# US 2008/0076838 A1 · Methods of preparing silica sols, and stable high-solids silica sols prepared thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0076838 A1
- Document ID: US20080076838A1
- Status: Published application
- Kind: A1
- Application number: 11/858,941
- Filed: 2007-09-21
- Published: 2008-03-27
- Earliest claimed: 2006-09-21
- Assignees: H.C. Starck GmbH
- Inventors: Lothar Puppe
- Web page: https://patentgrep.com/patent/US20080076838A1

## CPC

- F01M 11/04: Filling or draining lubricant of or from machines or engines
- C01B 33/148: Concentration; Drying; Dehydration; Stabilisation; Purification {(C01B33/1465 takes precedence)}
- F01M: LUBRICATING OF MACHINES OR ENGINES IN GENERAL; LUBRICATING INTERNAL COMBUSTION ENGINES; CRANKCASE VENTILATING
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

Methods comprising: (a) providing a silica sol having a BET surface area of 15 to 1000 m2/g and a solids content of up to 45% by weight of silicon dioxide, based on the silica sol; (b) mixing the silica sol and an anionic polyether carboxylate to form a mixture, wherein the anionic polyether carboxylate is mixed with the silica sol in an amount of 0.01 to 10% by weight, based on the mixture; and (c) concentrating the mixture to form a concentrated mixture having a solids content of 20 to 70% by weight of silicon dioxide, based on the concentrated mixture; and the concentrated sols prepared thereby.

## Claims

### Claim 1

A method comprising: (a) providing a silica sol having a BET surface area of 15 to 1000 m2/g and a solids content of up to 45% by weight of silicon dioxide, based on the silica sol; (b) mixing the silica sol and an anionic polyether carboxylate to form a mixture, wherein the anionic polyether carboxylate is mixed with the silica sol in an amount of 0.01 to 10% by weight, based on the mixture; and (c) concentrating the mixture to form a concentrated mixture having a solids content of 20 to 70% by weight of silicon dioxide, based on the concentrated mixture.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the silica sol has a BET surface area of 15 to 800 m2/g.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the silica sol has a pH of 2 to 12.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the silica sol has a pH of 8 to 11.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the silica sol comprises silicon dioxide particles having a mean particle diameter of 3 nm to 250 nm.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the silica sol comprises silicon dioxide particles having a mean particle diameter of 9 nm to 120 nm.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the concentrated mixture has a solids content of 35 to 65% by weight.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the concentrated mixture has a solids content of 40 to 60% by weight.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the anionic polyether carboxylate is mixed with the silica sol in an amount of 0.05 to 10% by weight, based on the mixture.

### Claim 10 (depends on 1)

The method according to claim 1, wherein concentrating the mixture comprises ultrafiltration.

### Claim 11 (depends on 1)

The method according to claim 1, wherein concentrating the mixture comprises thermal evaporation.

### Claim 12

A method comprising: (a) providing a silica sol having a BET surface area of 100 to 600 m2/g, wherein the silica sol comprises silicon dioxide particles having a mean particle diameter of 3 nm to 250 nm and a solids content of up to 45% by weight of silicon dioxide, based on the silica sol; (b) mixing the silica sol and an anionic polyether carboxylate to form a mixture, wherein the anionic polyether carboxylate is mixed with the silica sol in an amount of 0.05 to 10% by weight, based on the mixture; and (c) concentrating the mixture to form a concentrated mixture having a solids content of 40 to 60% by weight of silicon dioxide, based on the concentrated mixture.

### Claim 13 (depends on 1)

A concentrated mixture prepared by the method according to claim 1.

### Claim 14 (depends on 12)

A concentrated mixture prepared by the method according to claim 12.

### Claim 15

A concentrated silica sol mixture comprising: (a) silicon dioxide particles having a mean particle diameter of 3 nm to 250 nm and having a BET surface area of 15 to 1000 m2/g; and (b) an anionic polyether carboxylate; wherein the concentrated silica sol mixture has a solids content of 20 to 70% by weight of silicon dioxide, based on the concentrated mixture.