Methods for reducing carbon contamination when melting highly reactive alloys
AssigneeGeneral Electric Company
InventorsThomas Joseph Kelly, Michael James Weimer, Bernard Patrick Bewlay, Michael Francis Xavier Gigliotti
Life of this patent
Estimating the term…
Abstract
Methods for reducing carbon contamination when melting highly reactive alloys involving providing a graphite crucible having an interior, applying at least a first protective layer to the interior of the graphite crucible, placing a highly reactive alloy into the crucible having the first protective layer, and melting the highly reactive alloy to obtain a melted alloy having reduced carbon contamination.
Claims20
A method for reducing carbon contamination when melting highly reactive alloys comprising:
- providing a graphite crucible having an interior;
- applying at least a first protective layer to the interior of the graphite crucible;
- placing a highly reactive alloy into the crucible having the first protective layer;
- and
- melting the highly reactive alloy to obtain a melted alloy having reduced carbon contamination.
A method for reducing carbon contamination when melting highly reactive alloys comprising:
- providing a graphite crucible having an interior;
- applying a first protective layer to the interior of the graphite crucible;
- applying a second protective layer to the interior of the graphite crucible on top of the first protective layer;
- placing a highly reactive alloy into the crucible having the first protective layer and the second protective layer;
- and
- melting the highly reactive alloy to obtain a melted alloy having reduced carbon contamination.