARINGS
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A bearing having improved wear resistance has a bearing material of a copper-tin-bismuth alloy which may also include phosphorus which has excellent strength, due to the solid solution of copper, tin and phosphorus (when used), attached to a steel backing shell. The material also has good lubricity as a result of the presence of the bismuth which also promotes tin mobilization and formation of a layer of tin on the bearing surface upon use of the bearing. The addition of small amounts of relatively small hard particles in the copper-tin-matrix, particularly Fe3P, MoSi2 or a mixture thereof, provides a suitable hard surface artifact to improve the wear resistance of the bearing material. The bearing includes a sintered powder compact bearing material of a copper-tin-bismuth alloy powder and a metal compound powder which is bonded to a steel backing shell, wherein the metal compound powder has an average particle size of less than 10 μm.

## Claims

### Claim 1

A bearing comprising a sintered powder compact bearing material of a copper-tin-bismuth alloy powder and a metal compound powder which is bonded to a steel backing shell, wherein said metal compound powder has an average particle size of less than 10 μm.

### Claim 2 (depends on 1)

The bearing of claim 1, wherein said metal compound powder is selected from a group consisting of metal boride, metal silicide, metal oxide, metal nitride, metal carbide, metal phosphide and intermetallic compounds.

### Claim 3 (depends on 1)

The bearing of claim 1, wherein said copper-tin-bismuth alloy comprises, by weight: 8-15% tin, 1-30% bismuth and the balance essentially copper.

### Claim 4 (depends on 3)

The bearing of claim 3, wherein said copper-tin-bismuth alloy comprises, by weight: 8-12% tin, 1-<5% bismuth and the balance essentially copper.

### Claim 5 (depends on 1)

The bearing of claim 1, further comprising phosphorus as an alloy constituent of the copper-tin-bismuth alloy powder.

### Claim 6 (depends on 3)

The bearing of claim 3, further comprising phosphorus as an alloy constituent, wherein said phosphorus comprises, by weight, 0.03-0.8% of the copper-tin-bismuth alloy powder.

### Claim 7 (depends on 4)

The bearing of claim 4, wherein said phosphorus comprises, by weight, 0.03-0.08% of the copper-tin-bismuth alloy powder.

### Claim 8 (depends on 1)

The bearing of claim 1, wherein said metal compound powder comprises at least one of an Fe3P powder and an MoSi2 powder.

### Claim 9 (depends on 8)

The bearing of claim 8, wherein said metal compound powder comprises said Fe3P powder and said MoSi2 powder.

### Claim 10 (depends on 9)

The bearing of claim 9, wherein said MoSi2 powder comprises 0.1-0.5% by weight of the compact bearing material.

### Claim 11 (depends on 1)

The bearing of claim 1, wherein said metal compound powder comprises 0.1-10% by volume of the compact bearing material.

### Claim 12 (depends on 11)

The bearing of claim 11, wherein said metal compound powder comprises 1-2% by volume of the compact bearing material.

### Claim 13 (depends on 1)

The bearing of claim 1, wherein said copper-tin-bismuth alloy powder comprises a mixture of a gas atomized powder and a water atomized powder.

### Claim 14

A bearing comprising a sintered powder compact of a copper-tin-bismuth alloy powder, an Fe3P powder and an MoSi2 powder which is bonded to a steel backing shell.

### Claim 15 (depends on 14)

The bearing of claim 14, wherein said Fe3P powder and said MoSi2 powder together comprise 0.1-10% by volume of said compact.

### Claim 16 (depends on 14)

The bearing of claim 14, wherein said Fe3P powder and said MoSi2 powder each have an average particle size of less than 10 μm.

### Claim 17 (depends on 14)

The bearing of claim 14, wherein said copper-tin-bismuth alloy comprises, by weight: 8-15% tin, 1-30% bismuth and the balance essentially copper.

### Claim 18 (depends on 17)

The bearing of claim 17, wherein said copper-tin-bismuth alloy comprises, by weight: 8-12% tin, 1-<5% bismuth and the balance essentially copper.

### Claim 19 (depends on 14)

The bearing of claim 14, further comprising phosphorus as an alloy constituent of the copper-tin-bismuth alloy powder.

### Claim 20 (depends on 17)

The bearing of claim 17, further comprising phosphorus as an alloy constituent, wherein said phosphorus comprises, by weight, 0.03-0.8% of the copper-tin-bismuth alloy powder.

### Claim 21 (depends on 20)

The bearing of claim 20, wherein said phosphorus comprises, by weight, 0.03-0.08% of the copper-tin-bismuth alloy powder.

### Claim 22 (depends on 14)

The bearing of claim 14, wherein said MoSi2 comprises 0.1-0.5% by weight of the compact.

### Claim 23 (depends on 17)

The bearing of claim 17, further comprising a molybdenum phosphorus compound as a reaction product of said MoSi2 powder and at least one of said Fe3P powder or said phosphorus.

### Claim 24

A method of making a bearing comprising the steps of:
applying a mixture of a copper-tin-bismuth alloy powder and a metal compound powder having an average particle size of less than 10 μm to a steel backing shell;
heating the powder mixture and steel backing shell to produce a sintered powder mixture and bond the sintered powder mixture to the steel backing shell; and
rolling the sintered powder mixture and steel backing shell to reduce a porosity of the sintered powder mixture and produce a fully-dense sintered compact bearing material.

### Claim 25 (depends on 24)

The method of claim 24, further comprising a step of heating the fully dense bearing material sufficiently to promote interdiffusion within the bearing material at sites associated with the porosity.

### Claim 26 (depends on 25)

The method of claim 25, further comprising a step of running-in the bearing sufficiently to produce a tin-rich surface layer.

### Claim 27 (depends on 24)

The method of claim 24, wherein said copper-tin-bismuth alloy powder comprises, by weight: 8-12% tin, 1-<5% bismuth, and the balance essentially copper, and the metal compound powder comprises at least one of an Fe3P powder and an MoSi2 powder.

### Claim 28 (depends on 27)

The method of claim 27, wherein the metal compound powder comprises Fe3P powder and MoSi2 powder.

### Claim 29

A method of making a bearing comprising the steps of:
applying a powder mixture of a copper-tin-bismuth alloy powder, an Fe3P powder and an MoSi2 powder to a steel backing shell;
heating the powder mixture and steel backing shell to produce a sintered powder mixture and bond the sintered powder mixture to the steel backing shell; and
rolling the sintered powder mixture and steel backing shell to reduce a porosity of the sintered powder mixture and produce a fully dense sintered compact bearing material.

### Claim 30 (depends on 29)

The method of claim 29, further comprising a step of heating the fully dense bearing material sufficiently to promote interdiffusion within the bearing material at sites associated with the porosity.

### Claim 31 (depends on 30)

The method of claim 30, further comprising a step of running-in the bearing sufficiently to produce a tin-rich surface layer.

### Claim 32 (depends on 29)

The method of claim 29, wherein said Fe3P powder and said MoSi2 powder together comprise 0.1-10% by volume of said compact.

### Claim 33 (depends on 29)

The method of claim 29, wherein said Fe3P powder and said MoSi2 powder each have an average particle size of less than 10 μm.

### Claim 34 (depends on 29)

The method of claim 29, wherein said copper-tin-bismuth alloy comprises, by weight: 8-12% tin, 1-<5% bismuth and the balance essentially copper.

### Claim 35 (depends on 34)

The method of claim 34, further comprising phosphorus as an alloy constituent of the copper-tin-bismuth alloy powder.

### Claim 36 (depends on 35)

The method of claim 35, wherein the phosphorus comprises, by weight, 0.03-0.8% of the copper-tin-bismuth alloy powder.

### Claim 37 (depends on 36)

The method of claim 36, wherein the MoSi2 comprises 0.1-0.5% by weight of the powder mixture.

### Claim 38 (depends on 35)

The method of claim 35, wherein the fully dense sintered compact bearing material comprises a molybdenum phosphorus compound as a reaction product of said MoSi2 powder and at least one of the F3P powder or the phosphorus.